Investigation of UV, ns-laser damage resistance of hafnia films produced by electron beam evaporation and ion beam sputtering deposition methods

Laser-induced damage in coating materials with a high index of refraction, such as hafnia, limits the performance of high power and high energy laser systems. Understanding the underlying physics responsible for laser damage holds the key for developing damage-resistant optical films. Previous studies have reported a substantial difference in laser damage onset for hafnia films produced by different deposition methods, yet the underlying mechanisms for the observed difference remain elusive. We combined laser damage testing with analytical characterizations and theoretical simulations to investigate the response of hafnia films produced by electron (e-) beam evaporation vs ion beam sputtering (IBS) methods upon UV ns-laser exposure. We found that e-beam produced hafnia films were overall more damage resistant; in addition, we observed a polarization anisotropy associated with the onset of damage in the e-beam films, while this effect was absent in the latter films. The observed differences can be attributed to the stark contrast in the pressure inside the pores inherent in both films. The high pressure inside the IBS-induced nanobubbles has been shown to reduce the threshold for laser-induced plasma breakdown leading to film damage. The polarization effects in the e-beam coatings can be related to the asymmetric electric field intensification induced by the columnar void structure. Our findings provide a fundamental basis for developing strategies to produce laser damage-resistant coatings for UV pulsed laser applications.

36 MATERIALS SCIENCE↗

Type-I ELM mitigation by continuous lithium granule gravitational injection into the upper tungsten divertor in EAST

Large edge-localized modes (ELMs) were mitigated by gravitational injection of lithium granules into the upper X-point region of the experimental advanced superconducting tokamak (EAST) device with tungsten plasma-facing components. The maximum ELM size was reduced by ~70% in high β N H-mode plasmas. Large ELM stabilization was sustained for up to about 40 energy confinement times, with constant core radiated power and no evidence of high-Z or low-Z impurity accumulation. The lithium granules injection reduced the edge plasma pedestal density and temperature and their gradients, due to increased edge radiation and reduced recycling from the plasma-facing components. Ideal stability calculations using the ELITE code indicate that the stabilization of large ELMs correlates with improved stability of intermediate-n peeling-ballooning modes, due to reduced edge current resulting from the profile changes. The pedestal pressure reduction was partially offset by a core density increase, which resulted in a modest ~7% drop in core stored energy and normalized energy confinement time. We surmise that the remnant small ELMs are triggered by the penetration of multiple Li granules just past the separatrix, similar to small ELMs triggered by deuterium pellet Futatani et al (2014 Nucl. Fusion 54 073008). This study extends previous ELM elimination with Li powder injection Maingi et al (2018 Nucl. Fusion 58 024003) in EAST because (1) use of small, dust-like powder and the related potential health hazards were eliminated, and (2) use of macroscopic granules should be more applicable to future devices, due to deeper penetration than dust particles, e.g. inside the separatrix with velocities ~10 m s -1 in EAST.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Four α correlations in nuclear fragmentation: a game of resonances *

Abstract Heavy ion collisions near the Fermi energy produce a ‘freezout’ region where fragments appear and later decay, emitting mainly neutrons, protons, alpha particles, and gamma rays. These decay products carry information about the decaying nuclei. Fragmentation events may result in high yields of boson particles, especially alpha particles, and may carry important information about the nuclear Bose Einstein condensate (BEC). We study ‘in medium’ four α correlations and link them to the ‘fission’ of 16 O in two 8 Be in the ground state or 12 C * (Hoyle state)+ α . Using novel techniques for the correlation functions, we confirm the resonance of 16 O at 15.2 MeV excitation energy, and the possibility of a lower resonance, close to 14.72 MeV. The latter resonance is the result of all α particles having 92 keV relative kinetic energies.

Physics↗

Nuclear temperature and its dependence on the source neutron-proton asymmetry deduced using the Albergo thermometer

Albergo thermometers with double isotope, isotone and isobar yield ratio pairs with one proton or/and neutron difference are investigated. Without any extra sequential decay correction, a real temperature value of 4.9 ± 0.5 MeV is deduced from the yields of the experimentally reconstructed primary hot intermediate mass fragments (IMFs) from 64 Zn + 112 Sn collisions at 40 MeV/nucleon using the Albergo thermometer for the first time. An experimental sequential decay correction from the apparent temperatures to the real ones for twelve other reaction systems with different neutron-proton (N/Z) asymmetries in the same experiment, 70 Zn, 64 Ni on 112,124 Sn, 58,64 Ni, 197 Au, 232 Th at 40 MeV/nucleon, is performed using an empirical correction factor approach of Tsang et al. with the deduced 4.9 MeV temperature value. The dependence of nuclear temperature on the source N/Z asymmetry is further investigated using these deduced real source temperature values from the present thirteen systems. It is found that the deduced real source temperatures at the present source N/Z range show a rather weak dependence on the source N/Z asymmetry. In conclusion, by comparison between our previous results and those from other independent experiments, a consistent description for the N/Z asymmetry dependence of nuclear temperature is addressed.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Suppression of edge localized modes with real-time boron injection using the tungsten divertor in EAST

