Striated composite layers of silica and hafnia offering advantageous properties for short-pulse optical coatings

Monolayers containing subnanometer striations of silica and hafnia to form composite materials at varying ratios are explored as a method to develop high-index dielectric layers with increased laser-induced–damage thresholds (LIDTs). These layers can then be used in multilayer dielectric coatings for short-pulse, high-peak-power laser applications, particularly in regions of the highest electric-field intensity. Fabrication is achieved by means of exposure to two different evaporant vapor plumes, where local exposure to each plume is controlled via shielding to prevent simultaneous exposure. The LIDT of the resulting layers has been evaluated at 1053 nm with 600-fs pulses. The results indicate that such hafnia/silica layers exhibit LIDTs similar to silica for a refractive index of ≤1.65. These results suggest that the use of these layers in locations subjected to high electric-field intensity within multilayer dielectric coatings may significantly improve the LIDT, with this deposition process providing particular benefit for scaling to large-aperture, high-fluence components.

36 MATERIALS SCIENCE↗

Broadband, 920-nm mirror thin film damage competition

This year’s competition proposed to survey the state-of-the-art broadband, near-IR multilayer dielectric (MLD) mirrors designed for ultra-short, pulsed laser applications. The requirements for the coatings were a minimum reflection of 99.5% at 45-degree incidence angle for S-polarization from 830 nm to 1010 nm and group delay dispersion (GDD) < ± 50 fs 2 . The participants in this effort selected the coating materials, coating design, and deposition method. Samples were damage tested at a single testing facility to enable direct comparison among the participants using a 25 ± 5 fs OPCPA laser system operating at 5 Hz. A double blind test assured sample and submitter anonymity. The damage performance results, sample rankings, details of the deposition processes, coating materials and substrate cleaning methods are shared here. We found that multilayer coatings using tantala and/or hafnia as high index materials were top performers within several coating deposition groups. Specifically, dense coatings by ion-beam sputtering (IBS), magnetron sputtering (MS), and electron-beam ion assisted deposition (e-beam IAD) exhibited highest damage initiation onset (LIDT) while e-beam coatings were low performers. In addition, damage growth onset (LDGT) was also examined and the results are reported here for all samples as this performance metric plays an important role in establishing the safe operational conditions for larger aperture, ultrashort pulsed lasers. As a result, not all coating samples in the survey met the GDD requirements stated above and associated measurements are discussed in the context of the present and past competitions focused on similar broadband, near-IR MLD coatings.

42 ENGINEERING↗

Performance characterization of freeform finished surfaces of potassium dihydrogen phosphate using fluid jet polishing with a nonaqueous slurry

Abstract Potassium dihydrogen phosphate (KDP) and its deuterated analog (DKDP) are unique nonlinear optical materials for high power laser systems. They are used widely for frequency conversion and polarization control by virtue of the ability to grow optical-quality crystals at apertures suitable for fusion-class laser systems. Existing methods for freeform figuring of KDP/DKDP optics do not produce surfaces with sufficient laser-induced–damage thresholds (LIDT’s) for operation in the ultraviolet portion of high-peak-power laser systems. In this work, we investigate fluid jet polishing (FJP) using a nonaqueous slurry as a sub-aperture finishing method for producing freeform KDP surfaces. This method was used to selectively polish surface areas to different depths on the same substrate with removals ranging from 0.16 μm to 5.13 μm. The finished surfaces demonstrated a slight increase in roughness as the removal depth increased along with a small number of fracture pits. Laser damage testing with 351 nm, 1 ns pulses demonstrated excellent surface damage thresholds, with the highest values in areas devoid of fracture pits. This work demonstrates, for the first time, a method that enables fabrication of a waveplate that provides tailored polarization randomization that can be scaled to meter-sized optics. Furthermore, this method is based on FJP technology that incorporates a nonaqueous slurry specially designed for use with KDP. This novel nonaqueous FJP process can be also used for figuring other types of materials that exhibit similar challenging inherent properties such as softness, brittleness, water-solubility, and temperature sensitivity.

36 MATERIALS SCIENCE↗

Multiparameter laser performance characterization of liquid crystals for polarization control devices in the nanosecond regime

Abstract Interactions of liquid crystals (LC’s) with polarized light have been studied widely and have spawned numerous device applications, including the fabrication of optical elements for high-power and large-aperture laser systems. Currently, little is known about both the effect of incident polarization state on laser-induced–damage threshold (LIDT) and laser-induced functional threshold (LIFT) behavior at sub-LIDT fluences under multipulse irradiation conditions. This work reports on the first study of the nanosecond-pulsed LIDT’s dependence on incident polarization for several optical devices employing oriented nematic and chiral-nematic LC’s oriented by surface alignment layers. Accelerated lifetime testing was also performed to characterize the ability of these devices to maintain their functional performance under multipulse irradiation as a function of the laser fluence at both 1053 nm and 351 nm. Results show that the LIDT varies as a function of input polarization by 30–80% within the same device, while the multipulse LIFT (which can differ from the nominal LIDT) depends on irradiation conditions such as laser fluence and wavelength.

47 OTHER INSTRUMENTATION↗

Methods and apparatus for comprehensive characterization of performance attributes and damage thresholds of ultrafast laser optics

It is presently well understood that the operational performance limits of optics are determined by three fundamental attributes: the initiation of laser-induced damage, the growth of damage sites, and the transient (nondamaging) modification of optical parameters. The comprehensive characterization of the performance limitations of ultrafast optics requires consideration of all three fundamental attributes. Here, the vast majority of literature to date, however, has focused primarily on damage-initiation and testing systems that are largely focused on determining the damage-initiation threshold under single- and multipulse excitation. In this work, we discuss a testing apparatus that was designed to offer the capability to adequately characterize all three of these performance attributes under femtosecond, near-infrared laser irradiation. Key aspects of methodology are discussed, including high-dynamic-range energy control, variable beam size, wavelength tunability, B-integral management, and functional performance characterization to explore the true operational limits of the components. Example results for a metal-dielectric mirror demonstrate the test station’s operation.

42 ENGINEERING↗