Data for EMSL Project 47953 from March 2020
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Kim, Do Heui.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
The selective catalytic reduction of NOsub>x with NH 3 (NH 3 -SCR) at low temperatures is still a major challenge in environmental catalysis research. Metal oxide based catalysts have attracted great attention due to their excellent low-temperature activity. In this study, CeO 2 -supported cobalt (Co)-oxide with variable Co/Ce weight ratios were prepared by the incipient-wetness impregnation method. The effect of Co loading as well as the effect of temperature on catalytic behaviors have been studied for the NO reduction and NO oxidation reactions. Thorough characterization by means of BET, XRD, and Raman has shown the topological model of the catalyst and interpretation of the observed reactivity trends. The activity test of CoO x /CeO 2 catalysts showed that the addition of Co enhanced the activity of NO reduction as well as that of NO oxidation. The most active catalyst with 10 wt% Co loading showed 70% NO reduction and 85% NO oxidation activity. Catalyst characterization results indicated that Co was monodispersed on ceria surface with the low Co loading amount, while Co 3 O 4 was formed on ceria with high Co loading amounts that affected the overall catalytic activity.
Not Available
The effects of K loading and thermal aging on the structural properties and high temperature performance of Pt/K/Al2O3 lean NOx trap (LNT) catalysts were investigated using in situ X-ray diffraction (XRD), temperature-programmed decomposition/desorption of NOx (NOx-TPD), transmission electron microscopy (TEM), NO oxidation and NOx storage tests. In situ XRD results demonstrate that KNO3 becomes extremely mobile on the Al2O3 surface, and experiences complex transformations between orthorhombic and rhombohedral structures, accompanied by sintering, melting and thermal decomposition upon heating. NOx storage results show an optimum K loading around 10% for the best performance at high temperatures. At lower K loadings where the majority of KNO3 stays as a surface layer, the strong interaction between KNO3 and Al2O3 promotes KNO3 decomposition and deteriorates high-temperature performance. At K loadings higher than 10%, the performance drop is not caused by NOx diffusion limitations as for the case of barium-based LNTs, but rather from the blocking of Pt sites by K species, which adversely affects NO oxidation. Thermal aging at 800 ºC severely deactivates the Pt/K/Al2O3 catalysts due to Pt sintering. However, in the presence of potassium, some Pt remains in a dispersed and oxidized form. These Pt species interact strongly with K and, therefore, do not sinter. After a reduction treatment, these Pt species remain finely dispersed, contributing to a partial recovery of NOx storage performance.
We have investigated nitrate formation and decomposition processes, and measured NOx storage performance on Pt-K2O/Al2O3 catalysts as a function of potassium loading. After NO2 adsorption at room temperature, ionic and bidentate nitrates were observed by fourier transform infra-red (FTIR) spectroscopy. The ratio of the former to the latter species increased with increasing potassium loading up to 10 wt%, and then stayed almost constant with additional K, demonstrating a clear dependence of loading on the morphology of the K species. Although both K2O(10)/Al2O3 and K2O(20)/Al2O3 samples have similar nitrate species after NO2 adsorption, the latter has more thermally stable nitrate species as evidenced by FTIR and NO2 temperature programmed desorption (TPD) results. With regard to NOx storage performance, the temperature of maximum NOx uptake (Tmax) is 573 K up to a potassium loading of 10 wt%. As the potassium loading increases from 10 wt% to 20 wt%, Tmax shifted from 573 K to 723 K. Moreover, the amount of NO uptake (38 cm3 NOx/g catal) at Tmax increased more than three times, indicating that efficiency of K in storing NOx is enhanced significantly at higher temperature, in good agreement with the NO2 TPD and FTIR results. Thus, a combination of characterization and NOx storage performance results demonstrates an unexpected effect of potassium loading on nitrate formation and decomposition processes; results important for developing Pt-K2O/Al2O3 for potential applications as high temperature NOx storage-reduction catalysts.
