Comprehending interface shearing behavior within a bulk Cu-Nb alloy using micromechanical testing
Not Available
Engineering topics
Publications and source records attributed to Ma, Xiaolong.
Not Available
Previous research suggested that friction-based processing is a promising method for fabricating oxide dispersion-strengthened (ODS) steel. In this study, we combined friction consolidation and friction extrusion to successfully manufacture ODS steel rods using precursor powder made with gas atomization reaction synthesis. We examined the microstructure evolution from the initial powder to the final extruded rod, which revealed the dispersion process of Y. Additionally, by comparing the microstructures of three rods extruded at different temperatures, we showed that low-temperature friction extrusion effectively enhanced microstructure uniformity and prevented grain coarsening, leading to improved mechanical properties. Furthermore, our findings provide practical guidelines for adjusting processing parameters in the production of ODS steel using friction-based processing.
Two Cu-Cr-Nb alloys, denoted as alloy 1 (comprising Cu-0.89 at% Cr-0.42 at% Nb) and alloy 2 (comprising Cu-1.84 at% Cr-0.99 at% Nb), were produced through a series of manufacturing processes including vacuum induction melting, melt spinning, consolidation, brazing, and baking, with both alloys aimed at achieving a nominal Cr-to-Nb atomic ratio of 2. Microstructural characterization using transmission electron microscopy and X-ray diffraction identified the cubic C15 Laves-phase Cr 2 Nb as the dominant precipitate in both alloys, cross-validated by thermodynamic calculations and atomistic simulation-based density functional theory (DFT). Besides cubic C15 Cr 2 Nb, hexagonal C14-phase Cr 2 Nb and α-BiF3 cubic structured Cr 3 Nb were also observed in the alloys, including a coherent interface formed between the Cr 3 Nb precipitate and the Cu matrix. The hardness of the alloys increases, and the electrical conductivity decreases with increasing alloying addition content; two practical equations described the trends. Further DFT simulations revealed that the electrical conductivity (conductance) of the Cu/Cr 2 Nb interface is an order of magnitude higher than the intrinsic Cu high-angle grain boundaries.
Oxide dispersion strengthened (ODS) steels, traditionally fabricated by ball milling and conventional powder metallurgy techniques to achieve bulk form, followed by intricate rolling and thermal treatment steps to achieve plate or sheet form. Here, we present a novel processing route that combines cold spray (CS) with friction stir processing (FSP) to manufacture ODS steel plate directly from gas atomization reaction synthesis (GARS)-prepared powder, thus no rolling steps involved. Microstructural and mechanical characterizations were performed to assess the quality and properties of the resulting ODS steel plate. Our findings demonstrate that the slightly porous CS deposited layer was fully consolidated after FSP, yielding a fully dense ODS steel plate that exhibited a favorable tradeoff between strength and ductility upon extraction from the substrate. Furthermore, through microstructural analysis, we revealed the presence of an appreciable density (∼10 22 /m 3 ) of nano-sized oxide particles, with the majority being smaller than 5 nm via the combined CS + FSP fabrication route. This work serves as a first proof-of-concept demonstration of the manufacturing approach described herein, offering a possible alternative route for producing ODS steel plates.
Friction stir processing of 304/304L stainless steel is an area of interest for repair of spent nuclear fuel canisters. To enable repair without canister deflection or fracture, it is necessary to define the limitations for the depth of the processing zone which will be critically dependent on the thermal history of the material. Here, this work provides the first direct measurement of the interface temperature for friction stir processing of steel. The measured temperature is in the range of 850–1050 °C which is 20–30 % higher than previously reported values. Notably, the peak temperature occurs at the pin tip which is attributed to a higher sticking fraction and subsequently higher strain rate near the tool axis of rotation. Furthermore, a clear correlation between the temperature, grain size, and hardness is established within a single weld nugget and across different processing conditions. In the future, this data may lead to improved process modelling through direct validation and allow for property optimization through direct microstructure control.
In this work we used friction extrusion (FE), a solid phase processing technique, to produce dense, fully consolidated 5?mm rods of aluminum alloy 6061 (AA6061). The combination of large shear stresses and high temperatures at the tool-billet interface during extrusion produced equiaxed, dynamically recrystallized grains and finely distributed precipitates. Texture and microstructure evolution during extrusion was investigated in detail using scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy. Smoothed particle hydrodynamics simulation was performed to study complex material flow during extrusion. Simulation results suggest spiral material flow during extrusion which corroborated experimental results. Advantages of friction extruded microstructure over conventionally extruded counterparts are also explored using flash annealing for solution treatment followed by artificial aging. Mechanical properties of the as-friction extruded, and the artificially aged specimens were evaluated using tensile testing and compared with conventional extruded material properties.
