Search NASA⌕ Search

Engineering topics

Kuo, Helen A.

Publications and source records attributed to Kuo, Helen A..

Unraveling the Ion Adsorption Kinetics in Microporous Carbon Electrodes: A Multiscale Quantum-Continuum Simulation and Experimental Approach

With the understanding that sorption in porous carbon electrodes is crucial to many environmental and energy technologies, such as capacitive deionization (CDI), supercapacitor energy storage, and activated carbon filters. In each of these examples, a practical model that can describe ion electrosorption kinetics is highly desirable for accelerating material design. Here, we proposed a multiscale model to study the ion electrosorption kinetics in porous carbon electrodes by combining quantum mechanical simulations with continuum approaches. Our model integrates the Butler-Volmer (BV) equation for sorption kinetics and a continuously stirred tank reactor (CSTR) formulation with atomistic calculations of ion hydration and ion-pore interactions based on density functional theory (DFT). We validated our model experimentally by using ion mixtures in a flow-through electrode CDI device and developed an in-line UV absorption system to provide unprecedented resolution of individual ions in the separation process. We showed that the multiscale model captures unexpected experimental phenomena that cannot be explained by the traditional ion electrosorption theory. The proposed multiscale framework provides a viable approach for modeling separation processes in systems where pore sizes and ion hydration effects strongly influence the sorption kinetics, which can be leveraged to explore possible strategies for improving carbon-based and, more broadly, pore-based technologies

36 MATERIALS SCIENCE↗

Understanding resistances in capacitive deionization devices

The desalination characteristics of capacitive deionization (CDI) are significantly impacted by the cell resistance. Here we apply electrochemical impedance spectroscopy (EIS) to analyze the resistive properties of a CDI device, which include EIS measurements on a complete assembled cell (in two wire mode) and EIS measurements with additional contacts to decouple electrode/electrolyte and contact impedances (four wire mode). These measurements shed light on the interface between current collector and electrode as well as the internal capacitive and resistive elements of the cell. With two-wire and four-wire EIS measurements, we find that the often observed high-frequency arc(s) in the impedance spectra can be due to contact effects and/or an internal ionic-transfer resistance that is locally in parallel with macropore wall capacitance. In some cases, the two associated arcs in the Nyquist plot are overlapping and present simultaneously, making their identification in the EIS spectra difficult unless both two-wire and four-wire measurements are made. Despite causing a large high-frequency arc in the Nyquist plot, we find that the apparent internal ionic-transfer resistance is negligible compared to the resistances of the electrode, separator, and external electronic components. Here, an investigation of the contact impedance between the electrode and current collector reveals a parallel RC arc that can grow over time if an improper material is used (e.g., titanium). In our system, the electrode ionic resistance dominates the total Ohmic power dissipation, which has implications for scale-up of CDI systems and future improvements of cell design.

36 MATERIALS SCIENCE↗