Long-Term Stability in Perovskite Solar Cells Through Atomic Layer Deposition of Tin Oxide

Robust contact schemes that boost stability and simplify the production process are needed for perovskite solar cells (PSCs). We codeposited perovskite and hole-selective contact while protecting the perovskite to enable deposition of SnOx/Ag without the use of a fullerene. The SnOx, prepared through atomic layer deposition, serves as a durable inorganic electron transport layer. Tailoring the oxygen vacancy defects in the SnOx layer led to power conversion efficiencies (PCEs) of >25%. Our devices exhibit superior stability over conventional p-i-n PSCs, successfully meeting several benchmark stability tests. They retained >95% PCE after 2000 hours of continuous operation at their maximum power point under simulated AM1.5 illumination at 65degrees C. Additionally, they boast a certified T97 lifetime exceeding 1000 hours.

c60↗

Enabling High Stability of Co-Free LiNiO 2 Cathode via a Sulfide-Enriched Cathode Electrolyte Interface

Cobalt-free lithium nickel oxide (LNO) has garnered significant interest as the end member of high-nickel layered oxide cathodes for next-generation batteries. However, its practical performance notably underperforms expectations because of the structural degradation and unstable interfacial chemistry with electrolytes during cycling. Here, in this study, we report that a durable cathode-electrolyte interface (CEI), enriched by in situ formed sulfides and borides, can inhibit LNO structural degradation and suppress Ni ion dissolution. With the CEI protection, the stability of LNO can be remarkably extended, and batteries demonstrate a capacity retention rate of 84% (30 °C) and 79% (50 °C) after 200 cycles at 1C, respectively. These results demonstrate that enriching CEI with sulfur-containing species can effectively stabilize the interfacial chemistry of LNO, particularly at an elevated temperature of 50 °C. This finding provides valuable perspectives on designing electrolytes for cobalt-free LNO and other high-Ni cathodes toward the development of next-generation high-energy-density lithium-ion batteries.

25 ENERGY STORAGE↗

Regulating the Electron Distribution of Metal-Oxygen for Enhanced Oxygen Stability in Li-rich Layered Cathodes

Li-rich Mn-based layered oxides (LLO) hold great promise as cathode materials for lithium-ion batteries (LIBs) due to their unique oxygen redox (OR) chemistry, which enables additional capacity. However, the LLOs face challenges related to the instability of their OR process due to the weak transition metal (TM)-oxygen bond, leading to oxygen loss and irreversible phase transition that results in severe capacity and voltage decay. Herein, a synergistic electronic regulation strategy of surface and interior structures to enhance oxygen stability is proposed. In the interior of the materials, the local electrons around TM and O atoms may be delocalized by surrounding Mo atoms, facilitating the formation of stronger TM—O bonds at high voltages. Besides, on the surface, the highly reactive O atoms with lone pairs of electrons are passivated by additional TM atoms, which provides a more stable TM—O framework. Hence, this strategy stabilizes the oxygen and hinders TM migration, which enhances the reversibility in structural evolution, leading to increased capacity and voltage retention. This work presents an efficient approach to enhance the performance of LLOs through surface-to-interior electronic structure modulation, while also contributing to a deeper understanding of their redox reaction.

25 ENERGY STORAGE↗

Prognostic analysis of high-flow nasal cannula therapy and non-invasive ventilation in mild to moderate hypoxemia patients and construction of a machine learning model for 48-h intubation prediction—a retrospective analysis of the MIMIC database

