Role of Si on the Diffusional Interactions between U-Mo and Al-Si Alloys at 823 K (550 degrees C)

U-Mo dispersions in Al-alloy matrix and monolithic fuels encased in Al-alloy are under development to fulfill the requirements for research and test reactors to use low-enriched molybdenum stabilized uranium alloys fuels. Significant interaction takes place between the U-Mo fuel and Al during manufacturing and in-reactor irradiation. The interactions products are Al-rich phases with physical and thermal characteristics that adversely affect fuel performance and lead to premature failure. Detailed analysis of the interdiffusion and microstructural development of this system was carried through diffusion couples consisting of U-7wt.%Mo, U-10wt.%Mo and U-12wt.%Mo in contact with pure Al, Al-2wt.%Si, and Al-5wt.%Si, annealed at 823K for 1, 5 and 20 hours. Scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were employed for the analysis. Diffusion couples consisting of U-Mo vs. pure Al contained UAl3, UAl4, U6Mo4Al43, and UMo2Al20 phases. The addition of Si to the Al significantly reduced the thickness of the interdiffusion zone. The interdiffusion zones developed Al and Si enriched regions, whose locations and size depended on the Si and Mo concentrations in the terminal alloys. In the couples, the (U,Mo)(Al,Si)3 phase was observed throughout interdiffusion zone, and the U6Mo4Al43 and UMo2Al20 phases were observed only where the Si concentrations were low.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

TEM Characterization of U-7Mo/Al-2Si Dispersion Fuel Irradiated to Intermediate and High Fission Densities

This paper will discuss the results of TEM analysis that was performed on two samples taken from the low flux and high flux sides of the fuel plate with U-7Mo fuel particles dispersed in U-2Si matrix. The corresponding local fission density of the fuel particles and the peak fuel plate centerline temperature between the low flux and high flux samples are 3.32 x 10{sup 27} f/m{sup 3} and 90 C, and 6.31 x 10{sup 27} f/m{sup 3} and 120 C, respectively. The results of this work showed the presence of a bubble superlattice within the U-7Mo grains that accommodated fission gases (e.g., Xe). The presence of this structure helps the U-7Mo exhibit a stable swelling behavior during irradiation. The Si-rich interaction layers that develop around the fuel particles at the U-7Mo/matrix interface during fuel plate fabrication and irradiation become amorphous during irradiation. The change in bubble distribution at the high fission density suggests that the bubble superlattice is stable as the U-7Mo matrix remains crystalline. It appears that there is a threshold Si content in the fuel particle above which the U-Mo turns to amorphous under irradiation. The threshold Si content is approximately 8 at.% and 4 at.% for low flux and high flux condition, respectively.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural Analysis of Irradiated U-Mo Fuel Plates: Recent Results

Microstructural characterization of irradiated dispersion and monolithic RERTR fuel plates using scanning electron microscopy (SEM) is being performed in the Electron Microscopy Laboratory at the Idaho National Laboratory. The SEM analysis of samples from U-Mo dispersion fuel plates focuses primarily on the behavior of the Si that has been added to the Al matrix to improve the irradiation performance of the fuel plate and on the overall behavior of fission gases (e.g., Xe and Kr) that develop as bubbles in the fuel microstructure. For monolithic fuel plates, microstructural features of interest, include those found in the U-Mo foil and at the U-Mo/Zr and Zr/6061 Al cladding interfaces. For both dispersion and monolithic fuel plates, samples have been produced using an SEM equipped with a Focused Ion Beam (FIB). These samples are of very high quality and can be used to uncover some very unique microstructural features that are typically not observed when characterizing samples produced using more conventional techniques. Overall, for the dispersion fuel plates with matrices that contained Si, narrower fuel/matrix interaction layers are typically observed compared to the fuel plates with pure Al matrix, and for the monolithic fuel plates microstructural features have been observed in the U-10Mo foil that are similar to what have been observed in the fuel particles found in U-Mo dispersion fuels. Most recently, more prototypic monolithic fuel samples have been characterized and this paper describes the microstructures that have been observed in these samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure of the Irradiated U3Si2/Al Silicide Dispersion Fuel