Two primary NOx after-treatment technologies have been recognized as the most promising approaches for meeting stringent NOx emission standards for diesel vehicles within the Environmental Protection Agency’s (EPA’s) 2007/2010 mandated limits, NOx Storage Reduction (NSR) and NH3 selective catalytic reduction (SCR); both are, in fact being commercialized for this application. However, in looking forward to 2015 and beyond with expected more stringent regulations, the continued viability of the NSR technology for controlling NOx emissions from lean-burn engines such as diesels will require at least two specific, significant and inter-related improvements. First, it is important to reduce system costs by, for example, minimizing the precious metal content while maintaining, even improving, performance and long-term stability. A second critical need for future NSR systems, as well as for NH3 SCR, will be significantly improved higher and lower temperature performance and stability. Furthermore, these critically needed improvements will contribute significantly to minimizing the impacts to fuel economy of incorporating these after-treatment technologies on lean-burn vehicles. To meet these objectives will require, at a minimum an improved scientific understanding of the following things: i) the various roles for the precious and coinage metals used in these catalysts; ii) the mechanisms for these various roles; iii) the effects of high temperatures on the active metal performance in their various roles; iv) mechanisms for higher temperature NOx storage performance for modified and/or alternative storage materials; v) the interactions between the precious metals and the storage materials in both optimum NOx storage performance and long term stability; vi) the sulfur adsorption and regeneration mechanisms for NOx reduction materials; vii) materials degradation mechanisms in CHA-based NH3 SCR catalysts. The objective of this CRADA project between PNNL and Cummins, Inc. is to develop a fundamental understanding of the above-listed issues. Model catalysts that are based on literature formulations are the focus of the work being carried out at PNNL. In addition, the performance and stability of more realistic high temperature NSR catalysts, supplied by JM, are being studied in order to provide baseline data for the model catalysts that are, again, based on formulations described in the open literature. For this short summary, we will primarily highlight representative results from our recent studies of the stability of candidate high temperature NSR materials.
We investigate the effects of initial sulfur loadings on the desulfation chemistry and the subsequent final activity of a commercial LNT catalyst. Identical total amounts of SO2 are applied to the samples, albeit with the frequency of desulfation varied. The results indicate that performance is better with less frequent desulfations. The greater the amount of sulfur deposited before desulfation, the more amount of SO2 evolution before H2S is observed during desulfation, which can be explained by two sequential reactions; initial conversion of sulfate to SO2, followed by the reduction of SO2 to H2S. After completing all sulfation/desulfation steps, the sample with only a single desulfation results in a fairly uniform sulfur distribution along the z-axis inside of the monolith. We expect that the results obtained in this study will provide useful information for optimizing regeneration strategies in vehicles that utilize the LNT technology.
Mesoporous materials synthesized from commercial ferrierite (MMZ-FER) were applied to butanol dehydration. The MMZ-FER was produced by disassembling ferrierite into unit structures in the presence of an alkali solution, adding a surfactant as a templating material, followed by hydrothermal treatment. The effect of the alkali/(Si+Al) ratio in the disassembling step on the characteristics of the catalyst and butanol dehydration performance were investigated. The MMZ-FER materials, synthesized in a condition in which the NaOH/(Si + Al) mole ratio in the disassembling step was 0.67 and 1.0, demonstrated similar textural properties to those of MCM-41. Many weak acid sites developed on the MMZ-FER(0.67) and MMZ-FER(1.0) samples, which is attributed to the creation of ferrierite-induced acid sites. The MMZ-FER materials showed excellent catalytic activity, selectivity, and stability during the dehydration of 2-butanol.
