Differentiating Zr/Hf IV Aqueous Polyoxocation Chemistry with Peroxide Ligation
Not provided.
Engineering topics
Publications and source records attributed to Keszler, Douglas A..
Not provided.
Not Available
Thin films formed by the condensation of metal oxo–hydroxo clusters offer a promising approach to ultrahigh-resolution patterning including next-generation photolithography using extreme ultraviolet (EUV) radiation and electron-beam lithography. In this work, we elucidate the thermal and radiative mechanisms that drive the chemical transformations in these materials and therefore control the patterning performance. Beginning from aqueous hafnium clusters, peroxide and sulfate additions serve to modify the clusters and, upon spin coating to form a thin film, provide the chemical contrast necessary to create resist. The coordination and functionality of peroxide and sulfate in hafnium-based metal oxo–hydroxo clusters were monitored at various stages of the patterning process which provided insight into the chemical and structural evolution of the material. Peroxide serves as the radiation sensitive species while sulfate enhances solubility and controls the concentration of hydroxide in the films. In conclusion, peroxide and hydroxide species decompose via radiative and thermal energy, respectively, to form hafnium oxide; controlling these processes is central to the function of the resist.
Fast, refined models of amorphous IGZO are made possible by new pair potentials, convergence tests and X-ray total scattering show.
The atomic solid state energy (SSE) scale originates from a plot of the electron affinity (EA) and ionization potential (IP) versus band gap (E{sub G}). SSE is estimated for a given atom by assessing an average EA (for a cation) or an average IP (for an anion) for binary inorganic compounds having that specific atom as a constituent. Physically, SSE is an experimentally-derived average frontier orbital energy referenced to the vacuum level. In its original formulation, 69 binary closed-shell inorganic semiconductors and insulators were employed as a database, providing SSE estimates for 40 elements. In this contribution, EA and IP versus E{sub G} are plotted for an additional 92 compounds, thus yielding SSE estimates for a total of 64 elements from the s-, p-, d-, and f-blocks of the periodic table. Additionally, SSE is refined to account for its dependence on oxidation state. Although most cations within the SSE database are found to occur in a single oxidation state, data are available for nine d-block transition metals and one p-block main group metal in more than one oxidation state. SSE is deeper in energy for a higher cation oxidation state. Two p-block main group non-metals within the SSE database are found to exist in both positive and negative oxidation states so that they can function as a cation or anion. SSEs for most cations are positioned above −4.5 eV with respect to the vacuum level, and SSEs for all anions are positioned below. Hence, the energy −4.5 eV, equal to the hydrogen donor/acceptor ionization energy ε(+/−) or equivalently the standard hydrogen electrode energy, is considered to be an absolute energy reference for chemical bonding in the solid state. - Highlights: • Atomic solid-state energies are estimated for 64 elements from experimental data. • The relationship between atomic SSEs and oxidation state is assessed. • Cations are positioned above and absolute energy of −4.5 eV and anions below.
Abstract not provided
We demonstrate generation and characterization of crystalline bismuth thin film from triphenyl bismuth in methanol. Upon ultraviolet (267 nm) femtosecond laser irradiation of the solution, a thin film of elemental bismuth forms on the inner side of the sample cuvette, confirmed by detection of the coherent A{sub 1g} optical phonon mode of crystalline bismuth at ∼90 cm{sup −1}. Probe pulses at 267 and 400 nm are used to elucidate the excited state potential energy surface and photochemical reaction coordinate of triphenyl bismuth in solution with femtosecond resolution. The observed phonon mode blueshifts with increasing irradiation time, likely due to the gradual thickening of nascent bismuth thin film to ∼80 nm in 90 min. From transient absorption with the 400 nm probe, we observe a dominant ∼4 ps decay time constant of the excited-state absorption signal, which is attributed to a characteristic metal-ligand bond-weakening/breaking intermediate enroute to crystalline metallic thin film from the solution precursor molecules. Our versatile optical setup thus opens an appealing avenue to characterize the laser-induced crystallization process in situ and prepare high-quality thin films and nanopatterns directly from solution phase.
Explore the source record for details and available documents.
A comparison was made of Al{sub 2}O{sub 3} films deposited on Si via prompt inorganic condensation (PIC) and atomic layer deposition (ALD). Current–voltage measurements as a function of annealing temperature indicate that the solution-processed PIC films, annealed at 500 °C, exhibit lower leakage and roughly equivalent breakdown strength in comparison to ALD films. PIC films are less dense than as-deposited ALD films and capacitance–voltage measurements indicate a lower relative dielectric constant. On the basis of x-ray photoelectron spectroscopy, transmission electron microscopy, and energy dispersive x-ray spectroscopy, it is found that the 500 °C anneal results in the formation of a ∼6 nm thick interfacial SiO{sub 2} layer at the Si interface. This SiO{sub 2} interfacial layer significantly affects the electrical performance of PIC Al{sub 2}O{sub 3} films deposited on Si.
Explore the source record for details and available documents.
Abstract not provided
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.