We report an observation of robust suppression of edge-localized modes (ELMs) in the Experimental Advanced Superconducting Tokamak (EAST), enabled by continuous boron (B) powder injection. Edge harmonic oscillations appear during B powder injection, providing sufficient particle transport to maintain constant density and avoid impurity accumulation in ELM-stable plasmas. Here, quasi-steady ELM suppression discharges are demonstrated with modest energy confinement improvement and over a wide range of conditions: heating power and technique variation, electron density range over a factor ~3.5, deuterium or helium ion species, and with either direction of the toroidal magnetic field. ELM suppression is observed above a threshold edge B intensity and ceases within 0.5 s of termination of the B injection. In contrast to ELM suppression accompanied by recycling reduction during Li powder injection in NSTX and EAST (Maingi et al 2018 Nucl. Fusion 58 024003), reduced recycling due to hydrogenic species retention is unnecessary for the ELM suppression with B powder injection, paving the way for its consideration as an ELM control tool for future fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Novel observation of isospin structure of short-range correlations in calcium isotopes

Short Range Correlations (SRCs) have been identiffed as being responsible for the high momentum tail of the nucleon momentum distribution, n(k). Hard, short-range interactions of nucleon pairs generate the high momentum tail and imprint a universal character on n(k) for all nuclei at large momentum. Triple coincidence experiments have shown a strong dominance of np pairs, but these measurements involve large final state interactions. This paper presents the results from Jefferson Lab experiment E08014 which measured inclusive electron scattering cross-section from Ca isotopes. Here, by comparing the inclusive cross section from 48 Ca to 40 Ca in a kinematic region dominated by SRCs we provide a new way to study the isospin structure of SRCs.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Deuterium retention characteristics in Li film by coating and during flowing liquid Li limiter operation in experimental advanced superconducting tokamak

Lithium (Li) is a promising low-Z material for particle recycling and impurity control to improve plasma performance in fusion devices. In the experimental advanced superconducting tokamak (EAST), Li coating has become a routine method for wall conditioning, and a flowing liquid Li (FLiLi) limiter has been successfully tested several times. Deuterium retention characteristics in the Li film coated on the international thermonuclear experimental reactor-like tungsten divertor and FLiLi during plasma discharges, which is important for the utilization of Li in future fusion devices, were investigated in EAST. It is found that the absorption of the fuel particles by Li coatings decreases gradually, and recycling gradually increases over a series of discharges. The maximum net amount of deuterium retained reached ~0.8 g, corresponding to 12% deuterium in the Li. Furthermore, this corresponds to a whole day's worth of shots with a total of 87 plasma discharges and a total of ~640s plasma time after 11.75 g Li was deposited. Compared to the Li coating, it is shown that FLiLi continuously traps fuel particles and achieves a higher deuterium retention ratio over both the short- and long-term, leading to lower recycling. Meanwhile, it is also observed that the fuel particle retention ratio increases when FLiLi is closer to the plasma. This result is likely due to higher plasma heating power and limiter temperature, which cause an increased Li efflux from FLiLi due to a higher limiter temperature, which then redeposits on the other plasma-facing surfaces and increases fuel particle absorption. It is estimated that ≥ 80% of the retained D particles are captured by the continual renewal of the Li redeposition film during the FLiLi operation. This investigation would also be useful for D/T retention in future fusion devices if Li is used as a plasma-facing component.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Lithium splashing from flowing liquid lithium limiter and its effect on high confinement plasma performance in EAST tokamak

To study the potential applications of liquid lithium (Li) as plasma facing material, the third generation of flowing liquid Li (FLiLi) limiter has been designed and successfully tested in EAST tokamak H-mode discharges in the 2018 run campaign. Here, the stability of liquid Li on FLiLi surface, and Li splashing and its effect on the plasma performance are investigated in detail. Li splashing was observed in L-mode and H-mode discharges due to Rayleigh-Taylor (R-T) instability, resulting from electromagnetic forces J → x B → . Li splashing in low-parameter plasma decreased both core and edge electron temperatures, resulting in the degradation of plasma energy confinement and even H-L back transition, however, it almost did not influence plasma confinement performance in high-parameter plasma. These findings indicate that high-parameter plasma has higher tolerance to Li impurities than low-parameter plasma. By contrast, tungsten splashing from the melted layer on the upper divertor was also induced by the R-T instability but generally resulted in plasma disruption, which suggests lower tolerance to tungsten impurities in EAST tokamak.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Corrosion of 304 stainless steel in static liquid lithium under high vacuum