Multiple catalytic functions (NOx conversion, NO and NH3 oxidation, NH3 storage) of a commercial Cu-zeolite urea/NH3-SCR catalyst were assessed in a laboratory fixed-bed flow reactor system after differing degrees of hydrothermal aging. Catalysts were characterized by using x-ray diffraction (XRD), 27Al solid state nuclear magnetic resonance (NMR) and transmission electron microscopy (TEM) / energy dispersive X-ray (EDX) spectroscopy to develop an understanding of the degradation mechanisms during catalyst aging. The catalytic reaction measurements of laboratory-aged catalysts were performed, which allows us to obtain a universal curve for predicting the degree of catalyst performance deterioration as a function of time at each aging temperature. Results show that as the aging temperature becomes higher, the zeolite structure collapses in a shorter period of time after an induction period. The decrease in SCR performance was explained by zeolite structure destruction and/or Cu agglomeration, as detected by XRD/27Al NMR and by TEM/EDX, respectively. Destruction of the zeolite structure and agglomeration of the active phase also results in a decrease in the NO/NH3 oxidation activity and the NH3 storage capacity of the catalyst. Selected laboratory aging conditions (16 h at 800oC) compare well with a 135,000 mile vehicle-aged catalyst for both performance and characterization criteria.
The hydrothermal stability of Cu/beta NH3 SCR catalysts are explored here. In particular, this paper focuses on the interesting ability of this catalyst to maintain and even enhance high-temperature performance for the "standard" SCR reaction after modest (900 °C, 2 hours) hydrothermal aging. Characterization of the fresh and aged catalysts was performed with an aim to identify possible catalytic phases responsible for the enhanced high temperature performance. XRD, TEM and 27Al NMR all showed that the hydrothermally aging conditions used here resulted in almost complete loss of the beta zeolite structure between 1 and 2 hours aging. While the 27Al NMR spectra of 2 and 10 hour hydrothermally-aged catalysts showed significant loss of a peak associated with tetrahedrally-coordinated Al species, no new spectral features were evident. Two model catalysts, suggested by these characterization data as possible mimics of the catalytic phase formed during hydrothermal aging of Cu/beta, were prepared and tested for their performance in the "standard" SCR and NH3 oxidation reactions. The similarity in their reactivity compared to the 2 hour hydrothermally-aged Cu/beta catalyst suggests possible routes for preparing multi-component catalysts that may have wider temperature windows for optimum performance than those provided by current Cu/zeolite catalysts.
Currently precious metal-based diesel oxidation catalysts (DOC) containing platinum (Pt) and palladium (Pd) are most commonly used for the oxidation of hydrocarbon and NO in diesel exhaust hydrocarbon oxidation. The present work has been carried out to investigate the deactivation mechanisms of the DOC from its real-world vehicle operation by coupling its catalytic activity measurements with surface characterization including x-ray diffraction, transmission electron microscopy, and x-ray photoelectron spectroscopy. A production Pt-Pd DOC was obtained after being aged on a vehicle driven for 135,000 miles in order to study its deactivation behavior. The performance of the vehicle-aged part was correlated with that of the simulated hydrothermal lab aged sample assuming that Pt-Pd sintering plays a major role in irreversible catalyst deactivation. In addition to the hydrothermal sintering, the deterioration of hydrocarbon and NO oxidation performance was caused by surface poisoning. The role of the various aging factors in determining long-term performance in mobile applications will be discussed.
We report the various characteristics of Pt-K/MgAl{sub 2}O{sub 4} lean NOx trap (LNT) catalysts including the effect of K loading on nitrate formation/decomposition, NOx storage activity and durability. Upon the adsorption of NO{sub 2} on K/MgAl{sub 2}O{sub 4} samples, potassium nitrates formed on Mg-related sites in MgAl{sub 2}O{sub 4} support are observed, in addition to the typical two potassium nitrates (ionic and bidentate) formed also on Al{sub 2}O{sub 3} supported sample. Based on NO{sub 2} TPD and FTIR results, the Mg-bound KNO{sub 3} thermally decompose at higher temperature than Al-bound KNO{sub 3}, implying its superior thermal stability. At a potassium loading of 5wt%, the temperature of maximum NOx uptake (T{sub max}) is 300 C. Increasing the potassium loading from 5wt% to 10 wt%, the T{sub max} gradually shifted from 300 C to 450 C, indicating the dependence of T{sub max} on the potassium loading. However, increase in potassium loading above 10 wt% only gives rise to the reduction in the overall NOx storage capacity. This work also underlines the obstacles these materials have prior to their practical application (e.g., durability and sulfur poisoning/ removal). This work provides fundamental understanding of Pt-K/MgAl{sub 2}O{sub 4}-based lean NOx trap catalysts, which could be good candidates for high temperature LNT applications.
