Round superconductor wires

A round superconductor wire and method for fabricating same are disclosed. Embodiments are directed to a round superconductor wire including at least two superconductor tapes wound on a wire former. Each superconductor tape includes: bottom stabilizer and silver layers; substrate disposed above the bottom silver layer; buffer film stack disposed above the substrate; superconductor film disposed above the buffer film stack; top silver layer disposed above the superconductor film; and top stabilizer layer disposed above the top silver layer. At least one of the bottom stabilizer layer, bottom silver layer, substrate, buffer film stack, superconductor film, top silver layer, or top stabilizer layer is of a different width, thickness, or material composition in one of the superconductor tapes than in another of the superconductor tapes. These and other embodiments achieve a round superconductor wire having improved current density in high magnetic field applications when made in small diameters.

Majkic, Goran↗

Effect of Aging Treatment on the Precipitation Behavior and Mechanical Properties of Mg-9Gd-3Y-1.5Zn-0.5Zr Alloy

Aging heat treatments of an extruded Mg-9Gd-3Y-1.5Zn-0.5Zr (wt.%) alloy at 200, 225, and 250 °C for various times were studied. The results show that dynamic recrystallization (DRX) occurred during the extrusion process and the alloy exhibited a significant aging hardening response at temperatures ranging from 200 to 225 °C. The precipitation sequence of the alloy at 225 °C was supersaturated solid solution (SSSS) → β″ (D0{sub 19}, Mg{sub 3}RE) → β′ (bco, Mg{sub 15}RE{sub 3}), where the β′ phase was the primary precipitated phase. A large amount of discontinuous lamellar-shaped 14H-structure long period stacking ordered (LPSO) phase was also observed in the α-Mg matrix before and after aging treatments. Owing to the combined strengthening effect of fine DRXed grains, β′ nanoparticles, and widespread LPSO phases, the ultimate tensile strength and tensile yield strength of the peak-aged extruded alloy reached 409 and 303 MPa, respectively. The elongation in this circumstance was ~7.1%, which was slightly lower than that of the alloy before aging treatment.

36 MATERIALS SCIENCE↗