Search NASA⌕ Search

Engineering topics

Jansen, Andrew N.

Publications and source records attributed to Jansen, Andrew N..

At least 19 records

Fast-charging lithium-ion batteries: Synergy of carbon nanotubes and laser ablation

Advancing lithium-ion battery (LiB) technology to achieve 10–15-min extreme fast charging (XFC) while maintaining high energy density and longevity poses a significant challenge. Addressing Li-plating is crucial, as it depletes useable Li, causing deterioration and safety issues. Here, this study explores a holistic approach incorporating Single-Wall Carbon Nanotubes (SWCNTs) and Laser Ablation (LA) to mitigate Li-plating while maintaining high charge acceptance under 10–15-min XFC. SWCNTs enhance the electrical conductivity and mechanical integrity of the positive electrode (PE), reducing overall cell overpotential at high charging rates. Concurrently, LA is applied to negative electrodes (NE) to reduce tortuosity of ion-diffusion pathways and increase surface wettability, improving Li-ion transport. Combining SWCNTs in the PE and LA on the NE, our experimental findings demonstrate a significant reduction in Li-plating and maintained high charge acceptance of ~84.33 % after 800 5C (12 min) charge cycles for cells having PE with ~3.3 mAh cm –2 and NE with 3.9 mAh cm –2 loadings. This study highlights the potential of combining SWCNTs and LA to address Li-plating in LiBs and opens new avenues for designing battery systems capable of achieving 10–15-min XFC.

24 POWER TRANSMISSION AND DISTRIBUTION↗

Inactive Overhang in Silicon Anodes

Li-ion batteries contain excess anode area to improve manufacturability and prevent Li plating. These overhang areas in graphite electrodes are active but experience decreased Li + flux during cycling. Over time, the overhang and the anode portions directly opposite to the cathode can exchange Li + , driven by differences in local electrical potential across the electrode, which artificially inflates or decreases the measured cell capacity. Here, we show that lithiation of the overhang is less likely to happen in silicon anodes paired with layered oxide cathodes. The large voltage hysteresis of silicon creates a lower driving force for Li + exchange as lithium ions transit into the overhang, rendering this exchange highly inefficient. For crystalline Si particles, Li + storage at the overhang is prohibitive, because the low potential required for the initial lithiation can act as thermodynamic barrier for this exchange. We use micro-Raman spectroscopy to demonstrate that crystalline Si particles at the overhang are never lithiated even after cell storage at 45 °C for four months. Because the anode overhang can affect the forecasting of cell life, cells using silicon anodes may require different methodologies for life estimation compared to those used for traditional graphite-based Li-ion batteries.

25 ENERGY STORAGE↗

Carbon-Binder Optimization for Lithium-Ion Battery Extreme Fast Charge

Battery performance is strongly correlated with electrode microstructure and weight loading of the electrode components. Among them are the carbon-black and binder additives that enhance effective conductivity and provide mechanical integrity. However, these both reduce effective ionic transport in the electrolyte phase and reduce energy density. Therefore, an optimal additive loading is required to maximize performance, especially for fast charging where ionic transport is essential. Such optimization analysis is however challenging due to the nanoscale imaging limitations that prevent characterizing this additive phase and thus quantifying its impact on performance. Herein, an additive-phase generation algorithm has been developed to remedy this limitation and identify percolation threshold used to define a minimal additive loading. Improved ionic transport coefficients from reducing additive loading has been then quantified through homogenization calculation, macroscale model fitting, and experimental symmetric cell measurement, with good agreement between the methods. Rate capability test demonstrates capacity improvement at fast charge at the beginning of life, from 37% to 55%, respectively for high and low additive loading during 6C CC charging, in agreement with macroscale model, and attributed to a combination of lower cathode impedance, reduced electrode tortuosity and cathode thickness.

carbon-binder additives↗

Large Local Currents in a Lithium-Ion Battery during Rest after Fast Charging

Increasing electric vehicle (EV) adoption requires lithium-ion batteries that can be charged quickly and safely. Some EV batteries have caught on fire despite being neither charged nor discharged. While the lithium that plates on graphite during fast charging affects battery safety, so do the internal ionic currents that can occur when the battery is at rest after charging. These currents are difficult to quantify; the external current that can readily be measured is zero. Here we study a graphite electrode at rest after 6C fast charging using operando X-ray microtomography. We quantify spatially resolved current density distributions that originate at plated lithium and end in underlithiated graphite particles. The average current densities decrease from 1.5 to 0.5 mA cm -2 in about 20 min after charging is stopped. Surprisingly, the range of the stripping current density is independent of time, with outliers above 20 mA cm -2 . In conclusion, the persistence of outliers provides a clue as to the origin of catastrophic failure in batteries at rest.