The silicide dispersion fuel of U3Si2/Al is recognized as the best performance fuel for many nuclear research and test reactors with up to 4.8 gU/cm3 for low-enriched uranium fuel (LEU, 235U < 20%). An irradiated U3Si2/Al dispersion fuel (235U {approx}75%) from the high flux side of a fuel plate (U0R040) from the Reduced Enrichment for Research and Test Reactors (RERTR)-8 test was characterized using transmission electron microscopy (TEM). The fuel was irradiated in the Advanced Test Reactor (ATR) for 105 days. The average irradiation temperature and fission density of the U3Si2 fuel particles for the TEM sample are estimated to be approximately 110 C and 5.4 x 1027 f/m3. The characterization was performed using a 200 kV TEM. Detailed microstructural information along with composition analysis is obtained. The results and their implication on the performance of the U3Si2/Al silicide dispersion fuel are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase Constituents and Microstructure of Interaction Layer Formed in U-Mo Alloys vs Al Diffusion Couples Annealed at 873 K (600°C)

U-Mo dispersion and monolithic fuels are being developed to fulfill the requirements for research reactors, under the Reduced Enrichment for Research and Test Reactors program. In dispersion fuels, particles of U-Mo alloys are embedded in the Al-alloy matrix, while in monolithic fuels, U-Mo monoliths are roll bonded to the Al-alloy matrix. In this study, interdiffusion and microstructural development in the solid-to-solid diffusion couples, namely, U-15.7 at. pct Mo (7 wt pct Mo) vs pure Al, U-21.6 at. pct Mo (10 wt pct Mo) vs pure Al, and U-25.3 at. pct Mo (12 wt pct Mo) vs pure Al, annealed at 873 K (600 degrees C) for 24 hours, were examined in detail. Scanning electron microscopy (SEM), transmission electron microscopy (TEM), and electron probe microanalysis (EPMA) were employed to examine the development of a very fine multiphase interaction layer with an approximately constant average composition of 80 at. pct Al. Extensive TEM was carried out to identify the constituent phases across the interaction layer based on selected area electron diffraction and convergent beam electron diffraction (CBED). The cubic-UAl3, orthorhombic-UAl4, hexagonal-U6Mo4Al43, and cubic-UMo2Al20 phases were identified within the interaction layer that included two- and three-phase layers. Residual stress from large differences in molar volume, evidenced by vertical cracks within the interaction layer, high Al mobility, Mo supersaturation, and partitioning toward equilibrium in the interdiffusion zone were employed to describe the complex microstructure and phase constituents observed. A mechanism by compositional modification of the Al alloy is explored to mitigate the development of the U6Mo4Al43 phase, which exhibits poor irradiation behavior that includes void formation and swelling.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

RECENT DEVELOPMENT IN TEM CHARACTERIZATION OF IRRADIATED RERTR FUELS

The recent development on TEM work of irradiated RERTR fuels includes microstructural characterization of the irradiated U-10Mo/alloy-6061 monolithic fuel plate, the RERTR-7 U-7Mo/Al-2Si and U-7Mo/Al-5Si dispersion fuel plates. It is the first time that a TEM sample of an irradiated nuclear fuel was prepared using the focused-ion-beam (FIB) lift-out technical at the Idaho National Laboratory. Multiple FIB TEM samples were prepared from the areas of interest in a SEM sample. The characterization was carried out using a 200kV TEM with a LaB6 filament. The three dimensional orderings of nanometer-sized fission gas bubbles are observed in the crystalline region of the U-Mo fuel. The co-existence of bubble superlattice and dislocations is evident. Detailed microstructural information along with composition analysis is obtained. The results and their implication on the performance of these fuels are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructure of RERTR Du-Alloys Irradiated with Krypton Ions up to 100 dpa

The radiation stability of the interaction product formed at the fuel–matrix interface of research reactor dispersion fuels, under fission-product bombardment, has a strong impact on fuel performance. Three depleted uranium alloys were cast that consisted of the following five phases to be investigated: U(Si, Al)3, (U, Mo)(Si, Al)3, UMo2Al20, U6Mo4Al43, and UAl4. Irradiation of transmission electron microscopy (TEM) disc samples with 500-keV Kr ions at 200 °C to doses up to 100 displacements per atom (dpa) were conducted using a 300-keV electron microscope equipped with an ion accelerator. TEM results show that the U(Si, Al)3 and UAl4 phases remain crystalline at 100 dpa without forming voids. The (U, Mo)(Si, Al)3 and UMo2Al20 phases become amorphous at 1 and 2 dpa, respectively, and show no evidence of voids at 100 dpa. The U6Mo4Al43 phase goes to amorphous at less than 1 dpa and reveals high density voids at 100 dpa.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of Interaction Layer in U-Mo-X (X = Nb, Zr) and U-Nb-Zr vs. Al Diffusion Couples Annealed at 600 Degrees C for 10 Hours

