Water-gas shift: Characterization and testing of nanoscale YSZ supported Pt catalysts

Nano-scale Y-doped zirconium oxide materials were prepared with high surface areas (150-200 m(2)/g) and small nano-crystallites (<8 nm). A combination of XANES and EXAFS was used to show that ZrO2 exhibited the tetragonal phase, while the Zr0.5Y0.5O1.75 support displayed the cubic phase. A comparison with undoped zirconia suggests that the Zr0.9Y0.1O1.95 support was tetragonal in structure. A slight increase in d-spacing observed in HR-TEM for the Zr0.9Y0.1O1.95 support relative to undoped ZrO2, along with a shift to lower 2 theta in XRD, provide evidence that Y-doping caused macrostrain. STEM imaging confirmed that the Pt clusters ranged from 0.5 to 2 nm over all three supports. Catalyst reducibility was explored by H-2-TPR, XANES at the Zr K-edge, and TPR-XANES at the Pt L-III edge. A higher concentration of surface defects for the 0.5%Pt/Zr0.9Y0.1O1.95 catalyst relative to 0.5%Pt/ZrO2 was confirmed by DRIFTS of adsorbed CO, while a greater surface mobility of surface formate was suggested based on forward formate decomposition experiments in steam. The Y-doped Pt promoted catalysts displayed higher water-gas-shift activity relative to the 0.5%Pt/ZrO2 catalyst when the Y content was at or below 50%, with the best catalyst being 0.5%Pt/Zr0.9Y0.1O1.95. (C) 2015 Elsevier B.V. All rights reserved.

Pt/YSZ↗

Substitutional Mechanism of Ni into the Wide-Band-Gap Semiconductor InTaO4 and its Implications for Water Splitting Activity in the Wolframite Structure Type

The mechanism of Ni substitution into the oxide semiconductor InTaO{sub 4} has been studied through a combination of structural and spectroscopic techniques, providing insights into its previously reported photoactivity. Magnetic susceptibility and X-ray absorption near-edge spectroscopy (XANES) measurements demonstrate that nickel is divalent within the host lattice. The combined refinement of synchrotron X-ray and neutron powder diffraction data indicates that the product of Ni doping has the stoichiometry of (In{sub 1-x}Ni{sub 2x/3}Ta{sub x/3})TaO{sub 4} with a solubility limit of x {approx} 0.18, corresponding to 12% Ni on the In site. Single-phase samples were only obtained at synthesis temperatures of 1150 C or higher due to the sluggish reaction mechanism that is hypothesized to result from small free energy differences between (In{sub 1-x}Ni{sub 2x/3}Ta{sub x/3})TaO{sub 4} compounds with different x values. Undoped InTaO{sub 4} is shown to have an indirect band gap of 3.96 eV, with direct optical transitions becoming allowed at photon energies in excess of 5.1 eV. Very small band-gap reductions (less than 0.2 eV) result from Ni doping, and the origin of the yellow color of (In{sub 1-x}Ni{sub 2x/3}Ta{sub x/3})TaO{sub 4} compounds instead results from a weak {sup 3}A{sub 2g} {yields} {sup 3}T{sub 1g} internal d {yields} d transition not associated with the conduction or valence band that is common to oxide compounds with Ni{sup 2+} in an octahedral environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fischer-Tropsch Synthesis: Influence of CO Conversion on Selectivities H2/CO Usage Ratios and Catalyst Stability for a 0.27 percent Ru 25 percent Co/Al2O3 using a Slurry Phase Reactor

The effect of CO conversion on hydrocarbon selectivities (i.e., CH{sub 4}, C{sub 5+}, olefin and paraffin), H{sub 2}/CO usage ratios, CO{sub 2} selectivity, and catalyst stability over a wide range of CO conversion (12-94%) on 0.27%Ru-25%Co/Al{sub 2}O{sub 3} catalyst was studied under the conditions of 220 C, 1.5 MPa, H{sub 2}/CO feed ratio of 2.1 and gas space velocities of 0.3-15 NL/g-cat/h in a 1-L continuously stirred tank reactor (CSTR). Catalyst samples were withdrawn from the CSTR at different CO conversion levels, and Co phases (Co, CoO) in the slurry samples were characterized by XANES, and in the case of the fresh catalysts, EXAFS as well. Ru was responsible for increasing the extent of Co reduction, thus boosting the active site density. At 1%Ru loading, EXAFS indicates that coordination of Ru at the atomic level was virtually solely with Co. It was found that the selectivities to CH{sub 4}, C{sub 5+}, and CO{sub 2} on the Co catalyst are functions of CO conversion. At high CO conversions, i.e. above 80%, CH{sub 4} selectivity experienced a change in the trend, and began to increase, and CO{sub 2} selectivity experienced a rapid increase. H{sub 2}/CO usage ratio and olefin content were found to decrease with increasing CO conversion in the range of 12-94%. The observed results are consistent with water reoxidation of Co during FTS at high conversion. XANES spectroscopy of used catalyst samples displayed spectra consistent with the presence of more CoO at higher CO conversion levels.

