Interfacial Pressure Improves Calendar Aging of Lithium Metal Anodes

Lithium metal is a very attractive anode material because its theoretical specific capacity is approximately 10 times higher than conventional graphite anodes. Despite great promise, Li anodes suffer from capacity fade due to instabilities with the electrolyte as well as stranding of active Li. We have previously shown that applied interfacial pressure improves Li anode cycling because the pressure reduces the propensity for Li isolation and enables easier reconnection. Many researchers have also shown that calendar aging can lead to Li capacity loss and this has been attributed to either electrolyte decomposition with concurrent Li corrosion or to the formation of stranded Li. Our prior research focused on calendar aging during cycling suggests the mechanism for calendar aging is largely related to stranding of Li during rest and reconnection of the stranded Li upon further cycling, evidenced by similar average Coulombic efficiencies and Li loss in cells with and without rest. Because our calendar aging studies suggest Li stranding as a major cause of Coulombic efficiency drops and our Li cycling studies suggest this can be mitigated partially through applied interfacial pressure, we hypothesized that applied pressure would improve calendar aging by reducing stranded Li and enabling reconnection. We systematically varied applied pressure (0-1000 kPa) on Li metal anodes during cycling tests with and without intermittent calendar aging periods. Though the Coulombic efficiency decreases during aging periods, the lost capacity is recovered during subsequent cycles, as shown though average Coulombic efficiency and cumulative Li capacity loss analysis. We find that application of pressure partially mitigates calendar aging, in accordance with our hypothesis that calendar aging is caused by Li standing and can be mitigated to some degree with interfacial pressure. This is further supported by our results showing that the average Coulombic efficiency and cumulative Li capacity losses are similar over 50 cycles for cells that were continuously cycled and cells with periodic calendar aging periods. This result indicates that the losses during aging are reversible, which is consistent with Li stranding and reconnection. We show that pressure is one mitigation technique that helps reduce Li calendar aging in this study, but our finding that calendar aging is primarily governed by the stranding and reconnection of dead Li has wider implications. This research suggests that other mitigations which have been shown to prevent dead Li formation or encourage reconnection during cycling would also likely be successful for the purpose of improving calendar aging. The authors were supported by a Laboratory Directed Research and Development (LDRD) program. This work was performed, in part, at the Center for Integrated Nanotechnologies, an Office of Science User Facility operated for the U.S. Department of Energy (DOE) Office of Science. Sandia National Laboratories is a multi-mission laboratory managed and operated by National Technology & Engineering Solutions of Sandia, LLC (NTESS), a wholly owned subsidiary of Honeywell International Inc., for the U.S. Department of Energy's National Nuclear Security Administration (DOE/NNSA) under contract DE-NA0003525. This written work is authored by an employee of NTESS. The employee, not NTESS, owns the right, title and interest in and to the written work and is responsible for its contents. This work was authored in part by the National Renewable Energy Laboratory, operated by Alliance for Sustainable Energy, LLC, for the U.S. Department of Energy (DOE) under Contract No. DE-AC36-08GO28308. Any subjective views or opinions that might be expressed in the written work do not necessarily represent the views of the U.S. Government.

applied pressure↗

Effects of Applied Interfacial Pressure on Li-Metal Cycling Performance and Morphology in 4 M LiFSI in DME

Lithium-metal anodes can theoretically enable 10x higher gravimetric capacity than conventional graphite anodes. However, Li-metal anode cycling has proven difficult due to porous and dendritic morphologies, extensive parasitic solid electrolyte interphase reactions, and formation of dead Li. We systematically investigate the effects of applied interfacial pressure on Li-metal anode cycling performance and morphology in the recently developed and highly efficient 4 M lithium bis(fluorosulfonyl)imide in 1,2-dimethoxyethane electrolyte. We present cycling, morphology, and impedance data at a current density of 0.5 mA/cm 2 and a capacity of 2 mAh/cm 2 at applied interfacial pressures of 0, 0.01, 0.1, 1, and 10 MPa. Cryo-focused ion beam milling and cryo-scanning electron microscopy imaging in cross section reveal that increasing the applied pressure during Li deposition from 0 to 10 MPa leads to greater than a fivefold reduction in thickness (and therefore volume) of the deposited Li. This suggests that pressure during cycling can have a profound impact on the practical volumetric energy density for Li-metal anodes. A “goldilocks zone” of cell performance is observed at intermediate pressures of 0.1–1 MPa. Increasing pressure from 0 to 1 MPa generally improves cell-to-cell reproducibility, cycling stability, and Coulombic efficiency. However, the highest pressure (10 MPa) results in high cell overpotential and evidence of soft short circuits, which likely result from transport limitations associated with increased pressure causing local pore closure in the separator. All cells exhibit at least some signs of cycling instability after 50 cycles when cycled to 2 mAh/cm 2 with thin 50 μm Li counter electrodes, though instability decreases with increasing pressure. In contrast, cells cycled to only 1 mAh/cm 2 perform well for 50 cycles, indicating that capacity plays an important role in cycling stability.

25 ENERGY STORAGE↗

Partitioning of Complex Fluids at Mineral Surfaces

This report summarizes the results obtained during the LDRD project entitled "Partitioning of Complex Fluids at Mineral Interfaces." This research addressed fundamental aspects of such interfaces, which are relevant to energy-water applications in the subsurface, including fossil energy extraction and carbon sequestration. This project directly addresses the problem of selectivity of complex fluid components at mineral-fluid interfaces, where complex fluids are defined as a mixture of hydrophobic and hydrophilic components: e.g., water, aqueous ions, polar/nonpolar organic compounds. Specifically, this project investigates how adsorption selectivity varies with surface properties and fluid composition. Both experimental and molecular modeling techniques were used to better understand trends in surface wettability on mineral surfaces. The experimental techniques spanned the macroscale (contact angle measurements) to the nanoscale (cryogenic electronic microscopy and vibrational spectroscopy). We focused on an anionic surfactant and a well-characterized mineral phase representative of clay phases present in oil- and gas-producing shale deposits. Collectively, the results consistently demonstrate that the presence of surfactant in the aqueous fluid significantly affects the mineral-fluid interfacial structure. Experimental and molecular modeling results reveal details of the surfactant structure at the interface, and how this structure varies with surfactant coverage and fluid composition.

04 OIL SHALES AND TAR SANDS↗