Alloys for shaped charge liners method for making alloys for shaped charge liners

One embodiment of the invention provides an alloy with a density greater than 10 g/cm3, the alloy comprising a single phase solution of tungsten, nickel, and iron. Also provided is a cone liner for use in shaped charges, the liner comprised of a tungsten, nickel, iron alloy having a single phase microstructure. Substantially no precipitates or second phases exist in the alloy. One embodiment of the invention further provides a method for producing a single phase alloy, the method comprising establishing a melt of iron and nickel; dissolving tungsten in the melt to form a solution; wherein the atomic percents of the nickel, tungsten and iron range from between approximately Ni-7%W-0%Fe, Ni-18%W-0%Fe, and Ni-8%W-24%Fe, wherein Ni is the remainder, maintaining the solution at a first temperature sufficient to create a homogeneous mixture; allowing the homogeneous mixture to solidify; and thermochemically treating the solidified mixture for a time to dissolve any second phases or microstructure within the mixture.

36 MATERIALS SCIENCE↗

Advanced Electron Microscopy and Micro analytical technique development and application for Irradiated TRISO Coated Particles from the AGR-1 Experiment

A series of up to seven irradiation experiments are planned for the Advanced Gas Reactor (AGR) Fuel Development and Quantification Program, with irradiation completed at the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) for the first experiment (i.e., AGR-1) in November 2009 for an effective 620 full power days. The objective of the AGR-1 experiment was primarily to provide lessons learned on the multi-capsule test train design and to provide early data on fuel performance for use in fuel fabrication process development and post-irradiation safety testing data at high temperatures. This report describes the advanced microscopy and micro-analysis results on selected AGR-1 coated particles.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Progress Report on Alloy 617 Notched Specimen Testing

Creep behavior of Alloy 617 has been extensively characterized to support the development of a draft Code Case to qualify Alloy 617 in Section III division 5 of the ASME Boiler and Pressure Vessel Code. This will allow use of Alloy 617 in construction of nuclear reactor components at elevated temperatures and longer periods of time (up to 950°C and 100,000 hours). Prior to actual use, additional concerns not considered in the ASME code need to be addressed. Code Cases are based largely on uniaxial testing of smooth gage specimens. In service conditions, components will generally be under multi axial loading. There is also the concern of the behavior at discontinuities, such as threaded components. To address the concerns of multi axial creep behavior and at geometric discontinuities, notched specimens have been designed to create conditions representative of the states that service components experience. Two general notch geometries have been used for these series of tests: U notch and V notch specimens. The notches produce a tri axial stress state, though not uniform across the specimen. Characterization of the creep behavior of the U notch specimens and the creep rupture behavior of the V notch specimens provides a good approximation of the behavior expected of actual components. Preliminary testing and analysis have been completed and are reported in this document. This includes results from V notch specimens tested at 900°C and 800°C. Failure occurred in the smooth gage section of the specimen rather than at the root of the notch, though some damage was present at the root of the notch, where initial stress was highest. This indicates notch strengthening behavior in this material at these temperatures.

36 MATERIALS SCIENCE↗

Microstructural Characterization of Alloy 617 Crept into the Tertiary Regime

The microstructure of Alloy 617 was characterized following creep tests interrupted at total creep strains ranging from 2-20%. A range of creep temperatures (750-1000oC) and initial creep stresses (10-145 MPa) produced creep test durations ranging from 1 to 5800 hours. Image analysis of optical photomicrographs on longitudinal sections of the gage length was used to document the fraction of creep porosity as a function of creep parameters. Creep porosity was negligible below tertiary creep strains of 10% and increased with tertiary creep strain, thereafter. For a given temperature and total creep strain, creep porosity increased with decreasing creep stress. Creep porosity increased linearly with duration of the creep experiment. TEM performed on the gage sections did not reveal significant creep cavity formation on grain boundaries at the sub-micron level. It was concluded that the onset of tertiary creep did not result from creep cavitation and more likely arose due to the formation of low energy dislocation substructures with increasing tertiary strain.

Alloy 617↗

Properties of Alloy 617 for Heat Exchanger Design

Abstract – Alloy 617 is among the primary candidates for very high temperature reactor heat exchangers anticipated for use up to 950ºC. Elevated temperature properties of this alloy and the mechanisms responsible for the observed tensile, creep and creep-fatigue behavior have been characterized over a wide range of test temperatures up to 1000ºC. Properties from the current experimental program have been combined with archival information from previous VHTR research to provide large data sets for many heats of material, product forms, and weldments. The combined data have been analyzed to determine conservative values of yield and tensile strength, strain rate sensitivity, creep-rupture behavior, fatigue and creep- fatigue properties that can be used for engineering design of reactor components. Phenomenological models have been developed to bound the regions over which the engineering properties are well known or can be confidently extrapolated for use in design.

Alloy 617↗

Methods of forming aluminum oxynitride-comprising bodies, including methods of forming a sheet of transparent armor

The invention includes methods of forming an aluminum oxynitride-comprising body. For example, a mixture is formed which comprises A:B:C in a respective molar ratio in the range of 9:3.6-6.2:0.1-1.1, where "A" is Al.sub.2O.sub.3, "B" is AlN, and "C" is a total of one or more of B.sub.2O.sub.3, SiO.sub.2, Si--Al--O--N, and TiO.sub.2. The mixture is sintered at a temperature of at least 1,600.degree. C. at a pressure of no greater than 500 psia effective to form an aluminum oxynitride-comprising body which is at least internally transparent and has at least 99% maximum theoretical density.

36 MATERIALS SCIENCE↗