Microstrain screening towards defect-less layered transition metal oxide cathodes

Microstrain and the associated surface-to-bulk propagation of structural defects are known to be major roadblocks to developing high-energy and long-life batteries. However, the origin and effects of microstrain during the synthesis of battery materials remain largely unknown. Here, in this study, we perform microstrain screening during real-time and realistic synthesis of sodium layered oxide cathodes. Evidence gathered from multiscale in situ synchrotron X-ray diffraction and microscopy characterization collectively reveals that the spatial distribution of transition metals within individual precursor particles strongly governs the nanoscale phase transformation, local charge heterogeneity and accumulation of microstrain during synthesis. This unexpected dominance of transition metals results in a counterintuitive outward propagation of defect nucleation and growth. These insights direct a more rational synthesis route to reduce the microstrain and crystallographic defects within the bulk lattice, leading to significantly improved structural stability. The present work on microstrain screening represents a critical step towards synthesis-by-design of defect-less battery materials.

25 ENERGY STORAGE↗

Light-induced Kondo-like exciton-spin interaction in neodymium(II) doped hybrid perovskite

Abstract Tuning the properties of a pair of entangled electron and hole in a light-induced exciton is a fundamentally intriguing inquiry for quantum science. Here, using semiconducting hybrid perovskite as an exploratory platform, we discover that Nd 2+ -doped CH 3 NH 3 PbI 3 (MAPbI 3 ) perovskite exhibits a Kondo-like exciton-spin interaction under cryogenic and photoexcitation conditions. The feedback to such interaction between excitons in perovskite and the localized spins in Nd 2+ is observed as notably prolonged carrier lifetimes measured by time-resolved photoluminescence, ~10 times to that of pristine MAPbI 3 without Nd 2+ dopant. From a mechanistic standpoint, such extended charge separation states are the consequence of the trap state enabled by the antiferromagnetic exchange interaction between the light-induced exciton and the localized 4 f spins of the Nd 2+ in the proximity. Importantly, this Kondo-like exciton-spin interaction can be modulated by either increasing Nd 2+ doping concentration that enhances the coupling between the exciton and Nd 2+ 4 f spins as evidenced by elongated carrier lifetime, or by using an external magnetic field that can nullify the spin-dependent exchange interaction therein due to the unified orientations of Nd 2+ spin angular momentum, thereby leading to exciton recombination at the dynamics comparable to pristine MAPbI 3 .

36 MATERIALS SCIENCE↗

Native lattice strain induced structural earthquake in sodium layered oxide cathodes

Abstract High-voltage operation is essential for the energy and power densities of battery cathode materials, but its stabilization remains a universal challenge. To date, the degradation origin has been mostly attributed to cycling-initiated structural deformation while the effect of native crystallographic defects induced during the sophisticated synthesis process has been significantly overlooked. Here, using in situ synchrotron X-ray probes and advanced transmission electron microscopy to probe the solid-state synthesis and charge/discharge process of sodium layered oxide cathodes, we reveal that quenching-induced native lattice strain plays an overwhelming role in the catastrophic capacity degradation of sodium layered cathodes, which runs counter to conventional perception—phase transition and cathode interfacial reactions. We observe that the spontaneous relaxation of native lattice strain is responsible for the structural earthquake (e.g., dislocation, stacking faults and fragmentation) of sodium layered cathodes during cycling, which is unexpectedly not regulated by the voltage window but is strongly coupled with charge/discharge temperature and rate. Our findings resolve the controversial understanding on the degradation origin of cathode materials and highlight the importance of eliminating intrinsic crystallographic defects to guarantee superior cycling stability at high voltages.

25 ENERGY STORAGE↗