25 ENERGY STORAGE↗

Consequences of utilizing a redox-active polymeric binder in Li-ion batteries

Development of new polymeric binders can help enable the use of silicon-rich anodes in Li-ion batteries, by providing stronger adhesion to the active material particles. The compositional features that improve interfacial interactions and mechanical properties can often impart electronic conductivity and redox activity to these polymers, which are generally seen as beneficial to cell performance. Alternatively, it is also possible that the addition of charge-transferring centers to the electrode can accelerate cell degradation. Here, we use an aromatic polyimide (∼320 mA h/g of reversible capacity) to explore how a redox-active conductive polymer can affect cell performance. We demonstrate that the lithiated polymer is less stable than the traditional binders upon storage, leading to increased rates of calendar aging. Furthermore, we determine that the adhesion properties of the polymer deteriorate upon repeated cycling, to an extent that is proportional to the degree of delithiation of the binder. More critically, we establish that progressive degradation of the redox behavior of the polymer leads to the release of “extra” Li + into the cell, which can give the false perception of good performance even under conditions of poor stability. In conclusion, our work suggests that redox-active conductive binders can sometimes be detrimental to cell performance, and that works evaluating new polymers must include careful experimental validation under realistic conditions.

25 ENERGY STORAGE↗

Cell-Format-Dependent Mechanical Damage in Silicon Anodes

Strong binders can be counterproductive for silicon anodes. Here, we show that stresses from cycling Si-based electrodes can cause permanent stretching and wrinkling of the current collector. Furthermore, this deformation damages the electrode coating and accelerates cell aging due to the inactivation of Si domains and facilitation of Li plating. Interestingly, we demonstrate that the formation of wrinkles is size-dependent, being present in pouch cells but absent from coin cells. This size-dependent performance decay indicates that, in extreme cases, testing outcomes are highly dependent on scale and that the validation of battery materials may require testing at larger cell formats.

25 ENERGY STORAGE↗

High‐Nickel Heterostructured Cathodes with Local Stoichiometry Control for High‐Voltage Operation

The growing demand for lithium‐ion batteries to power electric vehicles and other energy‐dense devices continues to fuel the need for cathodes of increasingly higher nickel in cathodes. The relentless pursuit of high Ni content, however, raises concerns on compromising cell lifetime and safety, especially under high‐voltage operation. Alternative to the traditional design of uniform or core–shell composition, we report a rational control of local stoichiometry in high‐Ni cathodes, enabling their high thermal and cycling stabilities—up to 258 °C at the fully charged state and 91.4% capacity retention for 100 cycles between 2.7 and 4.4 V. Multimodal synchrotron X‐ray characterization unveils the heterostructure of secondary particles, featuring a high‐Ni core (LiNi 0.90 Mn 0.05 Co 0.05 O 2 ) covered by a thin Ni‐gradient layer that remains stable over prolonged cycling due to suppressed oxygen release and structural deterioration. This work underlines, the intricate interplay between local stoichiometry and redox reactions in stabilizing high‐Ni cathodes for high‐voltage operation while ensuring safety.

