Search NASA⌕ Search

Engineering topics

Lercher, Johannes A.

Publications and source records attributed to Lercher, Johannes A..

At least 55 records · Page 3

Critical role of solvent-modulated hydrogen-binding strength in the catalytic hydrogenation of benzaldehyde on palladium

Protic and non-protic solvents influence the rate of benzaldehyde hydrogenation on Pd by one order of magnitude in the following sequence of increasing reactivity, dioxane < tetrahydrofuran < water < methanol. Despite these differences, the reaction pathway does not change; the majority of turnovers occurs via a Langmuir-Hinshelwood mechanism by stepwise addition of sorbed H to sorbed benzaldehyde, first to the carbonyl O and then to the C atom of the formyl group, forming benzyl alcohol. An analysis of the solvation energies shows that both ground and transition states are destabilized by the solvents compared to the same reaction at the gas-solid interface. The destabilization extent of the reacting organic substrates in both states are similar and, therefore, compensate each other, making the net kinetic effects inconsequential. In consequence, the marked reactivity differences arise solely from the differences in the surface stabilization of adsorbed hydrogen adatoms moderated by the four solvents-more weakly bound hydrogen adatoms, because of their solvation by solvent, exhibit higher rates of their hydrogenation reaction in kinetically relevant attack on the C atom.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Copper-Based Catalysts Confined in Carbon Nanocage Reactors for Condensed Ester Hydrogenation: Tuning Copper Species by Confined SiO 2 and Methanol Resistance

Hydrogenation of aliphatic esters to natural alcohols is an important strategy for the efficient utilization of biomass-derived oils. The synthesis of highly active copper (Cu)-based catalysts is a challenge for condensed-phase ester hydrogenation due to the difficulties in controlling active sites and catalyst deactivation. In this work, a copper-based catalyst confined in a carbon nanocage reactor was successfully designed and prepared. The copper catalyst with 56 wt % SiO 2 exhibited the best performance because of the optimum proportion of Cu + and Cu 0 sites and high dispersion. The interaction between SiO 2 and Cu particles contributes to the formation of Cu + species, which is the key site for the adsorption of carbonyl groups. Meanwhile, the confinement effect of the carbon nanocages effectively inhibited the agglomeration of the copper particles. The catalysts exhibited not only excellent thermal stability but also superior methanol resistance in comparison with the Cu/SiO 2 catalyst. On the basis of the density functional theory (DFT) calculations results, methanol resistance should be attributed to the fewer hydroxyl groups on the catalyst surface, which increase the activation barrier for the dissociation of silica, allowing the stable holding of the copper species in the methanol solvent.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Back Cover: Influence of Intracrystalline Ionic Strength in MFI Zeolites on Aqueous Phase Dehydration of Methylcyclohexanols (Angew. Chem. Int. Ed. 47/2021)

Here the impact of the concentration of hydrated hydronium ions and in turn of the local ionic strength in MFI zeolites has been investigated for the aqueous phase dehydration of 4-methylcyclohexanol (E1 mechanism) and cis-2-methylcyclohexanol (E2 mechanism). The E2 pathway with the latter alcohol led to a 2.5-fold higher activity. The catalytic activity normalized to the hydronium ions (turnover frequency, TOF) passed through a pronounced maximum, which is attributed to the increasing excess chemical potential of the alcohols in the pores, increasing in parallel with the ionic strength and the additional work caused by repulsive interactions and charge separation induced by the bulky alcohols. While the maximum in rate observed is invariant with the mechanism or substitution, the reaction pathway is influencing the activation parameters differently.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Influence of Intracrystalline Ionic Strength in MFI Zeolites on Aqueous Phase Dehydration of Methylcyclohexanols

Abstract The impact of the concentration of hydrated hydronium ions and in turn of the local ionic strength in MFI zeolites has been investigated for the aqueous phase dehydration of 4‐methylcyclohexanol (E1 mechanism) and cis ‐2‐methylcyclohexanol (E2 mechanism). The E2 pathway with the latter alcohol led to a 2.5‐fold higher activity. The catalytic activity normalized to the hydronium ions (turnover frequency, TOF) passed through a pronounced maximum, which is attributed to the increasing excess chemical potential of the alcohols in the pores, increasing in parallel with the ionic strength and the additional work caused by repulsive interactions and charge separation induced by the bulky alcohols. While the maximum in rate observed is invariant with the mechanism or substitution, the reaction pathway is influencing the activation parameters differently.

