Search NASA⌕ Search

Engineering topics

Huang, Xiaoxu

Publications and source records attributed to Huang, Xiaoxu.

In-situ synchrotron X-ray micro-diffraction investigation of ultra-low-strain deformation microstructure in laminated Ti-Al composites

An ultra-low-strain deformation microstructure was revealed for the first time non-destructively in the bulk interior of an annealed laminated Ti-Al composite-in the "fully recrystallized" Al layer-by a synchrotron-based micro-diffraction technique, namely differential aperture X-ray microscopy (DAXM), through real space mapping with a very high angular resolution (0.01 degrees). This ultra-low-strain deformation microstructure was found to result from the thermal stress, induced during cooling after annealing, due to the different coefficients of thermal expansion for the Ti and Al layers. The annealed sample was further tensile deformed to a strain of 1.66% and followed by in situ DAXM and analyzed by various misorientation mapping methods. The results pointed to the important effects of the initial microstructure and the interface constraint, as well as the grain size and crystal orientation, on the plastic deformation. A gradient in dislocation density from the layer interface to the center was found in the Al layer of the annealed sample, and this gradient increased slightly during tensile deformation. The variation of the dislocation density was further discussed based on the activation and interaction of dislocations in grains of different sizes and orientations during plastic deformation. The findings of this study provided valuable insights in understanding the constraint effect of the laminated metal composite and the design of novel composite materials. (c) 2020 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Crystallographic orientation↗

High-pressure strengthening in ultrafine-grained metals

The Hall–Petch relationship, according to which the strength of a metal increases as the grain size decreases, has been reported to break down at a critical grain size of around 10 to 15 nanometres. As the grain size decreases beyond this point, the dominant mechanism of deformation switches from a dislocation-mediated process to grain boundary sliding, leading to material softening. In one previous approach, stabilization of grain boundaries through relaxation and molybdenum segregation was used to prevent this softening effect in nickel–molybdenum alloys with grain sizes below 10 nanometres. Here we track in situ the yield stress and deformation texturing of pure nickel samples of various average grain sizes using a diamond anvil cell coupled with radial X-ray diffraction. Our high-pressure experiments reveal continuous strengthening in samples with grain sizes from 200 nanometres down to 3 nanometres, with the strengthening enhanced (rather than reduced) at grain sizes smaller than 20 nanometres. Here, we achieve a yield strength of approximately 4.2 gigapascals in our 3-nanometre-grain-size samples, ten times stronger than that of a commercial nickel material. A maximum flow stress of 10.2 gigapascals is obtained in nickel of grain size 3 nanometres for the pressure range studied here. We see similar patterns of compression strengthening in gold and palladium samples down to the smallest grain sizes. Simulations and transmission electron microscopy reveal that the high strength observed in nickel of grain size 3 nanometres is caused by the superposition of strengthening mechanisms: both partial and full dislocation hardening plus suppression of grain boundary plasticity. These insights contribute the ongoing search for ultrastrong metals via materials engineering.

36 MATERIALS SCIENCE↗