36 MATERIALS SCIENCE↗

Rational designs to enable 10-min fast charging and long cycle life in lithium-ion batteries

A daunting challenge in the design of lithium ion batteries (LiBs) is enabling 10-min extreme fast charging (XFC) while achieving appreciable charge acceptance and cycle life. This desirable outcome requires both a comprehensive understanding of LiB operation and aging behavior at different length scales and careful optimization. Lithium plating has been a critical bottleneck because, at XFC rates, it consumes cyclable lithium causing distinct aging and safety concerns even in moderate-loading LiBs. Here, we propose combining multiple solutions, including materials-to-electrode design-to-charging protocols, that are intended to overcome limitations in lithium-ion transport in the electrolyte phase, thus enabling 10-min XFC in LiBs. Some implemented strategies include cathode chemistry, optimized carbon binder domain in the cathode, dual layer anode design, improved separator and advanced electrolyte. Further, innovative charging protocols in moderately loading (~3 mAh/cm 2 anode/2.7 mAh/cm 2 cathode) single-layer pouch cells are proposed, together with demonstrated 10-min XFC with higher charge acceptance between 87.3 and 92.1% (or 2–2.1 mAh/cm 2 ) for 600 cycles without lithium plating. This methodical study with well-defined cells shows promise in combining multiple solution strategies to enable 10-min XFC, charting a pathway to achieve XFC in higher-loading energy-optimized LiBs.

25 ENERGY STORAGE↗

Designing Li 4 Ti 5 O 12 /LiMn 2 O 4 Cells: Negative-to-Positive Ratio and Electrolyte

Li 4 Ti 5 O12/LiMn2O 4 (LTO/LMO) system is a promising candidate for behind-the-meter storage (BTMS) applications due to its critical-material-free chemistry exhibiting good safety and long lifetime. In this paper we design LTO/LMO cells to mitigate their major degradation mechanism, loss of Li inventory, and improve their long-term cyclability. First, LMO electrodes with different loadings (2.61, 3.29, and 4.26 mAh cm -2 ) are paired with an LTO electrode (3.35 mAh cm -2 ) to create varying negative-to-positive ratios (N/P>1, =1, and <1). Additionally, conventional ethylene carbonate (EC)/ethyl methyl carbonate (EMC) mixture electrolyte and safety enhanced EC-only electrolyte are examined. We show that storing additional Li inventory in the cathode (i.e., using a thicker electrode and having N/P<1) is a convenient method to enhance the capacity retention of LTO/LMO cells, but only if the electrode utilization is not limited by the Li + ion transport. For systems that suffer from limited transport properties, prelithiating the anode will be more effective since LTO (~165 mAh g -1 LTO ) can store the same amount of capacity using less material compared to LMO (~100 mAh g -1 LMO ). In this work, we demonstrate how the electrolyte properties and the electrode thickness of LTO/LMO cells can be designed to enhance their performance.

25 ENERGY STORAGE↗

Pouch cells with 15% silicon calendar-aged for 4 years

Small amounts of high-capacity silicon-based materials are already used in the anode of commercial Li-ion batteries, helping increase their energy density. Despite their remarkable storage capability, silicon continu-ously reacts with the electrolyte, accelerating time-dependent cell performance fade. Nevertheless, very limited information is available on the specific consequences of this reactivity for the calendar aging of Li-ion cells. Here, we analyze aging effects on 450 mAh pouch cells containing 15 wt% of Si (and 73 wt% graphite) after storage at 21 °C for four years. We show that severe losses of Si capacity occurred due to particle isolation when cells were stored at high states of charge (SOC), but not when cells were fully discharged prior to storage. Impedance rise was also significantly higher when cells were kept at high SOCs and was mostly due to phenomena taking place at the cathode; the continuous electrolyte reduction at the anode did not lead to a major increase in bulk electrode resistance. A series of post-test characterization provided additional information on the effects of time and SOC on the calendar aging of Si-containing cells. In conclusion, our study highlights the many challenges posed by Si during calendar aging and can inform future studies in the field.

