Voltage waveform tailoring for high aspect ratio plasma etching of SiO 2 using Ar/CF 4 /O 2 mixtures: Consequences of low fundamental frequency biases

The use of non-sinusoidal waveforms in low pressure capacitively coupled plasmas intended for microelectronics fabrication has the goal of customizing ion and electron energy and angular distributions to the wafer. One such non-sinusoidal waveform uses the sum of consecutive harmonics of a fundamental sinusoidal frequency, f 0 , having a variable phase offset between the fundamental and even harmonics. In this paper, we discuss results from a computational investigation of the relation between ion energy and DC self-bias when varying the fundamental frequency f 0 for capacitively coupled plasmas sustained in Ar/CF 4 /O 2 and how those trends translate to a high aspect ratio etching of trenches in SiO 2 . The fundamental frequency, f 0 , was varied from 1 to 10 MHz and the relative phase from 0° to 180°. Two distinct regimes were identified. Average ion energy onto the wafer is strongly correlated with the DC self-bias at high f 0 , with there being a maximum at φ = 0° and minimum at φ = 180°. In the low frequency regime, this correlation is weak. Average ion energy onto the wafer is instead dominated by dynamic transients in the applied voltage waveforms, with a maximum at φ = 180° and minimum at φ = 0°. The trends in ion energy translate to etch properties. In both, the high and low frequency regimes, higher ion energies translate to higher etch rates and generally preferable final features, though behaving differently with phase angle.

36 MATERIALS SCIENCE↗

Voltage waveform tailoring for high aspect ratio plasma etching of SiO 2 using Ar/CF 4 /O 2 mixtures: Consequences of ion and electron distributions on etch profiles

The quality of high aspect ratio (HAR) features etched into dielectrics for microelectronics fabrication using halogen containing low temperature plasmas strongly depends on the energy and angular distribution of the incident ions (IEAD) onto the wafer, as well as potentially that of the electrons (EEAD). Positive ions, accelerated to high energies by the sheath electric field, have narrow angular spreads and can penetrate deeply into HAR features. Electrons typically arrive at the wafer with nearly thermal energy and isotropic angular distributions and so do not directly penetrate deeply into features. These differences can lead to positive charging of the insides of the features that can slow etching rates and produce geometric defects such as twisting. In this work, we computationally investigated the plasma etching of HAR features into SiO 2 using tailored voltage waveforms in a geometrically asymmetric capacitively coupled plasma sustained in an Ar/CF 4 /O 2 mixture at 40 mTorr. The tailored waveform consisted of a sinusoidal wave and its higher harmonics with a fundamental frequency of 1 MHz. We found that some degree of control of the IEADs and EEADs is possible by adjusting the phase of higher harmonics φ through the resulting generation of electrical asymmetry and electric field reversal. However, the IEADs and EEADs cannot easily be separately controlled. The control of IEADs and EEADs is inherently linked. The highest quality feature was obtained with a phase angle φ = 0° as this value generated the largest (most negative) DC self-bias and largest electric field reversal for accelerating electrons into the feature. That said, the consequences of voltage waveform tailoring (VWT) on etched features are dominated by the change in the IEADs. Although VWT does produce EEADs with higher energy and narrower angular spread, the effect of these electrons on the feature compared to thermal electrons is not large. Finally, this smaller impact of VWT produced EEADs is attributed to thermal electrons being accelerated into the feature by electric fields produced by the positive in-feature charging.

47 OTHER INSTRUMENTATION↗

Erosion of focus rings in capacitively coupled plasma etching reactors

In plasma etching reactors, the structure surrounding the wafer, often called a focus ring (FR), plays an important role in maintaining uniform fluxes of reactants across the wafer. The FR is typically made of dielectric materials. During the plasma etching process, the sheath that forms over the wafer to accelerate ions anisotropically into the surface extends over the FR. Electrical charging of the FR modifies the sheath relative to that over the wafer. On the one hand, one wants the sheath to be uniform across the wafer-FR boundary to enable uniform fluxes to the edge of the wafer. On the other hand, maintaining a high voltage sheath over the FR will erode the FR, which is undesirable as the FR is a consumable component that must be periodically replaced in high volume manufacturing. In this work, we computationally investigated the consequences of dielectric constant ε of the FR materials on erosion of the FR. The series capacitance of the FR and its underlying structure is typically smaller than that of the wafer and its underlying structure. As a result, the FR charges quickly relative to the wafer, which then reduces the voltage across the sheath on top of the FR. The ion energy and angular distributions (IEADs) striking the FR are, therefore, generally lower in energy with a broader angular distribution. With ε = 2, the ion energies striking the middle to the outer edge of the FR are 30–180 eV, whereas for ε = 100, the ion energies are 120–380 eV. At the transition between the wafer and the FR, there is a skew in the IEAD as large as 15° that results from the difference in sheath thickness above the wafer and the FR. This skew and the erosion rate across the FR are functions of the dielectric constant of the FR material. With low ε, the FR charges quickly, less plasma is produced above the FR, and there is less voltage across the sheath that results in less FR erosion. Increasing ε of the FR produces a higher sheath voltage as well as higher ion fluxes over the FR, which increases erosion, while the skew at the edge of the wafer is less severe. Further, the material of the subsurface portion of the FR, which dominates its capacitance, is an important consideration in the design of the substrate assembly.

36 MATERIALS SCIENCE↗

Electric field reversals resulting from voltage waveform tailoring in Ar/O 2 capacitively coupled plasmas sustained in asymmetric systems

The etching of nanometer scale high-aspect-ratio (HAR) features into dielectric materials in low pressure radio frequency excited plasmas is often accompanied by charge accumulation inside the features which can slow etching rates and produce distortions such as twisting. The intra feature charging is at least partially produced by differences in electron and ion energy and angular distributions (EADs). Positive ions, accelerated to high energies having narrow angular spreads by the sheath electric field, can penetrate deeply into HAR features. Electrons typically arrive at the wafer with nearly thermal and isotropic distributions and do not penetrate deeply into HAR features. These disparities lead to differential charging of the inside of the feature, which can lead to reductions in etch rate and feature distortion due to ion deflection. With in-creasing aspect ratio of features, charging challenges are expected to continue for the foreseeable future. In this work, the use of tailored voltage waveforms in geometrically asymmetric capacitively coupled plasmas sustained in Ar/O 2 at 40 mTorr was computationally investigated with the goal of shaping the EAD of electrons incident onto the substrate to address differential charging. The tailored waveform consisted of a sinusoidal wave and its higher harmonics with a fundamental frequency of 1 MHz. Further, we found that electric field reversals in the sheath and presheath can occur during the anodic portion of the cycle. The electric field reversal increases the energy and decreases the angular spread of electrons incident onto the substrate. The magnitude of the electric field reversal can be controlled by the phase angle of the even harmonics and the gas composition. Due to its electronegative nature, increasing mole fractions of O 2 impedes electron transport to the surface which further increases the electric field reversal.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