U-Mo has thus far proven to be one of the most feasible metallic fuel alloys for use in research and test reactors due to its high density and stability during irradiation. However, an adverse diffusional interaction can occur between the fuel alloy and the Al based matrix. This forms an interaction layer (IL) that has undesirable thermal properties and irradiation behavior leading to accelerated swelling and reduced fuel efficiency. This study focused on the effects of ternary alloying additions on the formation of IL between U based alloys and Al. Diffusion couples of U-8Mo-3Nb, U-7Mo-6Zr, and U-10Nb-4Zr (wt.%) vs. pure Al were assembled and annealed at 600 Degrees C for 10 hours. Both thickness and phase constituent analyses were performed via electron microscopy. The major phase constituent of the IL was determined to be the UAl3 intermetallic compound. The Nb and Zr alloying additions did not reduce growth rate of IL (1.3-1.4 {mu}m/sec1/2) as compared to couples made between binary U-Mo and Al (0.9-1.8 {mu}m/sec1/2).

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Microstructural Analysis of As-Processed U-10 wt% Mo Monolithic Fuel Plate in AA6061 Matrix with Zr Diffusion Barrier

For higher U-loading in low-enriched U-10wt.%Mo fuels, monolithic fuel plate clad in AA6061 is being developed as a part of Reduced Enrichment for Research and Test Reactor (RERTR) program. This paper reports the first characterization results from a monolithic U- 10wt.%Mo fuel plate with a Zr diffusion barrier that was fabricated as part of a plate fabrication campaign for irradiation testing in the Advanced Test Reactor (ATR). Both scanning and transmission electron microscopy (SEM and TEM) were employed for analysis. At the interface between the Zr barrier and U-10wt.%Mo, going from Zr-to-U(Mo), UZr2, ?-UZr, Zr solidsolution and Mo2Zr phases were observed. The interface between AA6061 cladding and Zr barrier plate consisted of four layers, going from Al-to-Zr, (Al,Si)2Zr, (Al,Si)Zr3 (Al,Si)3Zr, and AlSi4Zr5. Irradiation behavior of these intermetallic phases is discussed based on their constituents. Characterization of as-fabricated phase constituents and microstructure would help understand the irradiation behavior of these fuel plates, interpret post-irradiation examination, and optimize the processing parameters of monolithic fuel system.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural Characterization of U-Nb-Zr, U-Mo-Nb, and U-Mo-Ti Alloys via Electron Microscopy

Ternary uranium molybdenum alloys are currently being investigated for use as dispersion and monolithic nuclear fuels in research reactors. In this study, two such ternary alloys, with compositions U-8Mo-3Nb and U-7Mo-3Ti in wt.%, were examined using scanning electron microscopy (SEM), X-ray diffraction (XRD), and transmission electron microscopy (TEM) with high angle annular dark field (HAADF) imaging via scanning transmission electron microscopy (STEM) to identify phase constituents. These alloys were homogenized at 950°C for 96 hours and were expected to be single-phase bcc-!-U. However, upon examination, it was determined that despite homogenization, each of the alloys contained a small volume fraction precipitate phase. Through SEM and XRD, it was confirmed that the matrix retained the bcc-!-U phase, but the precipitate phases could not be identified using these methods. TEM specimens were prepared using site-specific focused ion beam (FIB) in situ lift out (INLO) technique to include at least one precipitate from each alloy. By electron diffraction, the precipitate phases for the U- 8Mo-3Nb and U-7Mo-3Ti alloys were identified as bcc-(Mo,Nb) solid solution and bcc- (Mo,Ti) solid solution, respectively.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of an Irradiated RERTR-7 Fuel Plate Using Transmission Electron Microscopy

