Engineering topics
Loboda, M
Publications and source records attributed to Loboda, M.
A method to determine fault vectors in 4H-SiC from stacking sequences observed on high resolution transmission electron microscopy images
A new method has been developed to determine the fault vectors associated with stacking faults in 4H-SiC from their stacking sequences observed on high resolution TEM images. This method, analogous to the Burgers circuit technique for determination of dislocation Burgers vector, involves determination of the vectors required in the projection of the perfect lattice to correct the deviated path constructed in the faulted material. Results for several different stacking faults were compared with fault vectors determined from X-ray topographic contrast analysis and were found to be consistent. This technique is expected to applicable to all structures comprising corner shared tetrahedra.
Characterization of 100 mm Diameter 4H-Silicon Carbide CrystalsWith Extremely Low Basal Plane Dislocation Density
Synchrotron White Beam X-ray Topography (SWBXT) studies are presented of basal plane dislocation (BPD) configurations and behavior in a new generation of 100mm diameter, 4H-SiC wafers with extremely low BPD densities (3-4 x 10{sup 2} cm{sup -2}). The conversion of non-screw oriented, glissile BPDs into sessile threading edge dislocations (TEDs) is observed to provide pinning points for the operation of single ended Frank-Read sources. In some regions, once converted TEDs are observed to re-convert back into BPDs in a repetitive process which provides multiple BPD pinning points.
Characterization of 100 mm diameter 4H-silicon carbide crystals with extremely low basal plane dislocation density
Synchrotron White Beam X-ray Topography (SWBXT) studies are presented of basal plane dislocation (BPD) configurations and behavior in a new generation of 100mm diameter, 4H-SiC wafers with extremely low BPD densities (3-4 x 10{sup 2} cm{sup -2}). The conversion of non-screw oriented, glissile BPDs into sessile threading edge dislocations (TEDs) is observed to provide pinning points for the operation of single ended Frank-Read sources. In some regions, once converted TEDs are observed to re-convert back into BPDs in a repetitive process which provides multiple BPD pinning points.
Micropipe Dissociation through Thick n+ Buffer Layer Growth
Thick (> 25 {mu}m) 4H n+ epitaxial layer growth was performed on 4H n+ substrates utilizing chlorine containing etch chemistries in a hot wall CVD system. Optimization of the n+ epitaxial layer growth was achieved by varying C/Si ratio and N2 flow. Desired epitaxial layers have doping levels > 5x1018 cm-3, epitaxial surface roughness <10 nm on a 20x20 {mu}m area and overall micropipe density reduction. To confirm the conversion of micropipes into closed core screw dislocations, microscopic examination of the epitaxial and wafer surfaces was carried out after KOH etching. Grazing incidence x-ray topography (XRT) as well as cross sectional XRT and microscopy were also performed. The cross sectional evaluation showed that the dissociation of the micropipes occurs very close to the epitaxy/wafer interface.