Advanced High-Voltage All-Solid-State Li-Ion Batteries Enabled by a Dual-Halogen Solid Electrolyte
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Lu, Shigang.
Explore the source record for details and available documents.
Large interfacial resistance resulting from interfacial reactions is widely acknowledged as one of the main challenges in sulfide electrolytes (SEs)-based all-solid-state lithium batteries (ASSLBs). However, the root cause of the large interfacial resistance between the SEs and typical layered oxide cathodes is not fully understood yet. Here we deciphered that interfacial oxygen loss from single-crystal LiNi 0.5 Mn 0.3 Co 0.2 O 2 (SC-NMC532) chemically oxidizes Li 10 GeP 2 S 12 , generating oxygen-containing interfacial species. Meanwhile, the interfacial oxygen loss also induces a structural change of oxide cathodes (layered-to-rocksalt). Besides, the high operation voltage can electrochemically oxidize SEs to form non-oxygen species (e.g. polysulfides). These chemically and electrochemically oxidized species, together with the interfacial structural change, are responsible for the large interfacial resistance at the cathode interface. More importantly, the widely adopted interfacial coating strategy is effective in suppressing chemically oxidized oxygen-containing species and mitigating the coincident interfacial structural change but is unable to prevent electrochemically induced non-oxygen species. These findings provide a deeper insight into the large interfacial resistance between the typical SE and layered oxide cathodes, which may be of assistance for the rational interface design of SE-based ASSLBs in future.
The pursuit of high energy density and safe lithium ion batteries (LIBs) is the urgent goal for the development of next-generation electric vehicles (EVs). All-solid-state batteries (ASSBs) with the combination of poly(ethylene oxide) (PEO)-based solid polymer electrolyte (SPE) and Ni-rich lithium nickel manganese cobalt oxide LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode are promising candidates for EVs due to their improved energy density and safety. However, the low electrochemical oxidation window of PEO-based SPE and the instability of NMC811 at the charge/discharge process seriously restrict the battery performance. Herein, a high voltage stable solid-state electrolyte layer lithium niobium oxide (LNO) is coated on the NMC811 electrode surface by atomic layer deposition for stabilizing NMC811-PEO solid polymer batteries. Electrochemical tests show that LNO coating can stabilize the NMC811 active materials and mitigate the decomposition of SPE upon the cycling process, rendering a good performance of NMC811-PEO solid polymer battery. Mechanism studies by SEM, STEM, XAS, and XPS disclose that the uncoated NMC811 suffers from chemomechanical degradations along with oxygen release triggering the decomposition of SPE, which results in unstable cathodic electrolyte interphase. With LNO coating, chemomechanical degradations and oxygen release are inhibited and the decomposition of SPE is mitigated. This paper renders a stable and high-performance high-energy-density SSB for high voltage application, which paves the way toward next-generation solid-state LIBs.
Advancement of all-solid-state lithium-ion (Li + ) batteries (ASSLIBs) has been hindered by the large interfacial resistance mainly originating from interfacial reactions between oxide cathodes and solid-state sulfide electrolytes (SEs). To suppress the interfacial reactions, an interfacial coating layer between cathodes and SEs is indispensable. However, the kinetics of interfacial Li + transport across the coating layer has not been well understood yet. Herein, we tune the interfacial ionic conductivity of the coating layer LiNb 0.5 Ta 0.5 O 3 (LNTO) by manipulating post-annealing temperature. It is found that the interfacial ionic conductivity determines interfacial Li + transport kinetics and enhancing the interfacial ionic conductivity can significantly boost the electrochemical performance of SE-based ASSLIBs. A representative cathode LiNi 0.5 Mn 0.3 Co 0.2 O 2 coated by LNTO with the highest interfacial ionic conductivity exhibits a high initial capacity of 152 mAh.g -1 at 0.1 C and 107.5 mAh.g -1 at 1C. This work highlights the importance of increasing interfacial ionic conductivity for high-performance SE-based ASSLIBs.
All-solid-state lithium-ion batteries (ASSLIBs) are receiving significant attention owing to their improved safety and energy density over liquid counterparts. However, single-crystal cathodes have never been investigated in ASSLIBs. In this work, single-crystal Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 (SC-NMC532) is used as the cathode material for ASSLIBs, which exhibits 6~14 times higher Li + diffusion coefficient than polycrystalline Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 (PC-NMC532). As a result, SC-NMC532 exhibits an initial specific capacity of 156.4 mAh.g -1 while PC-NMC532 shows an initial capacity of only 127.5 mAh.g -1 . After 150 cycles, SC-NMC532 retains the capacity of 94.5 mAh.g -1 . More impressively, under a high current density of 1.3 mA.cm -2 , SC-NMC532 exhibits a capacity of 82 mAh.g -1 , much higher than that of PC-NMC532 (2.1 mAh.g -1 ). This work demonstrates that single-crystal NMC cathodes could enable both high power density and high energy density of ASSLIBs.
Explore the source record for details and available documents.
A significant amount of intra-layer Li–Sn intermixing was observed. It was shown that the intra-layer Li–Sn was the cause of the suppression of the characteristic high-order super-reflection peaks for the C 2/ c structure.