Transmission electron microscopy (TEM) has been used to characterize an irradiated fuel plate with Al-2Si matrix from the RERTR-7 experiment that was irradiated under moderate reactor conditions. The results of this work showed the presence of a bubble superlattice within the U-7Mo grains that accommodated fission gases (e.g., Xe). The presence of this structure helps the U-7Mo exhibit a stable swelling behaviour during irradiation. Furthermore, TEM analysis showed that the Si-rich interaction layers that develop around the fuel particles at the U-7Mo/matrix interface during fuel plate fabrication and irradiation become amorphous during irradiation, and in regions of the interaction layer that have relatively high Si concentrations the fission gas bubbles remain small and contained within the layer but in areas with lower Si concentrations the bubbles grow in size. An important question that remains to be answered about the irradiation behaviour of U-Mo dispersion fuels, is how do more aggressive irradiation conditions affect the behaviour of fission gases within the U-7Mo fuel particles and in the amorphous interaction layers on the microstructural scale that can be characterized using TEM? This paper discusses the results of TEM analysis that was performed on a sample taken from an irradiated RERTR-7 fuel plate with Al-2Si matrix. This plate was exposed to more aggressive irradiation conditions than was the sample taken from the RERTR-6 plate. The microstructural features present within the U-7Mo and the amorphous interaction layers will be discussed. The results of this analysis will be compared to what was observed in the earlier RERTR-6 fuel plate characterization.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SEM Characterization of an Irradiated Monolithic U-10Mo Fuel Plate

Results of scanning electron microscopy (SEM) characterization of irradiated U-7Mo dispersion fuel plates with differing amounts of matrix Si have been reported. However, to date, no results of SEM analysis of irradiated U-Mo monolithic fuel plates have been reported. This paper describes the first SEM characterization results for an irradiated monolithic U-10Mo fuel plate. Two samples from this fuel plate were characterized. One sample was produced from the low-flux side of the fuel plate, and another was produced at the high-flux side of the fuel plate. This characterization focused on the microstructural features present at the U-10Mo foil/cladding interface, particularly the interaction zone that had developed during fabrication and irradiation. In addition, the microstructure of the foil itself was investigated, along with the morphology of the observed fission gas bubbles. It was observed that a Si-rich interaction layer was present at the U-10Mo foil/cladding interface that exhibited relatively good irradiation behavior, and within the U-10Mo foil the microstructural features differed in some respects from what is typically seen in the U-Mo powders of an irradiated dispersion fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Transmission Electron Microscopy Characterization of Irradiated U-7Mo/Al-2Si Dispersion Fuel

The plate-type dispersion fuels, with the atomized U(Mo) fuel particles dispersed in the Al or Al alloy matrix, are being developed for use in research and test reactors worldwide. It is found that the irradiation performance of a plate-type dispersion fuel depends on the radiation stability of the various phases in a fuel plate. Transmission electron microscopy was performed on a sample (peak fuel mid-plane temperature approximately 109 degrees C and fission density approximately 4.5 x 10 27 fm-3) taken from an irradiated U–7Mo dispersion fuel plate with Al–2Si alloy matrix to investigate the role of Si addition in the matrix on the radiation stability of the phase(s) in the U–7Mo fuel/matrix interaction layer. A similar interaction layer that forms in irradiated U–7Mo dispersion fuels with pure Al matrix has been found to exhibit poor irradiation stability, likely as a result of poor fission gas retention. The interaction layer for both U–7Mo/Al–2Si and U–7Mo/Al fuels is observed to be amorphous. However, unlike the latter, the amorphous layer for the former was found to effectively retain fission gases in areas with high Si concentration. When the Si concentration becomes relatively low, the fission gas bubbles agglomerate into fewer large pores. Within the U–7Mo fuel particles, a bubble superlattice ordered as fcc structure and oriented parallel to the bcc metal lattice was observed where the average bubble size and the superlattice constant are approximately 3.5 nm and approximately 7.5 nm, respectively. The estimated fission gas inventory in the bubble superlattice correlates well with the fission density in the fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase Constituents of Al-rich U-Mo-Al Alloys Examined by Transmission Electron Microscopy

To supplement the understanding of diffusional interactions involving Al-rich region of the U-Mo-Al system, alloys with composition 85.7Al-11.44U-2.86Mo and 87.5Al-10U-2.5Mo in at.%, were examined to determine the equilibrium phase constituents at 500?C. These alloys were triple arc-melted, homogenized at 500?C for 200 hours, and water-quenched to preserve the high temperature microstructure. X-ray diffraction, scanning electron microscopy (SEM) with energy dispersive x-ray spectroscopy (XEDS), and transmission electron microscopy (TEM) with high angle annular dark field (HAADF) imaging via scanning transmission electron microscopy (STEM) were employed for the characterization. Alloy specimens for TEM/STEM were prepared using site-specific focused ion beam (FIB) in-situ lift-out (INLO) technique. Despite the homogenization time and temperature, five different phases, namely fcc-Al solid solution, cubic-UAl3, orthorhombic-UAl4, hexagonal-U6Mo4Al43 and diamond cubic-UMo2Al20, were observed. Based on U-Al, U-Mo and Al-Mo binary phase diagrams, previously proposed U-Mo-Al isotherms, and the solidification microstructure of these alloys, the Al-rich region of the equilibrium ternary isotherm at 500?C was constructed. The fcc-Al solid solution, orthorhombic-UAl4, and diamond cubic-UMo2Al20, which were determined to be the equilibrium phases in 85.7Al-11.44U-2.86Mo and 87.5Al-10U-2.5Mo alloys.