01 COAL, LIGNITE, AND PEAT↗

Fischer-Tropsch Synthesis: Characterization and Reaction Testing of Cobalt Carbide

Hydrogenation of carbon monoxide was investigated for cobalt carbide synthesized from Co{sub 3}O{sub 4} by CO carburization in a fixed-bed reactor. The cobalt carbide synthesized was characterized by BET surface area, X-ray diffraction, scanning electron microscopy, X-ray absorption near edge spectroscopy, and extended X-ray absorption fine structure spectroscopy. The catalysts were tested in the slurry phase using a continuously stirred tank reactor at P = 2.0 MPa, H{sub 2}/CO = 2:1 in the temperature range of 493-523 K, and with space velocities varying from 1 to 3 Nl h{sup -1} g{sub cat}{sup -1}. The results strongly suggest that a fraction of cobalt converts to a form with greater metallic character under the conditions employed. This was more pronounced on a Fischer-Tropsch synthesis run conducted at a higher temperature (523 versus 493 K).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Combined High Resolution XPS and EXAFS Study of Ag Photodissolution in a-As2S3

Changes of electronic and atomic structure during silver photodissolution in As{sub 2}S{sub 3} thin film are studied using a combination of high-resolution X-ray photoelectron spectroscopy (XPS) and extended X-ray absorption fine structure (EXAFS) methods. It is shown that the photodiffusion process starts already under the influence of Al K{sub {alpha}} and synchrotron X-ray probe radiations, forming a highly disordered metastable structure. Concurrent irradiation with UV/VIS light leads to the formation of a stable uniform ternary phase. The mechanisms of structural transformations and final chemical products are proposed. The influence of surface oxidation on the structure of Ag/As{sub 2}S{sub 3} bilayer is also investigated.

36 MATERIALS SCIENCE↗

Understanding the role of structural disorder on spin polarization in CeMnNi4 using XAFS

The role of disorder on ferromagnetism has generally been detrimental. We show how Mn-Ni antisite disorder enhances polarization in CeMnNi{sub 4}. The disorder is determined to be 6% by x-ray absorption fine structure. The electronic structure of pure CeMnNi{sub 4} is pseudo-half-metallic. Site exchange alters the near neighbor bond parameters and modifies the density of states favorably, increasing the polarization (obtained by first-principles calculations) from 13 to 47% (experimental {approx}66%).

36 MATERIALS SCIENCE↗

Quick extended x-ray absorption fine structure instrument with millisecond time scale, optimized for in situ applications

In order to learn about in situ structural changes in materials at subseconds time scale, we have further refined the techniques of quick extended x-ray absorption fine structure (QEXAFS) and quick x-ray absorption near edge structure (XANES) spectroscopies at beamline X18B at the National Synchrotron Light Source. The channel cut Si (111) monochromator oscillation is driven through a tangential arm at 5 Hz, using a cam, dc motor, pulley, and belt system. The rubber belt between the motor and the cam damps the mechanical noise. EXAFS scan taken in 100 ms is comparable to standard data. The angle and the angular range of the monochromator can be changed to collect a full EXAFS or XANES spectrum in the energy range 4.7-40.0 KeV. The data are recorded in ascending and descending order of energy, on the fly, without any loss of beam time. The QEXAFS mechanical system is outside the vacuum system, and therefore changing the mode of operation from conventional to QEXAFS takes only a few minutes. This instrument allows the acquisition of time resolved data in a variety of systems relevant to electrochemical, photochemical, catalytic, materials, and environmental sciences.

43 PARTICLE ACCELERATORS↗