Effect of deposition temperature of TiO{sub 2} on the piezoelectric property of PbTiO{sub 3} film grown by PbO gas phase reaction sputtering.

A 17 nm thick PbTiO{sub 3} (PTO) films were fabricated via PbO gas phase reaction with TiO{sub 2} starting layer in a sputtering chamber. The influence of deposition temperature of TiO{sub 2} on the piezoelectric properties of PTO thin films was investigated. The remnant piezoresponse of PTO films nonlinearly increased as a function of TiO{sub 2} deposition temperature, which is correlated with the increase in average grain diameter of PTO film. As grain size increases, the restriction on remnant piezoresponse imposed by the grain boundary via coupling between local strain and polarization becomes less pronounced, which results in the increase in remnant piezoresponse. Furthermore, we found that the vertical shift in piezoresponse hysteresis loops is closely related to the residual stress state. A strong correlation between the negative vertical shift and the residual tensile stress reveals that residual stress on the resulting PTO film contributed to the asymmetric piezoelectric property.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Nanoscale piezoresponse of 70-nm poly(vinylidene fluoride-trifluoroethylene) films annealed at different temperatures.

In order to characterize the piezoelectric properties of 70 nm thick poly(vinylidene fluoride-trifluoroethylene), P(VDF-TrFE), films grown by a spin-coating technique, both nanoscale manipulation and polarization switching were studied using piezoresponse force microscopy (PFM). We varied the annealing temperature from 75 C to 145 C and achieved a high-quality 70 nm P(VDF-TrFE) film annealed at the temperature of 95 C. Ferroelectric domains and their properties were confirmed using X-ray diffraction, grazing incidence reflection absorption Fourier Transform Infrared (GIRA-FTIR) and PFM analysis. The ferroelectric domains in the film were homogeneously switchable below 5 V with a remnant d{sub 33} of 14.9 pm/V. This offers our rationale for a promise in energy harvesting and switchability would be good for plastic electronics.

36 MATERIALS SCIENCE↗

Spin-polarized transport current in n-type codoped ZnO thin films measured by Andreev spectroscopy.

We use point-contact Andreev-reflection measurements to determine the spin polarization of the transport current in pulse laser deposited thin films of ZnO with 1% Al and with and without 2% Mn. Only films with Mn are ferromagnetic and show spin polarization of the transport current of up to 55 {+-} 0.5% at 4.2 K, in sharp contrast to measurements of the nonmagnetic films without Mn where the polarization is consistent with zero. Our results imply strongly that ferromagnetism in these Al-doped ZnO films requires the presence of Mn.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Vacancy defects in Fe : comparison between simulation and experiment.

The evolution of radiation damage under heavy-ion irradiation in thin foils of pure bcc Fe has been investigated by simulation and experiment. Simulations showed that vacancy loops are about as mobile as interstitial loops, and can be lost to the surface of a foil. Consistent with this, in situ real-time dynamic observations of the damage evolution showed that loops, many of which are believed to be of vacancy nature, were mobile and were often lost during irradiation. Atomistic simulations of vacancy defects in Fe showed that spherical voids, rather than vacancy loops, represent the lowest energy configurations for clusters of vacancies of any size. The simulations also indicated that the stability of loops strongly varies depending on their size. Closed loops above a critical diameter ({approx}2 nm) are highly metastable due to the difficulty of their transformation into voids. The greater stability of voids explains why the loop yield in Fe and other ferritic materials is very low.

36 MATERIALS SCIENCE↗

Particle size effect of hydrogen-induced lattice expansion of palladium nanoclusters.

In situ synchrotron x-ray diffraction experiments on bare palladium nanoclusters prepared by inert-gas aggregation and size selected (1.7-6.0 nm) show significant changes in lattice parameter upon hydrogen loading and a narrowing of the miscibility gap, as the cluster size decreases. The results show that the miscibility gap is open for all cluster sizes studied, in contrast to previous literature results from surfactant-encapsulated palladium clusters. We interpret these results by showing that the nature of the surface is critical in the hydrogenation behavior of the nanoclusters.