Search NASA⌕ Search

Engineering topics

Lu, Bingyu

Publications and source records attributed to Lu, Bingyu.

21 records · Page 2

Quantifying inactive lithium in lithium metal batteries

Lithium metal anodes offer high theoretical capacities (3,860 milliampere-hours per gram)1, but rechargeable batteries built with such anodes suffer from dendrite growth and low Coulombic efficiency (the ratio of charge output to charge input), preventing their commercial adoption. The formation of inactive (‘dead’) lithium— which consists of both (electro)chemically formed Li + compounds in the solid electrolyte interphase and electrically isolated unreacted metallic Li 0 —causes capacity loss and safety hazards. Quantitatively distinguishing between Li + in components of the solid electrolyte interphase and unreacted metallic Li 0 has not been possible, owing to the lack of effective diagnostic tools. Optical microscopy, in situ environmental transmission electron microscopy, X-ray microtomography and magnetic resonance imaging provide a morphological perspective with little chemical information. Nuclear magnetic resonance, X-ray photoelectron spectroscopy and cryogenic transmission electron microscopy can distinguish between Li + in the solid electrolyte interphase and metallic Li 0 , but their detection ranges are limited to surfaces or local regions. Here we establish the analytical method of titration gas chromatography to quantify the contribution of unreacted metallic Li 0 to the total amount of inactive lithium. We identify the unreacted metallic Li 0 , not the (electro)chemically formed Li + in the solid electrolyte interphase, as the dominant source of inactive lithium and capacity loss. By coupling the unreacted metallic Li 0 content to observations of its local microstructure and nanostructure by cryogenic electron microscopy (both scanning and transmission), we also establish the formation mechanism of inactive lithium in different types of electrolytes and determine the underlying cause of low Coulombic efficiency in plating and stripping (the charge and discharge processes, respectively, in a full cell) of lithium metal anodes. Here we propose strategies for making lithium plating and stripping more efficient so that lithium metal anodes can be used for next-generation high-energy batteries.

25 ENERGY STORAGE↗

New Insights on the Structure of Electrochemically Deposited Lithium Metal and Its Solid Electrolyte Interphases via Cryogenic TEM

Lithium metal has been considered as the “holy grail” anode material for rechargeable batteries though the dendritic growth and low Coulombic efficiency (CE) have crippled its practical use for decades. Its high chemical reactivity and low stability make it difficult to explore the intrinsic chemical and physical properties of the electrochemically deposited lithium (EDLi) and its accompanied solid electrolyte interphase (SEI). To prevent the dendritic growth and enhance the electrochemical reversibility, it is crucial to understand the nano- and meso- structures of EDLi. However, Li metal is very sensitive to beam damage and has low contrast for commonly used characterization techniques such as electron microscopy. Inspired by biological imaging techniques, this work demonstrates the power of cryogenic (cryo)- electron microscopy to reveal the detailed structure of EDLi and the SEI composition at the nano scale while minimizing beam damage during imaging. Surprisingly, the results show that the nucleation dominated EDLi (five minutes at 0.5 mA cm-2) is amorphous while there is some crystalline LiF present in the SEI. The EDLi grown from various electrolytes with different additives exhibits distinctive surface properties. Consequently, these results highlight the importance of the SEI and its relationship with the CE. Our findings not only illustrate the capabilities of cryogenic microscopy for beam (thermal)-sensitive materials, but it yields crucial structural information of the EDLi evolution with and without electrolyte additives.

electrochemical deposition↗