Milaković, Lara↗

Influence of Intracrystalline Ionic Strength in MFI Zeolites on Aqueous Phase Dehydration of Methylcyclohexanols

Abstract The impact of the concentration of hydrated hydronium ions and in turn of the local ionic strength in MFI zeolites has been investigated for the aqueous phase dehydration of 4‐methylcyclohexanol (E1 mechanism) and cis ‐2‐methylcyclohexanol (E2 mechanism). The E2 pathway with the latter alcohol led to a 2.5‐fold higher activity. The catalytic activity normalized to the hydronium ions (turnover frequency, TOF) passed through a pronounced maximum, which is attributed to the increasing excess chemical potential of the alcohols in the pores, increasing in parallel with the ionic strength and the additional work caused by repulsive interactions and charge separation induced by the bulky alcohols. While the maximum in rate observed is invariant with the mechanism or substitution, the reaction pathway is influencing the activation parameters differently.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electronic impact of Ni2P nanoparticle size on hydrogenation rates

Nickle phosphide, Ni2P, nanoparticles supported on SiO2 show a marked volcano shaped size dependence. Kinetic analysis and physicochemical characterization shows the electron density of Ni to increase with increasing Ni2P size, enhancing in turn the H2 adsorption strength. For particles below 15 nm, H adsorbs weakly causing a low surface coverage of H, gradually increasing with particle size. For large particles, hydrogen binds too strongly causing a high coverage but low catalytic activity. The remarkable size dependence of the electronic properties show that Ni2P particle size can be used to fine-tune its activity for hydrogenation.

Ni2P size effect, Electron density, H2 adsorption ↗

Activity of Cu-Al-oxo extra-framework clusters for selective methane oxidation on Cu exchanged zeolites

Cu-zeolites are able to directly convert methane to methanol via a 3-step process using O2 as oxidant. Among the different zeolite topologies, Cu-exchanged mordenite (MOR) shows the highest methanol yields, attributed to a preferential formation of active Cu-oxo species in its 8-MR pores. The presence of extra-framework or partially detached Al species entrained in the micropores of MOR leads to the formation of nearly homotopic redox active Cu-Al-oxo nanoclusters with the ability to activate CH4. Studies of the activity of these sites together with characterization by 27Al NMR and IR spectroscopy leads to the conclusion that the active species are located in the 8-MR side pockets of MOR and it consists of two Cu ions and one Al linked by O. This Cu-Al oxo cluster shows an activity per Cu in methane oxidation significantly higher than of any previ-ously reported active Cu-oxo species. In order to determine unambiguously the structure of the active Cu-Al-oxo cluster, we combine experimental XANES of Cu K- and L- edges, Cu K-edge HERFD-XANES and Cu K-edge EXAFS with TDDFT and AIMD-assisted simulations. Our results provide evidence of a [Cu2AlO3]2+ cluster exchanged on MOR Al pairs that is able to oxidize up to two methane molecules per cluster at ambient pressure.

Methane oxidation, Cu L3-edge XANES, HERFD, TDDFT,↗

Role of the ionic environment in enhancing the activity of reacting molecules in zeolite pores

Tailoring the molecular environment around catalytically active site allows the enhancement of catalytic reactivity via a hitherto unexplored pathway. In zeolites, the presence of water creates an ionic environment via the formation of hydrated hydronium ions and the negatively charged framework Al tetrahedra. The high density of cation-anion pairs determined by the aluminum concentration of a zeolite induces a high local ionic strength that increases the excess chemical potential of sorbed and uncharged organic reactants. Charged transition states (as for example, the carbenium ions in the discussed alcohol dehydration) are stabilized, reducing the energy barrier and leading to a higher reaction rate. Using the intramolecular dehydration of cyclohexanol on H-MFI in water, we show quantitatively the enhancement of the reaction rate by the presence of high ionic strength as well as potential limitations of this strategy. The approach opens a new pathway to systematically enhance catalytic reactivity rates and has wide-ranging implications for understanding catalysis in condensed phase.

Pfriem, Niklas↗

Confinement effects and acid strength in zeolites

Chemical reactivity and sorption in zeolites are coupled to confinement and—to a lesser extent—to the acid strength of Brønsted acid sites (BAS). In presence of water the zeolite Brønsted acid sites eventually convert into hydronium ions. The gradual transition from zeolite Brønsted acid sites to hydronium ions in zeolites of varying pore size is examined by ab initio molecular dynamics combined with enhanced sampling based on Well-Tempered Metadynamics and a recently developed set of collective variables. While at low water content (1–2 water/BAS) the acidic protons prefer to be shared between zeolites and water, higher water contents (n > 2) invariably lead to solvation of the protons within a localized water cluster adjacent to the BAS. At low water loadings the standard free energy of the formed complexes is dominated by enthalpy and is associated with the acid strength of the BAS and the space around the site. Conversely, the entropy increases linearly with the concentration of waters in the pores, favors proton solvation and is independent of the pore size/shape.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Environment of Metal–O–Fe Bonds Enabling High Activity in CO 2 Reduction on Single Metal Atoms and on Supported Nanoparticles

