Search NASA⌕ Search

Engineering topics

Ishikawa, Yasushi

Publications and source records attributed to Ishikawa, Yasushi.

Controllable modification of self-assembled monolayer surface by using N{sub 2} neutral beam process

A novel technique of low-energy N{sub 2} neutral beam (NB) (<10 eV) irradiation was investigated as a means of controlling the surface nitridation of self-assembled monolayers (SAMs). This low-energy process without UV photons was able to nitride the surfaces of terphenyl SAMs. Furthermore, by varying the on/off period for irradiation, a pulse-time modulated NB process could be used to control the atomic ratio of nitrogen in terphenyl molecules. Time-of-flight secondary ion mass spectra revealed that one H in the terphenyl group was substituted by a NH{sub 2} group because of irradiation by the N{sub 2} beam. The data suggested that the low-energy NB technique caused less damage to modified surfaces than the conventional plasma process did. Therefore, we believe that it is a potential damage-free process for modifying the surfaces of soft organic materials and films.

36 MATERIALS SCIENCE↗

UV photon-induced defect and its control in plasma etching processes

We found that the use of pulse-time-modulated (TM) plasma reduces ultraviolet (UV) photon-induced defects in SiO{sub 2} films formed during plasma etching. The pulse timing of the radio-frequency power in the TM plasma was modulated at a few tens of microseconds. During the pulse-off period, UV photon radiation significantly decreased because of reduced electron energy in the plasma. As a result, the density of UV photon-induced defects, such as E{sup '} centers, in SiO{sub 2} films was reduced when the TM plasma was used compared with that when a continuous wave (CW) plasma was used. In addition, we found that the energy level of excitation states of the E{sup '} centers generated in the TM plasma was less than that generated when the CW plasma was used. Low-temperature annealing was needed to reduce the number of E{sup '} centers when the TM plasma was used; whereas higher-temperature annealing was needed when the CW plasma was used. These results showed that the energy level of excitation states of UV photon-induced defects in SiO{sub 2} films was reduced by using the TM plasma.

36 MATERIALS SCIENCE↗

Generation and reduction in SiO{sub 2}/Si interface state density during plasma etching processes

During plasma processes, the SiO{sub 2}/Si interface state is generated by UV photon irradiation. We measured P{sub b} centers (Si dangling bond at SiO{sub 2}/Si interface) in SiO{sub 2}/Si film by electron spin resonance spectroscopy. The density of P{sub b} centers increased with increasing UV photon energy. This result indicates that high-energy photons effectively generate P{sub b} centers because of the absorption at the SiO{sub 2}/Si interface. At the same time, we found that UV photon flux is also an important factor in increasing the density of P{sub b} centers. On the other hand, ion irradiations were not a significant factor in the generation of P{sub b} centers. Ions can penetrate only the surface (less than 5 nm) but they cannot induce a P{sub b} center at the SiO{sub 2}/Si interface. Furthermore, pulse-time-modulated plasmas were used to reduce the UV photon irradiation during the plasma processes. The reduction in UV photon irradiation could completely eliminate the P{sub b} centers compared with the use of a conventional continuous wave plasma.

36 MATERIALS SCIENCE↗