Search NASASearch

Engineering topics

Li, Mengya

Publications and source records attributed to Li, Mengya.

Assessing cathode–electrolyte interphases in batteries

The cathode-electrolyte interphase plays a pivotal role in determining the usable capacity and cycling stability of electrochemical cells, yet it is overshadowed by its counterpart, the solid-electrolyte interphase. This is primarily due to the prevalence of side reactions, particularly at low potentials on the negative electrode, especially in state-of-the-art Li-ion batteries where the charge cutoff voltage is limited. However, as the quest for high-energy battery technologies intensifies, there is a pressing need to advance the study of cathode-electrolyte interphase properties. Here, we present a comprehensive approach to analyse the cathode-electrolyte interphase in battery systems. We underscore the importance of employing model cathode materials and coin cell protocols to establish baseline performance. Additionally, we delve into the factors behind the inconsistent and occasionally controversial findings related to the cathode-electrolyte interphase. In conclusion, we also address the challenges and opportunities in characterizing and simulating the cathode-electrolyte interphase, offering potential solutions to enhance its relevance to real-world applications.

25 ENERGY STORAGE

Pore-Filling Induced Solid Electrolyte Failure of Ti-Doped Na 3 Zr 2 Si 2 PO 12 Characterized by Operando Synchrotron X-Ray Tomography

Solid-state batteries (SSBs), particularly those utilizing sodium metal, are emerging as a promising technology due to their potential for enhanced safety, higher energy density, and longer cycle life. NASICON (Na superionic conductor) materials, known for their robust crystalline structure and high ionic conductivity, are pivotal in the development of efficient sodium all-solid-state batteries. These materials exhibit high room-temperature ionic conductivity and electrochemical stability, making them ideal for various applications. Research has focused on improving NASICON's ionic conductivity and stability through doping, interface regulation, and composite anode design. Recent advancements include Ti-doped Na 3 Zr 2 Si 2 PO 12 (Ti-NZSP), which demonstrates improved surface stability, higher ionic conductivity, and increased critical current density. However, challenges such as Na dendrite formation and mechanical integrity under operational conditions persist. Advanced imaging techniques like operando synchrotron X-ray tomography have provided insights into failure mechanisms, revealing that pore-filling and dendrite growth are significant issues. Understanding these processes is essential for enhancing the performance and safety of Na-based SSBs. Here, this study underscores the need for continued research to address these challenges and develop reliable, high-performance solid-state electrolytes for future energy storage solutions.

25 ENERGY STORAGE

Impact of electrolyte solutions on carbon dioxide fixation in single chamber Al–CO 2 battery

Governments and research & development (R&D) organizations are actively initiating various programs and research strategies for CO 2 capture, its utilization, and integration with long duration energy storage from renewable sources worldwide. In line with the carbon capture goals, here we report a novel electrochemical Al-CO 2 battery cell, that can simultaneously capture CO 2 and convert it into value-added products, in addition to long-duration energy generation and storage. Here, this innovative approach employs cost-effective Al metal as an anode and an in-house synthesized Ni–Fe based bimetallic double hydroxide catalyst as the cathode, with meticulously optimized compositions and morphologies. We explore the impact of different aqueous electrolyte solutions compositions on the cell performance, demonstrating up to 10 h of stable long duration energy storage with a stable voltage profile. The cell exhibits low polarization even at high current densities of up to 12 mA cm -2 and maintains stable cycling over 500 h. Through Fourier-transform infrared spectroscopy (FTIR), Raman spectroscopy, X-ray Diffraction and X-ray photoelectron spectroscopy (XPS) analysis, we determined that the discharge product is either NaAlCO 3 (OH) 2 or KAlCO 3 (OH) 2 , distinct from the Al 2 (CO 3 ) 3 typically reported in conventional Al–CO 2 batteries.

25 ENERGY STORAGE

Lithium Plating Characteristics in High Areal Capacity Li-Ion Battery Electrodes

Li-ion battery degradation and safety events are often attributed to undesirable metallic lithium plating. Since their release, Li-ion battery electrodes have been made progressively thicker to provide a higher energy density. However, the propensity for plating in these thicker pairings is not well understood. Herein, we combine an experimental plating-prone condition with robust mesoscale modeling to examine electrode pairings with capacities ranging from 2.5 to 6 mAh/cm 2 and negative to positive (N/P) electrode areal capacity ratio from 0.9 to 1.8 without the need for extensive aging tests. Using both experimentation and a mesoscale model, we identify a shift from conventional high state-of-charge (SOC) type plating to high overpotential (OP) type plating as electrode thickness increases. Further, these two plating modes have distinct morphologies, identified by optical microscopy and electrochemical signatures. We demonstrate that under operating conditions where these plating modes converge, a high propensity of plating exists, revealing the importance of predicting and avoiding this overlap for a given electrode pairing. Further, we identify that thicker electrodes, beyond a capacity of 3 mAh/cm 2 or thickness >75 μm, are prone to high OP, limiting negative electrode (NE) utilization and preventing cross-sectional oversizing the NE from mitigating plating. Here, it simply contributes to added mass and volume. The experimental thermal gradient and mesoscale model either combined or independently provide techniques capable of probing performance and safety implications of mild changes to electrode design features.

25 ENERGY STORAGE