25 ENERGY STORAGE↗

Electrolyte Study for High-Nickel LiNi 0.9 Mn 0.05 Co 0.05 O 2 Cathodes

With an increasing demand for intermittent renewable energy and electric vehicles, it is imperative to develop lithium-ion batteries with Earth-abundant cathode materials. Cobalt (Co) is preferred to be kept at a minimum because of its high cost and limited mining options, yet it has played an essential role in the high-performance transition metal oxides (TMOs). Herein, we report work from Argonne National Laboratory, conducted under the U.S. DoE's Vehicle Technologies Office, Deep Dive consortium on Next-Generation Cathodes, to optimize electrolytes for LiNi 0.9 Mn 0.05 Co 0.05 O 2 . LiNi 0.9 Mn 0.05 Co 0.05 O 2 is a high-Ni TMO benchmark as it outperforms most other TMOs under standard cycling conditions. In this study, we use the figure-of-merit approach to optimize electrolytes for this novel cathode material. Dual-salt carbonate electrolytes containing lithium difluorooxyphosphate and hexafluorophosphates were found to be the best for capacity retention and slowing the impedance rise. Importantly, transition metal dissolution and lithium inventory losses in the solid electrolyte interface were found to be the major causes for capacity fade.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Evolution of LiNi 0.5 Mn 0.3 Co 0.2 O 2 Particle Damage from Fast Charging in Optimized, Full Li-Ion Cells

Fast charging batteries are critical to the widespread adoption of electric vehicles to compete with refueling times of combustion-based vehicles. In the near term, adapting current commercial battery technologies to perform better under fast charging conditions through engineering optimizations will greatly expedite the process while exploratory fast-charging electrode materials are being pursued. To do so, the degradation modes in optimized Li-ion batteries need to be completely explored to understand fast charging limits while maintaining a high energy density and a long cycle life. While lithium plating on graphite still remains a challenge, cathode degradation also plays a key role in battery performance. In this work, we used nano- and micro-X-ray computed tomography to characterize the mechanical degradation of LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) in optimized Li-ion batteries cycled at three rates, 1C, 6C, and 9C, and at different stages of cycle life, 225 and 600 cycles. We report despite using a conservative upper voltage cutoff limit aimed to minimize extensive cathode degradation, higher charging rates and increased cycling caused the polycrystalline NMC532 particles to fracture and pulverize, which likely drives cathode capacity fade and contributes to the decrease in overall cell performance.

25 ENERGY STORAGE↗

Exploring the Promise of Multifunctional “Zintl-Phase-Forming” Electrolytes for Si-Based Full Cells

Li-M-Si ternary Zintl phases have gained attention recently due to their high structural stability, which can improve the cycling stability compared to a bulk Si electrode. Adding multivalent cation salts (such as Mg 2+ and Ca 2+ ) in the electrolyte was proven to be a simple way to form Li-M-Si ternary phases in situ in Si-based Li-ion cells. To explore the promise of Zintl-phaseforming electrolytes, we systematically investigated their application in pouch cells via electrochemical and multiscale postmortem analysis. The introduction of multivalent cations, such as Mg 2+ , during charging can form Li x M y Si ternary phases. They can stabilize Si anions and reduce side reactions with electrolyte, improving the bulk stability. More importantly, Mg 2+ and Ca 2+ incorporate into interfacial side reactions and generate inorganic-rich solid- electrolyte interphase, thus enhancing the interfacial stability. Therefore, the full cells with Zintl-phase-forming electrolytes achieve higher capacity retentions at the C/3 rate after 100 cycles, compared to a baseline electrolyte. Additionally, strategies for mitigating the electrode-level fractures of Si were evaluated to make the best use of Zintl-phase-forming electrolytes. In conclusion, this work highlights the significance of synergistic impact of multifunctional additives to stabilize both bulk and interface chemistry in high-energy Si anode materials for Li-ion batteries.

25 ENERGY STORAGE↗

Simultaneous neutron and X-ray tomography for visualization of graphite electrode degradation in fast-charged lithium-ion batteries

Advanced battery characterization using neutron and X-ray-based imaging modalities is crucial to reveal fundamental degradation modes of lithium-ion batteries (LIBs). Taking advantage of the sensitivity of neutrons to some low-Z (Li) and X-rays to high-Z materials (Cu), here we demonstrate the viability of simultaneous neutron and X-ray tomography (NeXT) as a non-destructive imaging platform for ex-situ 3D visualization of graphite electrode degradation following extreme fast charging (XFC). In addition, we underscore the benefits of the simultaneous of NeXT by combining the neutron and X-ray tomography data from the same sample location for material identification and segmentation of one pristine and two XFC-cycled graphite electrodes (9C charge for 450 cycles). Our ex-situ results and methodology development pave the way for the design of NeXT-friendly LIB geometries that will allow operando and/or in-situ 3D visualization of electrode degradation during XFC.