Single-atom catalysts are often reported to have catalytic properties that surpass those of nanoparticles, while a direct comparison of sites common and different for both is lacking. In this work, we show that single atoms of the Pt-group embedded into the surface of Fe 3 O 4 have a greatly enhanced interaction strength with CO 2 compared with Fe 3 O 4 surface. The strong CO 2 adsorption on single Rh atoms and corresponding low activation energies lead to two-orders-of-magnitude higher conversion rates of CO 2 compared to Rh nanoparticles. This high activity of single atoms stems from the partially oxidic state imposed by their coordination to the support. Fe 3 O 4 -supported Rh nanoparticles follow the behavior of single atoms for CO 2 interaction and reduction, which is attributed to the dominating role of partially oxidic sites at the Fe 3 O 4 -Rh interface. Thus, we show a likely common catalytic chemistry for two kinds of materials thought to be different, and we show that single atoms of Pt-group metals on Fe 3 O 4 are an especially successful material for catalyzed reactions that depend primarily upon sites with the metal-O-Fe environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Differences in Mechanism and Rate of Zeolite-Catalyzed Cyclohexanol Dehydration in Apolar and Aqueous Phase

The rate of acid-base catalyzed dehydration of alcohols strongly depends on the solvent and the environment of the acid sites. In this work, we find that Brønsted acidic sites in large-pore zeolites, but not in medium-pore zeolites, catalyze cyclohexanol dehydration in decalin at significantly higher rates than hydrated hydronium ions in aqueous phase. Specifically, the difference in turnover rates between the two solvents amounts to two to three orders of magnitude on H-BEA and H-FAU, while being very modest (within a factor of 2) for H-MFI. Combining kinetic, isotopic tracer and 2H NMR measurements, it is established that cyclohexanol dehydration generally follows an E1-elimination pathway in decalin. A notable exception is the monomer dehydration route on H-MFI, which exhibits a much lower activation energy and a substantially negative activation entropy that appear to be associated with an E2-type mechanism. The C-O bond cleavage displays a dominant degree of rate control in decalin, which stands in contrast to deprotonation (C-H cleavage) being rate-limiting in aqueous-phase dehydration.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Zeolite-Stabilized Di- and Tetranuclear Molybdenum Sulfide Clusters Form Stable Catalytic Hydrogenation Sites

Supercages of faujasite (FAU)-type zeolites serve as a robust scaffold for stabilizing dinuclear (Mo 2 S 4 ) and tetranuclear (Mo 4 S 4 ) molybdenum sulfide clusters. The FAU-encaged Mo 4 S 4 clusters have a distorted cubane structure similar to the FeMo-cofactor in nitrogenase. Both clusters possess one unpaired electron per Mo atom. Additionally, they show identical catalytic activity per sulfide cluster. Their catalytic activity is stable (> 150 h) for ethene hydrogenation, while layered MoS 2 structures deactivate significantly under the same reaction conditions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Directing the Rate‐Enhancement for Hydronium Ion Catalyzed Dehydration via Organization of Alkanols in Nanoscopic Confinements

Abstract Alkanol dehydration rates catalyzed by hydronium ions are enhanced by the dimensions of steric confinements of zeolite pores as well as by intraporous intermolecular interactions with other alkanols. The higher rates with zeolite MFI having pores smaller than those of zeolite BEA for dehydration of secondary alkanols, 3‐heptanol and 2‐methyl‐3‐hexanol, is caused by the lower activation enthalpy in the tighter confinements of MFI that offsets a less positive activation entropy. The higher activity in BEA than in MFI for dehydration of a tertiary alkanol, 2‐methyl‐2‐hexanol, is primarily attributed to the reduction of the activation enthalpy by stabilizing intraporous interactions of the C β ‐H transition state with surrounding alcohol molecules. Overall, we show that the positive impact of zeolite confinements results from the stabilization of transition state provided by the confinement and intermolecular interaction of alkanols with the transition state, which is impacted by both the size of confinements and the structure of alkanols in the E1 pathway of dehydration.

