Search NASA⌕ Search

Engineering topics

Lamneck, J. H.

Publications and source records attributed to Lamneck, J. H..

Photon-degradation effects in terrestrial silicon solar cells

The effect of instability in terrestrial solar cells and identification of mechanisms involved are presented. The effect is similar to photon-induced degradation in radiation-damaged space solar cells, with reduction in cell output in n(+)/p cells upon exposure to illumination or upon the application of a sufficiently high forward bias. It was found that the photon-degradation effect is caused by a recombination center identified as a complex of a lattice defect and a silver atom or cluster of atoms. The center is electrically inactive in its ground state but can be activated by raising the minority-carrier quasi-Fermi level to coincide with the position of the latent-center level in the band gap, or by direct excitation of electrons from the valence band to the latent-center level. Photon degradation can be prevented by avoiding the introduction of silver through the use of a clean diffusion system and clean initial material, or by eliminating lattice damage by sufficient surface material removal prior to diffusion and restricting diffusion temperatures to 875 C or below.

Weizer, V. G.↗

Photon degradation effects in terrestrial solar cells

A certain type of photon degradation effect has been observed experimentally in n(+)/p solar cells. It is found that this effect is caused by a recombination center, the formation of which requires the simultaneous presence of a lattice defect and a silver atom or complex of atoms. The center is electrically active in its equilibrium state; the energy level of the inactive center is located in the band gap, 0.37 eV below the conduction band. Conversion to an active recombination center can be brought about either by raising the minority carrier quasi-Fermi level to coincide with the position of the latent center level in the band gap or by the direct excitation of electrons from the valence band to the latent center level. Photon degradation can be prevented either by preventing the introduction of silver through the use of a clean diffusion system and clean initial material or by eliminating lattice damage through sufficient surface material removal prior to diffusion while at the same time restricting diffusion temperatures to 875 C or below.

Weizer, V. G.↗

Advances in the theory and application of BSF cells

The characteristics and behavior of p(+), p solar cells were investigated. The p(+), p cells were made by the removal of the n(+) surface layers from n(+), p p(+), BSF cells followed by application of a suitable contact to the resultant p(+), p structures. The open circuit voltage of p(+), p cells was found to increase with increasing 'p' bulk resistivity. The measured open circuit velocity-temperature coefficients were positive and increased with increasing resistivity. An outline of prior limitations in solar cell design is presented, and the removal of these limitations through use of BSF effects is pointed out. The study of BSF effects made feasible production of very thin high efficiency silicon cells as well as high resistivity-high efficiency cells, two desirable types of silicon cells which were previously impossible to make.

Mandelkorn, J.↗

Advances in the theory and application of BSF cells

A study to determine the influence of fabrication processes and bulk material properties on the behavior of back surface field (BSF) cells is reported. It is concluded that a photovoltage is generated at the p(+), p back junction of the cell. The concept of majority carrier collection is proposed as a possible mechanism for this generation. Advantages accruing to the advent of BSF cells are outlined.

Mandelkorn, J.↗

Design, fabrication and characteristics of new types of back surface field cells

Several new types of back surface field (BSF) cells were designed and fabricated. These include boron and phosphorus diffused BSF cells, single crystal epitaxially grown BSF cells and chemically vapor deposited (CVD) polycrystalline BSF cells. Boron diffusion yielded 10 ohm-cm BSF cells with 0.6 volt open-circuit voltages and collection efficiencies equal to those previously reported for aluminum alloying. The epitaxially grown cells also exhibited high open-circuit voltages and collection efficiencies and may be more radiation damage resistant. The polycrystalline cells had very high internal series resistance. No direct relationship was found to exist between collection efficiency and open-circuit voltage in BSF cells.

Mandelkorn, J.↗

Design, fabrication and characteristics of new types of back surface field cells

Several new types of back surface field (BSF) cells were designed and fabricated. These include boron and phosphorus diffused BSF cells, single crystal epitaxially grown BSF cells and chemically vapor deposited (CVD) polycrystalline BSF cells. Boron diffusion yielded 10 ohm-cm BSF cells with 0.6 volt open-circuit voltages and collection efficiencies equal to those previously reported for aluminum alloying. The epitaxially grown cells also exhibited high open-circuit voltages and collection efficiencies and may be more radiation damage resistant. The polycrystalline cells had very high internal series resistance. No direct relationship was found to exist between collection efficiency and open-circuit voltage, V sub oc in BSF cells. Results indicate that the V sub oc effect is not caused simply by the mechanism of blocking of minority carriers.

Mandelkorn, J.↗