To study the compatibility especially the corrosion characteristic of structural material stainless steel (SS) with liquid lithium (Li) is an important factor for the simultaneous application of liquid Li and SS as a blanket material or potential plasma facing material (PFM) in future fusion devices. Here, the corrosion behaviors of 304SS exposed to liquid Li at 700 K for 1320 hr under high vacuum were investigated. After exposure to liquid Li, 304SS produces non-uniform corrosion which includes corrosion products and grain boundary corrosion. Compared with the corrosion behaviors at 600 K and 640 K, temperature plays an important role in the corrosion behaviors of 304SS in static liquid Li. The weight loss, corrosion depth and corrosion products of 304SS specimens increase with the corrosion temperature. In general, the compatibility between 304SS and static liquid Li is relatively good under the experimental conditions. And besides, it is unexpectedly found that the compatibility of copper with Li is not good.

304SS↗

ELM Suppression by Boron Powder Injection and Comparison with Lithium Powder Injection on EAST

Type I edge-localized modes (ELMs) in the Experimental Advanced Superconducting Tokamak (EAST) were completely suppressed via boron powder injection into the X-point region of an upper-single null configuration over a wide range of operating conditions (2.8 < P aux < 7.5 MW, 3.8 × 10 19 < n e < 6 × 10 19 m -3 , RF-only and RF + NBI heating scenarios, both grad-B drift directions, and even He ion majority plasmas) (Sun et al. in Nucl. Fusion, 2020). A window of edge B concentration for stable long pulse operation was identified: too low and ELMs return, too high and the discharge suffers radiative collapse. The injection of boron powder above the minimum for ELM suppression coincided with the occurrence of an edge harmonic oscillation detected in magnetics (both on the high-field side and low-field side), in AXUV diodes near the upper X-point, divertor Dα emission, and in a range of other diagnostics (Diallo et al. in: Proceedings of 2020 IAEA fusion energy conference, 2021). Furthermore, no harmonic oscillation was observed when ELMs were present, and stored energy was slightly increased at constant density during ELM suppression. Core tungsten emission during ELM suppression either increased or decreased relative to ELMy H-mode, but the W emission was maintained at acceptable levels. The threshold B injection rate was measured for several conditions, and found to increase with heating power. Li powder injection into comparable discharges also resulted in a short phase of ELM suppression, but density and stored energy both decreased due to the strong pumping effect of lithium; no edge harmonic oscillation was observed with Li injection, indicating that the ELM suppression mechanisms differ. The new set of B-seeded, ELM-suppressed discharges exhibited certain characteristics of quiescent H-mode (Burrell et al. in Phys Plasmas 8:2153, 2001), but did not require high shear, counter beams, etc. The wide operating window and compatibility with RF-only discharges paves the way for future experiments targeting long pulse H-mode discharges with complete ELM suppression.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effect of lithium coating on long pulse high performance plasma discharges in EAST

Control of impurities, fuel recycling and hydrogen content by lithium evaporative coatings and real-time lithium powder injection (LPI) in EAST are studied for high performance H-mode discharges of up to ~100 s. The results show that the lithium evaporative coatings significantly reduced both the low-Z impurity carbon and high-Z impurity tungsten as well as molybdenum concentration in the plasmas, and the impurities concentration significantly reduced with the accumulated lithium coatings and maintained well afterwards. Specifically the high-Z tungsten core impurity concentration was maintained between 3 ppm–15 ppm during the 101 s H-mode discharge, which is acceptable for the long pulse operation. In addition, real-time wall conditioning via LPI successfully reduced the core high-Z metal impurities by 50% during ~35 s long pulse H-mode discharge, exhibiting strong compatibility between real-time LPI with long pulse discharges. In addition, evaporative lithium coatings demonstrated fuel recycling control, with fuel recycling obviously reducing with lithium coatings and maintaining well afterwards. Also, the lithium evaporative coatings reduced the hydrogen minority species content, represented by the density ratio H/(H + D), from ~50% down to ~5% with accumulated lithium coatings; low hydrogen fraction improved the ICRF minority heating efficiency. Finally the real-time LPI reduced the recycling coefficient R global from 0.95 to 0.82. With these wall conditionings help, the plasma density controlled well during the 101 s long pulse H-mode discharge. Furthermore, these results provide valuable references on impurities, fuel recycling and hydrogen content control for future longer pulse high performance H-mode operation (≥400 s) in EAST and future fusion devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Probing the neutron-proton asymmetry dependence of the nuclear source temperature with light charged particles