25 ENERGY STORAGE↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Batteries (2021 Annual Progress Report)

This document summarizes the progress of VTO battery R&D projects supported during the fiscal year 2021 (FY 2021). In FY 2021, the DOE VTO battery R&D funding was approximately $\$$115 million. Its R&D focus was on the development of high-energy batteries for EVs as well as very high-power devices for hybrid vehicles. The electrochemical energy storage roadmap (which can be found at the EERE Roadmap web page2) describes ongoing and planned efforts to develop electrochemical storage technologies for EVs. To advance battery technology, which can in turn improve market penetration of PEVs, the program investigates various battery chemistries to overcome specific technical barriers, e.g., battery cost, performance, life (both the calendar life and the cycle life), its tolerance to abusive conditions, and its recyclability/sustainability. VTO R&D has had considerable success, lowering the cost of EV battery packs to $\$$185/kWh in 2019 (representing more than 80% reduction since 2008) yet even further cost reduction is necessary for EVs to achieve head-to-head cost competitiveness with ICEs (without Federal subsidies). In addition, today’s batteries also need improvements in such areas as their ability to accept charging at a high rate, referred to as extreme fast charging (XFC) (15 minute charge) – to provide a “refueling” convenience similar to ICEs, and the ability to operate adequately at low temperatures. Research into “next-gen lithium-ion” batteries which would provide such functionalities is one of the R&D focus areas. VTO is funding research on both “next gen” chemistries (which employ an alloy anode and/or a high voltage cathode) and beyond lithium-ion (BLI) chemistries (which can, for example, employ a lithium metal anode).

25 ENERGY STORAGE↗

The influence of temperature on area-specific impedance and capacity of Li-ion cells with nickel-containing positive electrodes

The temperature-dependent behaviors of five nickel-containing positive electrodes (NCA, NMC811, NMC622, NMC532, and NMC111) in lithium-ion batteries are investigated using an electrochemical protocol involving rate studies, mild aging (~100 cycles), and hybrid pulse power characterization (HPPC). Tests are conducted using coin-cells with graphite negative electrodes at -20 °C, 0 °C, 20 °C, and 40 °C. Three techniques are compared for determining the area-specific impedance (ASI): i) fits to the rate study average voltages, ii) fitting to the entire voltage curves using a regularization scheme, and iii) HPPC. When fit to an Arrhenius-type equation, all methods yield similar apparent activation energies (±2 kJ/mol) for the impedance, which range from -20 to -31 kJ/mol for the electrodes. Impedance growth increases with temperature but remains at less than 0.2% per cycle for most electrodes and temperatures. NCA and NMC811 are the exceptions, which yield 0.5% and 1.5% increases in ASI per cycle, respectively, at 40 °C. For cells with the same electrodes, the capacities are similar at 20 and 40 °C but reduce at lower temperatures, with up to a 52% reduction at -20 °C and 2C. The fade in energy of the cells during C/3 cycling is attributed to decreasing capacity as opposed to increasing ASI.

25 ENERGY STORAGE↗

Synthesis of high-density olivine LiFePO 4 from paleozoic siderite FeCO 3 and its electrochemical performance in lithium batteries

The lithium-ion cathode material olivine LiFePO 4 (LFP) has been synthesized for the first time from natural paleozoic iron carbonate (FeCO 3 ). The ferrous carbonate starting material consists of the mineral siderite at about 92 wt. % purity. Because FeCO 3 has divalent iron, the reaction with lithium dihydrogen phosphate (LiH 2 PO 4 ) provides a unique method to develop iron-(II) containing LFP in an inert atmosphere. Since siderite FeCO 3 is a common mineral that can be directly mined, it may, therefore, provide an inexpensive route for the production of LFP. After carbon-coating, the LFP yields a capacity in the range of 80–110 mAh g -1 LFP (in one chosen specimen sample), which is lower than commercially available LiFePO 4 (150–160 mAh g -1 LFP ). However, the tap density of LFP derived from siderite is noticeably high at 1.65 g cm -3 . The material is likely to be improved with powder purification, nanosized processing, and more complete carbon-coating coverage with increased optimization.

36 MATERIALS SCIENCE↗