Publications and source records attributed to Imrich, K.

MAGNOX:BUTEX URANIUM BEARING GLASSES PHYSICAL AND CHEMICAL ANALYSIS DATA PACKAGE

Sellafield Ltd (United Kingdom) has requested technical support from the Savannah River National Laboratory (SRNL) to characterize a series of uranium-bearing, mixed alkali borosilicate glasses [WFO (2010)]. The specific glasses to be characterized are based on different blends of Magnox (WRW17 simulant) and Butex (or HASTs 1 and 2) waste types as well as different incorporation rates (or waste loadings) of each blend. Specific Magnox:Butex blend ratios of interest include: 75:25, 60:40, and 50:50. Each of these waste blend ratios will be mixed with a base glass additive composition targeting waste loadings (WLs) of 25, 28, and 32% which will result in nine different glasses. The nine glasses are to be fabricated and physically characterized to provide Sellafield Ltd with the technical data to evaluate the impacts of various Magnox:Butex blend ratios and WLs on key glass properties of interest. It should be noted that the use of 'acceptable' in the Work for Other (WFO) was linked to the results of a durability test (more specifically the Soxhlet leach test). Other processing (e.g., viscosity ({eta}), liquidus temperature (T{sub L})) or product performance (e.g., Product Consistency Test (PCT) results - in addition to the Soxhlet leach test) property constraints were not identified. For example, a critical hold point in the classification of an 'acceptable glass' prior to processing high-level waste (HLW) through the Defense Waste Processing Facility (DWPF) is an evaluation of specific processing and product performance properties against pre-defined constraints. This process is referred to as Slurry Mix Evaporator (SME) acceptability in which predicted glass properties (based on compositional measurements) are compared to predefined constraints to determine whether the glass is acceptable [Brown and Postles (1995)]. As an example, although the nominal melter temperature at DWPF is 1150 C, there is a T{sub L} constraint (without uncertainties applied) of 1050 C. Any glass which has a T{sub L} predicted value > 1050 C would be classified as unacceptable and the SME product would not be transferred to the melter. As another example, consider durability (as defined by the PCT test) and its related constraints to determine acceptability. If the glass composition yields predicted normalized release values that exceed those associated with the Environmental Assessment (EA) glass (with uncertainties applied) then the glass is deemed unacceptable. The issue of acceptability plays a critical role in high level waste processing but without knowing the pre-defined constraints for the UK HLW system, assessments of acceptability of the glasses to be characterized in this study can not be made. The results of this study will be compared to DWPF constraints to provide a benchmark for determining acceptability. The objective of this task is to provide Sellafield Ltd. with the technical data to evaluate the impacts of various Magnox:Butex blend ratios and WLs on key glass properties of interest. The uranium bearing glasses span a compositional region of interest to Sellafield Ltd. and were physically characterized for key processing and product performance properties as defined in the WFO [WFO (2010)]. One of the specific technical issues (as defined in the WFO) is the potential impact of increasing aluminum concentrations on key properties (in particular viscosity).

36 MATERIALS SCIENCE↗

DWPF GC FILTER ASSEMBLY SAMPLING AND ANALYSIS

On March 18, 2009 a Defense Waste Processing Facility (DWPF) GC Line Filter Assembly was received at the Savannah River National Laboratory (SRNL). This filter assembly was removed from operation following the completion of Sludge Batch 4 processing in the DWPF. Work on this sample was requested in a Technical Assistance Request. This document reports the pictures, observations, samples collected, and analytical results for the assembly. The assembly arrived at SRNL separated into its three component filters: high efficiency particulate air (HEPA)-1, HEPA-2, and a high efficiency mist evaporator (HEME). Each stage of the assembly's media was sampled and examined visually and by scanning electron microscopy (SEM). Solids built up in the filter housing following the first stage HEME, were dissolved in dilute nitric acid and analyzed by ICP-AES and the undissolved white solids were analyzed by x-ray diffraction (XRD). The vast majority of the material in each of the three stages of the DWPF GC Line Filter Assembly appears to be contaminated with a Hg compound that is {approx}59 wt% Hg on a total solids basis. The Hg species was identified by XRD analysis to contain a mixture of Hg{sub 4}(OH)(NO{sub 3}){sub 3} and Hg{sub 10}(OH){sub 4}(NO{sub 3}){sub 6}. Only in the core sample of the second stage HEPA, did this material appear to be completely covering portions of the filter media, possibly explaining the pressure drops observed by DWPF. The fact that the material migrates through the HEME filter and both HEPA filters, and that it was seen collecting on the outlet side of the HEME filter, would seem to indicate that these filters are not efficient at removing this material. Further SRAT off-gas system modeling should help determine the extent of Hg breakthrough past the Mercury Water Wash Tank (MWWT). The SRAT off-gas system has not been modeled since startup of the facility. Improvements to the efficiency of Hg stripping prior to the ammonia scrubber would seem to be the only way to prevent/mitigate the formation of the compounds found in the GC Line Filter Assembly filters and therefore prevent pluggage of this filter assembly.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

EVALUATION OF TGA AS A QUALITY ASSURANCE TOOL FOR SURFACEMODIFIED ZIRCOLOY-4

Thermogravimetric analysis (TGA) and coupled Mass Spectroscopy (MS) were evaluated to determine their suitability as a quality assurance tool for surface modified nickel plated zircaloy-4 liner tubes. Samples with 0, 0.1, 0.2, 0.3, and 0.4 mils of heat treated nickel plate were tested at 330, 370, and 400 C. Not all of the samples exhibited the expected typical parabolic shaped oxidation curve. The measured weight change was consistent for the as received and 0.2 mil and the 0.4 mil surface modified samples. None of the samples were tested under aggressive enough conditions to consume the surface modified materials during the test duration. Use of the Mass Spectrometer in conjunction with the TGA did not produce valuable data and was only used for the 400 C test series; however, the TGA was valuable. The 0.1 and 0.3 mil surface modified Zr-4 samples exhibited thru surface modified layer cracks which could account for the variation in oxidation behavior. TGA tests for periods up to six hours appear viable as a method to ascertain oxidation behavior for consistent results. Additional testing of samples with known variations in surface modified layer thickness and quality is recommended as part of the QA acceptance testing.

36 MATERIALS SCIENCE↗