The dependence of the nuclear temperature on the source neutron-proton (N/Z) asymmetry was experimentally investigated with the light charged particles (LCPs) generated from thirteen reaction systems with different N/Z asymmetries, 64 Zn on 112 Sn and 70 Zn, 64 Ni on 112,124 Sn, 58,64 Ni, 197 Au, 232 Th at 40 MeV/u. A rather weak N/Z asymmetry dependence of the source temperature was qualitatively inferred from the extracted N/Z asymmetry dependence of the apparent temperature and that of the relative temperature change by the sequential decay effects with the help of the theoretical simulations. Comparing the present result with those from our previous work and other available experimental results, a weak N/Z asymmetry dependence of nuclear temperature is commonly observed in different independent experiments and with different thermometers, except for the result reported by McIntosh et al. [Phys. Lett. B 719, 337 (2013)]. Here, the origin of the difference between the conclusion of the former group and that of McIntosh et al. was addressed, using statistical multifragmentation model (SMM) simulations.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Results from a new flowing liquid Li limiter with TZM substrate during high confinement plasmas in the EAST device

A third generation flowing liquid lithium (FLiLi) limiter with a substrate made of TZM, an alloy with >99% Mo, was fabricated by conventional manufacturing techniques. TZM has a high corrosion resistance, a high sputtering threshold, and a good wettability to Li, as compared to stainless steel (SS), which had been used as an FLiLi substrate surface in 2014 and 2016. The third generation FLiLi was inserted into the edge in EAST H-mode plasmas in an upper single-null configuration with an ion grad-B drift toward the upper divertor with a limiter temperature of 330–380 °C and an auxiliary heating power of about 2–8 MW. Analysis has shown that by using TZM FLiLi, fuel particle recycling continuously decreased and near-complete edge localized mode elimination was achieved in H-mode plasmas with RF-only heating. The main impurities during the initial FLiLi discharges were Mo, Fe, and W resulting from strong plasma interaction at the Mo plate side, the SS collector, and the upper W divertor. Plasma stored energy increased by about 10 kJ in subsequent FLiLi discharges due to decreased impurity radiation. Engineering analysis shows a uniform lithium flow with an ~80% Li coverage ratio on the limiter surface, similar to the second FLiLi, even though only one of two J × B pumps was functioning. Despite technical difficulties, the FLiLi gen.3 improved the overall plasma performance, providing support for flowing liquid Li plasma facing component applications in present and future devices.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Improvement on the plasma performances via application of flowing lithium limiters in EAST tokamak

Three generation of flowing liquid lithium (FLiLi) limiters have been developed and successfully tested in EAST since 2014. It was confirmed that liquid Li could be driven by an innovative in-vessel DC electromagnetic J × B pump to form a recirculating loop. The FLiLi design was continuously upgraded, resulting in improvement of the liquid Li surface coverage (>80%), elimination of surface erosion, and the increase of heat exhaust capability. Promising results are obtained during FLiLi operations, including a reduction of impurities and recycling to improve plasma confinement, and a mitigation of ELM activity in H-mode plasmas. The FLiLi limiter program has shown basic compatibility with H-mode discharges with auxiliary heating power up to 8.3 MW. These efforts will expand to flowing liquid Li PFC in high heat flux zones, e.g. near the divertor strike point in reactors.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Real-time gas cooling of flowing liquid lithium limiter for the EAST

A novel continuously flowing liquid lithium limiter (FLiLi) which employs an in-vessel electro-magnetic pump to drive liquid Li flowing on the surface of limiter has been successfully designed and tested in the experimental advanced superconducting tokamak (EAST) device in 2014. In order to better control the surface temperature, an upgraded design and the real-time gas cooling were performed in 2016. Two kinds of cooling gas, helium (He) and argon (Ar) were tested on the FLiLi system prior to the experiment. It was found that the cooling rates of He and Ar at 2.5 MPa are 34.2 °C/min, 10.2 °C/min or 31.7 °C/kL and 28.1 °C/kL, respectively. The cooling performance of He is more effective than Ar. Experimental results show that the real-time He cooling could effectively contain the FLiLi surface temperature increase and prevent the strong passive evaporation of lithium during plasma discharges. Limiter heat flux up to 0.2 MW/m2 was removed during ohmic discharge with 2.5 MPa He gas. Finally, Because of the upgraded design and real-time gas cooling, the surface of FLiLi was not damaged by heat flux after entire plasma discharge.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