The structural and chemical characteristics of Pt/BaO lean-NO{sub x} trap (LNT) catalysts supported on {gamma}-Al{sub 2}O{sub 3} and MgAl{sub 2}O{sub 4} are compared in this study. The Pt-BaO/MgAl{sub 2}O{sub 4} sample shows relatively low NO{sub x} uptake at temperatures below 300 C, and the temperature of maximum NO{sub x} uptake (T{sub max}) is shifted to 350 C in comparison to that of Pt-BaO/Al{sub 2}O{sub 3} (T{sub max} {approx}250 C). More importantly, the NO{sub x} uptake over the MgAl{sub 2}O{sub 4}-supported catalyst at 350 C is twice that of the alumina-based one. The shift toward the higher temperature NO{sub x} uptake is explained by the larger interfacial area between Pt and BaO, due to smaller Pt clusters as evidenced by TEM and Pt L3 EXAFS. In situ TR-XRD results demonstrate that the formation of a BaAl{sub 2}O{sub 4} phase in the BaO/MgAl{sub 2}O{sub 4} LNT catalyst occurs at a temperature about 100 C higher than on BaO/Al{sub 2}O{sub 3}, which may also represent a beneficial attribute of the BaO/MgAl{sub 2}O{sub 4} LNT with respect to catalyst stability.
DOE FY 2011 Advanced Combustion Technologies Annual Report. CLEERS is a research and development focus project of the Diesel Cross-Cut Team. The overall objective is to promote the development of improved computational tools for simulating realistic full-system performance of lean-burn engines and the associated emissions control systems. Three fundamental research projects are sponsored at PNNL through CLEERS: DPF, SCR, and LNT. Resources are shared between the three efforts in order to actively respond to current industrial needs. In FY 2011, more emphasis was placed on the SCR and LNT activities because of urgent application issues associated with these technologies. Objectives of this project are to lead and contribute to the Cross-Cut Lean Exhaust Emissions Reduction Simulations (CLEERS) activities - (a) Provide project updates to the industry sub-team, solicit feedback, and adjust work scope accordingly; and (b) Lead technical discussions, invite distinguished speakers, and maintain an open dialogue on selective catalytic reduction (SCR), lean-NOx trap (LNT), and diesel particulate filter (DPF) modeling issues. Fiscal Year (FY) 2011 Objectives are to: (1) Develop improved modeling capabilities for SCR and DPFs through fundamental experiments; and (2) Develop a fundamental understanding of SCR and LNT catalysts with primary focus on reaction mechanisms and material characterization. Some accomplishments are: (1) Participated in monthly CLEERS teleconferences and coordinated the calls focused on SCR, LNT and DPF technologies; (2) Updated PNNL's SCR model for the state-of-the-art commercial Cu-zeolite SCR catalyst to extract kinetic parameters and to quantitatively describe the effects of hydrothermal aging; (3) Examined the effects of hydrothermal aging on the physicochemical properties and SCR reactions using the commercial Cu catalyst in collaboration with Oak Ridge National Laboratory (ORNL); (4) Investigated the nature of Cu species and obtained kinetic parameters for small-pore zeolite-based Cu SCR catalyst. (5) Examined the effects of support materials for Ba-based LNT catalysts, and found magnesium aluminate may improve the oxides of nitrogen (NO{sub x}) reduction performance at high temperatures; (6) Investigated soot oxidation mechanisms for relevant oxidants (O{sub 2}, NO{sub 2}) through reactor experiments and transmission electron spectroscopy (TEM) analysis; (7) Seven publications and 21 public presentations (eight invited) during the past FY; and (8) Co-organized sessions on emission control and modeling for the SAE World Congress and the American Society of Mechanical Engineers Internal Combustion Engine Conference.