Search NASA⌕ Search

Engineering topics

Li, Tianyi (ORCID:0000000262346096)

Publications and source records attributed to Li, Tianyi (ORCID:0000000262346096).

Parasitic structure defect blights sustainability of cobalt-free single crystalline cathodes

Abstract Recent efforts to reduce battery costs and enhance sustainability have focused on eliminating Cobalt (Co) from cathode materials. While Co-free designs have shown notable success in polycrystalline cathodes, their impact on single crystalline (SC) cathodes remains less understood due to the significantly extended lithium diffusion pathways and the higher-temperature synthesis involved. Here, we reveal that removing Co from SC cathodes is structurally and electrochemically unfavorable, exhibiting unusual voltage fade behavior. Using multiscale diffraction and imaging techniques, we identify lithium-rich nanodomains (LRNDs) as a heterogeneous phase within the layered structure of Co-free SC cathodes. These LRNDs act as critical tipping points, inducing significant chemo-mechanical lattice strain and irreversible structural degradation, which exacerbates the voltage and capacity loss in electrochemical performance. Our findings highlight the considerable challenges of developing Co-free SC cathodes compared to polycrystalline ones and emphasize the need for new strategies to balance the interplay between cost, sustainability, and performance.

36 MATERIALS SCIENCE↗

Microstrain screening towards defect-less layered transition metal oxide cathodes

Microstrain and the associated surface-to-bulk propagation of structural defects are known to be major roadblocks to developing high-energy and long-life batteries. However, the origin and effects of microstrain during the synthesis of battery materials remain largely unknown. Here, in this study, we perform microstrain screening during real-time and realistic synthesis of sodium layered oxide cathodes. Evidence gathered from multiscale in situ synchrotron X-ray diffraction and microscopy characterization collectively reveals that the spatial distribution of transition metals within individual precursor particles strongly governs the nanoscale phase transformation, local charge heterogeneity and accumulation of microstrain during synthesis. This unexpected dominance of transition metals results in a counterintuitive outward propagation of defect nucleation and growth. These insights direct a more rational synthesis route to reduce the microstrain and crystallographic defects within the bulk lattice, leading to significantly improved structural stability. The present work on microstrain screening represents a critical step towards synthesis-by-design of defect-less battery materials.

25 ENERGY STORAGE↗

Development of high-energy non-aqueous lithium-sulfur batteries via redox-active interlayer strategy

Abstract Lithium-sulfur batteries have theoretical specific energy higher than state-of-the-art lithium-ion batteries. However, from a practical perspective, these batteries exhibit poor cycle life and low energy content owing to the polysulfides shuttling during cycling. To tackle these issues, researchers proposed the use of redox-inactive protective layers between the sulfur-containing cathode and lithium metal anode. However, these interlayers provide additional weight to the cell, thus, decreasing the practical specific energy. Here, we report the development and testing of redox-active interlayers consisting of sulfur-impregnated polar ordered mesoporous silica. Differently from redox-inactive interlayers, these redox-active interlayers enable the electrochemical reactivation of the soluble polysulfides, protect the lithium metal electrode from detrimental reactions via silica-polysulfide polar-polar interactions and increase the cell capacity. Indeed, when tested in a non-aqueous Li-S coin cell configuration, the use of the interlayer enables an initial discharge capacity of about 8.5 mAh cm −2 (for a total sulfur mass loading of 10 mg cm −2 ) and a discharge capacity retention of about 64 % after 700 cycles at 335 mA g −1 and 25 °C.

25 ENERGY STORAGE↗