Background This study aims to investigate the clinical outcome between high-flow nasal cannula (HFNC) and non-invasive ventilation (NIV) therapy in mild to moderate hypoxemic patients on the first ICU day and to develop a predictive model of 48-h intubation. Methods The study included adult patients from the MIMIC III and IV databases who first initiated HFNC or NIV therapy due to mild to moderate hypoxemia (100 < PaO2/FiO2 ≤ 300). The 48-h and 30-day intubation rates were compared using cross-sectional and survival analysis. Nine machine learning and six ensemble algorithms were deployed to construct the 48-h intubation predictive models, of which the optimal model was determined by its prediction accuracy. The top 10 risk and protective factors were identified using the Shapley interpretation algorithm. Result A total of 123,042 patients were screened, of which, 673 were from the MIMIC IV database for ventilation therapy comparison (HFNC n = 363, NIV n = 310) and 48-h intubation predictive model construction (training dataset n = 471, internal validation set n = 202) and 408 were from the MIMIC III database for external validation. The NIV group had a lower intubation rate (23.1% vs. 16.1%, p = 0.001), ICU 28-day mortality (18.5% vs. 11.6%, p = 0.014), and in-hospital mortality (19.6% vs. 11.9%, p = 0.007) compared to the HFNC group. Survival analysis showed that the total and 48-h intubation rates were not significantly different. The ensemble AdaBoost decision tree model (internal and external validation set AUROC 0.878, 0.726) had the best predictive accuracy performance. The model Shapley algorithm showed Sequential Organ Failure Assessment (SOFA), acute physiology scores (APSIII), the minimum and maximum lactate value as risk factors for early failure and age, the maximum PaCO 2 and PH value, Glasgow Coma Scale (GCS), the minimum PaO 2 /FiO 2 ratio, and PaO 2 value as protective factors. Conclusion NIV was associated with lower intubation rate and ICU 28-day and in-hospital mortality. Further survival analysis reinforced that the effect of NIV on the intubation rate might partly be attributed to the other impact factors. The ensemble AdaBoost decision tree model may assist clinicians in making clinical decisions, and early organ function support to improve patients’ SOFA, APSIII, GCS, PaCO 2 , PaO 2 , PH, PaO 2 /FiO 2 ratio, and lactate values can reduce the early failure rate and improve patient prognosis.

Fu, Wei↗

Unit-cell-thick zeolitic imidazolate framework films for membrane application

Zeolitic imidazolate frameworks (ZIFs) are a subset of metal–organic frameworks with more than 200 characterized crystalline and amorphous networks made of divalent transition metal centres (for example, Zn 2+ and Co 2+ ) linked by imidazolate linkers. ZIF thin films have been intensively pursued, motivated by the desire to prepare membranes for selective gas and liquid separations. To achieve membranes with high throughput, as in ångström-scale biological channels with nanometre-scale path lengths, ZIF films with the minimum possible thickness—down to just one unit cell—are highly desired. However, the state-of-the-art methods yield membranes where ZIF films have thickness exceeding 50 nm. Here we report a crystallization method from ultradilute precursor mixtures, which exploits registry with the underlying crystalline substrate, yielding (within minutes) crystalline ZIF films with thickness down to that of a single structural building unit (2 nm). The film crystallized on graphene has a rigid aperture made of a six-membered zinc imidazolate coordination ring, enabling high-permselective H 2 separation performance. The method reported here will probably accelerate the development of two-dimensional metal–organic framework films for efficient membrane separation.

36 MATERIALS SCIENCE↗

Stabilizing the Deep Sodiation Process in Layered Sodium Manganese Cathodes by Anchoring Boron Ions

Advanced high-energy-density sodium-ion batteries (SIBs) are inseparable from cathode materials with high specific capacities. Layered manganese-rich oxides (Na x MnO 2 , 0.6 ≤ x ≤1) are promising cathode materials owing to their ease of intercalation and extraction of a considerable amount of sodium ions. However, lattice interactions, especially electrostatic repulsive forces and anisotropic stresses, are usually caused by deep desodiatin/sodiation process, resulting in intragranular cracks and capacity degradation in SIBs. Here, boron ions are introduced into the layered structure to build up B-O-Mn bonds. Further, the regulated electronic structure in Na 0.637 B 0.038 MnO 2 (B-NMO) materials inhibits the deformation of MnO 6 octahedra, which finally achieves a gentle structural transition during the deep sodiation process. B-NMO electrode exhibits a high capacity (141 mAh g –1 ) at 1 C with a capacity retention of 81% after 100 cycles. Therefore, anchoring boron to manganese-rich materials inhibits the detrimental structural evolution of deep sodiation and can be used to obtain excellent cathode materials for SIBs.