Search NASA⌕ Search

Engineering topics

Kang, S -H

Publications and source records attributed to Kang, S -H.

Study of Li{sub 1+x}(Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9}){sub 1-x}O{sub 2} cathode materials for vehicle battery applications.

Li{sub 1+x}(Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9}){sub 1-x}O{sub 2} with two lithium content (x = 0 and 0.05) has been synthesized using coprecipitated (Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9})(OH){sub 2} and their electrochemical properties have been investigated. Compared with the x = 0 material, the lithium-rich material (x = 0.05) exhibited superior electrochemical properties. When cycled between 2.5 and 4.4 V, the Li/Li{sub 1.05}(Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9}){sub 0.95}O{sub 2} cells showed high first-cycle coulombic efficiency (93%), reversible discharge capacity of 187 mAh/g at C/12 with 99% capacity retention after 40 cycles, and excellent rate performance (86% of C/12 rate at 5 C discharge current). The Li{sub 1.05}(Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9}){sub 0.95}O{sub 2} electrode also showed a full-cell pulse power characteristics (5 C discharge pulse) comparable to Li{sub 1.05}(Mn{sub 1/3}Co{sub 1/3}Ni{sub 1/3}){sub 0.95}O{sub 2} electrode and better thermal stability at charged state (4.4 V) than charged LiNi{sub 0.8}Co{sub 0.15}Al{sub 0.05}O{sub 2} (4.2 V). Using a battery design and cost model developed in-house, calculations found battery packs with Li{sub 1.05}(Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9}){sub 0.95}O{sub 2} as the positive electrode to be of lower cost and higher energy density than those with LiNi{sub 0.8}Co{sub 0.15}Al{sub 0.05}O{sub 2} and Li{sub 1.05}(Mn{sub 1/3}Co{sub 1/3}Ni{sub 1/3}){sub 0.95}O{sub 2} electrodes. The experimental and modeling results obtained in this work suggest Li{sub 1.05}(Mn{sub 4/9}Co{sub 1/9}Ni{sub 4/9}){sub 0.95}O{sub 2} to be a promising cathode material for vehicle battery applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structural Complexity of Layered-spinel Composite Electrodes for Li-ion Batteries

The complexity of layered-spinel yLi{sub 2}MnO{sub 3} {center_dot} (1-y)Li{sub 1+x}Mn{sub 2-x}O{sub 4} (Li:Mn = 1.2:1; 0 = x = 0.33; y = 0.45) composites synthesized at different temperatures has been investigated by a combination of x-ray diffraction (XRD), x-ray absorption spectroscopy (XAS), and nuclear magnetic resonance (NMR). While the layered component does not change substantially between samples, an evolution of the spinel component from a high to a low lithium excess phase has been traced with temperature by comparing with data for pure Li{sub 1+x}Mn{sub 2-x}O{sub 4}. The changes that occur to the structure of the spinel component and to the average oxidation state of the manganese ions within the composite structure as lithium is electrochemically removed in a battery have been monitored using these techniques, in some cases in situ. Our 6Li NMR results constitute the first direct observation of lithium removal from Li{sub 2}MnO{sub 3} and the formation of LiMnO{sub 2} upon lithium reinsertion.

25 ENERGY STORAGE↗

Li{sub 2}O removal from Li{sub 5}FeO{sub 4} - a cathode precursor for lithium-ion batteries.

Lithium has been extracted both electrochemically and chemically from the defect antifluorite-type structure, Li{sub 5}FeO{sub 4} (5Li{sub 2}O {center_dot} Fe{sub 2}O{sub 3}). The electrochemical data show that four lithium ions can be removed from Li{sub 5}FeO{sub 4} between 3.5 and 4.5 V. vs Li{sup 0}. X-ray absorption spectroscopy (XAS) data of electrochemically delithiated samples show evidence of some Fe{sup 3+} to Fe{sup 4+} oxidation during the initial charge. On the other hand, XAS data of chemically delithiated samples show no evidence of Fe{sup 3+} to Fe{sup 4+} oxidation, but rather a change in coordination of the Fe{sup 3+} ions from tetrahedral to octahedral coordination, suggesting that lithium extraction from Li{sub 5}FeO{sub 4} is accompanied predominantly by the release of oxygen, the net loss being lithia (Li{sub 2}O); the residual lithium-iron-oxide product has a Fe{sub 2}O{sub 3}-rich composition. The high lithium content in Li{sub 5}FeO{sub 4} renders it an attractive cathode precursor for loading the graphite (C{sub 6}) anode of lithium-ion electrochemical cells with sufficient lithium to enable the discharge of a charged component in the parent cathode, Li{sub 1.2}V{sub 3}O{sub 8}, as well as the residual Fe{sub 2}O{sub 3}-rich component. The electrochemical behavior of C{sub 6}/Li{sub 5}FeO{sub 4}?Li{sub 1/2}V{sub 3}O{sub 8} lithium-ion cells is compared to C{sub 6}/Li{sub 2}MnO{sub 3}?Li{sub 1.2}V{sub 3}O{sub 8} cells containing a layered Li{sub 2}MnO{sub 3} (Li{sub 2}O {center_dot} MnO{sub 2}) cathode precursor with a lower Li{sub 2}O content, from which lithia can be extracted at higher potentials, typically >4 V vs metallic lithium. The ability to remove Li{sub 2}O electrochemically from metal oxide host structures with a high lithium content, such as Li{sub 5}FeO{sub 4}, has implications for Li-air cells.

74 ATOMIC AND MOLECULAR PHYSICS↗

Enhancing the rate capability of high capacity xLi{sub 2}MnO{sub 3} {sm_bullet} (1-x)LiMO{sub 2} (M=Mn, Ni, Co) electrodes.

The rate capability of high capacity xLi{sub 2}MnO{sub 3} {center_dot} (1 - x)LiMO{sub 2} (M = Mn, Ni, Co) electrodes for lithium-ion batteries has been significantly enhanced by stabilizing the electrode surface by reaction with a Li-Ni-PO{sub 4} solution, followed by a heat-treatment step. Reversible capacities of 250 mAh/g at a C/11 rate, 225 mAh/g at C/2 and 200 mAh/g at C/1 have been obtained from 0.5Li{sub 2}MnO{sub 3} {center_dot} 0.5LiNi{sub 0.44}Co{sub 0.25}Mn{sub 0.31}O{sub 2} electrodes between 4.6 and 2.0 V. The data bode well for their implementation in batteries that meet the 40-mile range requirement for plug-in hybrid vehicles.

25 ENERGY STORAGE↗

Examining the solid electrolyte interphase on binder-free graphite electrodes.

The solid electrode interphase (SEI) on graphite electrodes is important to the performance, calendar life, and safety characteristics of lithium-ion cells. This article examines the SEI formed on binder-free graphite electrodes prepared by electrophoretic deposition. X-ray photoelectron spectroscopy, Fourier transform infrared spectroscopy, and thermogravimetric analysis data were obtained on electrodes cycled in cells containing four electrolytes comprising ethylene carbonate: ethylmethyl carbonate (3:7 by weight) solvent and 1.2 M LiPF{sub 6}, 1 M LiF{sub 2}BC{sub 2}O{sub 4}, 1 M LiBF{sub 4}, or 0.7 M LiB(C{sub 2}O{sub 4}){sub 2} salt. Our observations suggest that, in addition to solvent reduction, the reduction of electrolyte salts plays an important role in SEI formation. Mechanisms to account for the formation of these SEI constituents are included in the article.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