Shetty, Manish↗

Directing the Rate‐Enhancement for Hydronium Ion Catalyzed Dehydration via Organization of Alkanols in Nanoscopic Confinements

Abstract Alkanol dehydration rates catalyzed by hydronium ions are enhanced by the dimensions of steric confinements of zeolite pores as well as by intraporous intermolecular interactions with other alkanols. The higher rates with zeolite MFI having pores smaller than those of zeolite BEA for dehydration of secondary alkanols, 3‐heptanol and 2‐methyl‐3‐hexanol, is caused by the lower activation enthalpy in the tighter confinements of MFI that offsets a less positive activation entropy. The higher activity in BEA than in MFI for dehydration of a tertiary alkanol, 2‐methyl‐2‐hexanol, is primarily attributed to the reduction of the activation enthalpy by stabilizing intraporous interactions of the C β ‐H transition state with surrounding alcohol molecules. Overall, we show that the positive impact of zeolite confinements results from the stabilization of transition state provided by the confinement and intermolecular interaction of alkanols with the transition state, which is impacted by both the size of confinements and the structure of alkanols in the E1 pathway of dehydration.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Copper-zirconia interfaces in UiO-66 enable selective catalytic hydrogenation of CO 2 to methanol

Molecular interactions with both oxides and metals are essential for heterogenous catalysis, leading to remarkable synergistic impacts on activity and selectivity. Here, we show that the direct link between the two phases (and not merely being together) is required to selectively hydrogenate CO 2 to methanol on catalysts containing Cu and ZrO 2 . Materials consisting of isolated Cu particles or atomically dispersed Cu–O–Zr sites only catalyze the reverse watergas shift reaction. In contrast, a metal organic framework structure (UiO-66) with Cu nanoparticles occupying missing-linker defects maximizes the fraction of metallic Cu interfaced to ZrO 2 nodes leading to a material with high adsorption capacity for CO 2 and high activity and selectivity for low-temperature methanol synthesis.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rate Enhancement of Acid-Catalyzed Alcohol Dehydration by Supramolecular Organic Capsules

The presence of a (sub)nanometric environment has been demonstrated to enhance the rate of homogeneous acid-catalyzed reactions. Conventionally, such catalysts are constructed by directly embedding a catalytically active acid site into the structure of a porous material, linking the acid properties with the properties of the embedding solid. Here, a holoenzyme mimicking approach was used, in which a self-assembled hexameric resorcinarene capsule (1.4 nm 3 cavity) acts like an apoenzyme that transforms into a catalytically active site by hosting hydrated HCl as a cofactor. This capsule binds the hydronium ion together with cyclohexanol (CyOH) and catalyzes the dehydration to cyclohexene with enhanced rates that are 2 orders of magnitude higher than those in the unconstrained environment. Kinetic analysis shows that cyclohexanol dehydration proceeds via an E2 mechanism on hydrated HCl in the unconstrained environment, while the constrained environment of the active capsule induces the stabilization of an ionic intermediate, allowing an E1 mechanism to dominate. By comparison with the reaction in zeolite environments, we show that the direct chemical environment of the capsule or a zeolite wall exerts only a minor direct influence. The volume constraint increases the reaction rate by inducing a larger activation entropy, indicating the stabilization of a later transition state in the E1 mechanism, as well as a higher reaction space of the carbenium ion constituting the transition state.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrocatalytic Hydrogenation of Biomass-Derived Organics: A review

Sustainable energy generation calls for a shift away from centralized, high-temperature, energy-intensive processes to decentralized, low-temperature conversions that can be powered by electricity produced from renewable sources. Electrocatalytic conversion of biomass-derived feedstocks would allow carbon recycling of distributed, energy-poor resources in the absence of sinks and sources of high-grade heat. Selective, efficient electrocatalysts that operate at low temperatures are needed for electrocatalytic hydrogenation (ECH) to upgrade the feedstocks. For effective generation of energy-dense chemicals and fuels, two design criteria must be met: (i) a high H:C ratio via ECH to allow for high-quality fuels and blends, and (ii) a lower O:C ratio in the target molecules via electrochemical decarboxylation/deoxygenation to improve the stability of fuels and chemicals. The goal of this review is to determine whether the following questions have been sufficiently answered in open literature, and if not, what additional information is required: (1) What organic functionalities are accessible for electrocatalytic hydrogenation under a set of reaction conditions? How do substitutions and functionalities impact the activity and selectivity of ECH? (2) What material properties cause an electrocatalyst to be active for ECH? Can general trends in ECH be formulated based on the type of electrocatalyst? (3) What is the impact of reaction (electrolyte concentration, pH, operating potential) and reactor type conditions?

Catalysts, redox reactions, hydrocarbons, Aromatic↗