99 GENERAL AND MISCELLANEOUS↗

SEM and TEM Characterization of As-Fabricated U-7Mo Disperson Fuel Plates

The starting microstructure of a dispersion fuel plate can have a dramatic impact on the overall performance of the plate during irradiation. To improve the understanding of the as-fabricated microstructures of dispersion fuel plates, SEM and TEM analysis have been performed on RERTR-9A archive fuel plates, which went through an additional hot isostatic procsssing (HIP) step during fabrication. The fuel plates had depleted U-7Mo fuel particles dispersed in either Al-2Si or 4043 Al alloy matrix. For the characterized samples, it was observed that a large fraction of the ?-phase U-7Mo alloy particles had decomposed during fabrication, and in areas near the fuel/matrix interface where the transformation products were present significant fuel/matrix interaction had occurred. Relatively thin Si-rich interaction layers were also observed around the U-7Mo particles. In the thick interaction layers, (U)(Al,Si)3 and U6Mo4Al43 were identified, and in the thin interaction layers U(Al,Si)3, U3Si3Al2, U3Si5, and USi1.88-type phases were observed. The U3Si3Al2 phase contained some Mo. Based on the results of this work, exposure of dispersion fuel plates to relatively high temperatures during fabrication impacts the overall microstructure, particularly the nature of the interaction layers around the fuel particles. The time and temperature of fabrication should be carefully controlled in order to produce the most uniform Si-rich layers around the U-7Mo particles.

99 GENERAL AND MISCELLANEOUS↗

Interdiffusion in Diffusion Couples: U-Mo v. Al and Al-Si

Interdiffusion and microstructural development in the U-Mo-Al system was examined using solid-tosolid diffusion couples consisting of U-7wt.%Mo, U-10wt.%Mo and U-12wt.%Mo vs. pure Al, annealed at 600°C for 24 hours. The influence of Si alloying addition (up to 5 wt.%) in Al on the interdiffusion microstructural development was also examined using solid-to-solid diffusion couples consisting of U-7wt.%Mo, U-10wt.%Mo and U-12wt.%Mo vs. pure Al, Al-2wt.%Si, and Al-5wt.%Si annealed at 550°C up to 20 hours. Scanning electron microscopy (SEM), transmission electron microscopy (TEM) and electron probe microanalysis (EPMA) were employed to examine the development of a very fine multiphase intermetallic layer. In ternary U-Mo-Al diffusion couples annealed at 600°C for 24 hours, interdiffusion microstructure varied of finely dispersed UAl3, UAl4, U6Mo4Al43, and UMo2Al20 phases while the average composition throughout the interdiffusion zone remained constant at approximately 80 at.% Al. Interdiffusion microstructure observed by SEM/TEM analyses and diffusion paths drawn from concentration profiles determined by EPMA appear to deviate from the assumption of “local thermodynamic equilibrium,” and suggest that interdiffusion occurs via supersaturated UAl4 followed by equilibrium transformation into UAl3, U6Mo4Al43, UAl4 and UMo2Al20 phases. Similar observation was made for U-Mo vs. Al diffusion couples annealed at 550°C. The addition of Si (up to 5 wt.%) in Al significantly reduced the thickness of the intermetallic layer by changing the constituent phases of the interdiffusion zone developed in U-Mo vs. Al-Si diffusion couples. Specifically, the formation of (U,Mo)(Al,Si)3 with relatively large solubility for Mo and Si, along with UMo2Al20 phases was observed along with disappearance of U6Mo4Al43 and UAl4 phases. Simplified understanding based on U-Al, U-Si, and Mo-Si binary phase diagrams is discussed in the light of the beneficial effect of Si alloying addition.

99 GENERAL AND MISCELLANEOUS↗