Not Available
Accurate temperature measurement is critical to understanding the thermomechanical conditions and microstructural evolution that materials experience during severe plastic deformation (SPD). Others have previously measured the interface between a non-deforming tool and metal workpiece using thermocouples, infrared measurement, and the thermoelectric principle. Measuring temperature within the deforming material itself, especially at a high-shear deforming interface, has proven to be extremely difficult, thus limiting the application of these measurements to fundamental SPD research. In this study, the thermoelectric principle is used to directly measure temperature at the interface between copper and nickel billets undergoing SPD. This is done by utilizing the deforming materials themselves as two halves of a thermocouple junction. The spatial resolution of this measurement is shown via microscopy to be less than 1 micron. Temperature changes are sensed almost instantly, with time delays on the order of the data logger frequency (0.01 seconds). Process variations that are both very brief (<0.05 seconds) and minute (<3°C) are able to be detected by this method.
Solid phase processing by introducing shear deformation into materials can result in unique microstructure evolution and enhanced mechanical properties, especially for immiscible systems such as Cu/Nb. To better understand the correlation between microstructure and deformation behavior during shear, a dedicated testing design of stress localization at predicted sites is necessary. In this study, a specialized S-shaped specimen geometry is implemented to apply localized simple-shear loading in pure-Cu and Cu/Nb accumulative roll-bonded nanolaminates. The nanoscale microstructure and proximity of interfaces in Cu/Nb offer a ~2.8-fold increase in shear stresses than pure-Cu. In pure-Cu, the plastic instability causes shear banding and an in-plane lattice rotation. In Cu/Nb, a partial bending of the interfaces occurred, resulting in a localized lattice rotation. The adapted geometry for micro-scale specimens thus successfully captures the shear deformation at predicted sites in two distinct material systems and could potentially be a powerful technique to study the deformation mechanisms.
Shear Assisted Processing and Extrusion (ShAPE), a severe plastic deformation technique that is fast and scalable, was used to produce thin-wall tubing from alloy 6082 (Al-0.8Mg-0.9Si-0.7Mn) with in-situ solutionization during processing quickly followed by quenching. Quench medium and input material heat treatment were varied and natural aging behavior (T1 heat treatment) was evaluated using tensile testing. As-cast input material was found to have higher strength early in post-ShAPE natural aging and homogenized input material was found to have strengthening during natural aging. Compared to air quenching, water quenching gave greater strength both early in and after natural aging. These observations along with microscopy suggest that: 1. air quenching was too slow; 2. as-cast material was not fully solutionized but plastic deformation broke up the coarse intermetallic particles, which provided strengthening; and 3. homogenized material was solutionized well, which led to good natural aging behavior.
Two-phase layered thin films with a high density of semi-coherent interfaces exhibit excellent mechanical properties and thermal stability. Here, in this study, a magnetron-sputtered Cu-Nb dual-layered thin film (~500 nm for Cu and ~150 nm for Nb) having an amorphous interface between Cu and Nb with a high density of aligned growth twins in Cu is subjected to severe surface deformation. The material is loaded using indentation and cyclic shear under tribological testing. The strain accommodation in the subsurface microstructure after deformation varies based on the local structure and deformation mode. Grain refinement and crack formations in the stressed region of the Nb layer and localized crystallization of the amorphous interface are observed after indentation and scratch testing. Pronounced detwinning of growth twins in the Cu layer under the cyclic shear strain leaves large dislocations sites and loops which are observed both by high-resolution transmission electron microscopy and experiment-guided molecular dynamic (MD) simulations. Our simulations provided insights into understanding the pathway for the detwinning process under cyclic shear loading.
Meters-long oxide dispersion strengthened copper rods were manufactured directly from powder by a single-step process, called friction extrusion. The average grain size was 880 nm, which was refined 40 times from powder precursor due to extensive shear deformation. Meanwhile, the average size of alumina particles was 60 nm which retains a decent oxide dispersion strengthening. Here, mechanical properties, including hardness, tensile strength, and ductility, were tested and found to have better or similar values than conventional sintered-then-extruded oxide dispersion strengthened copper materials. The presented technique promises a convenient avenue for the fabrication of oxide dispersion strengthened copper from powder.
The temperature effect on forming gradient structure in an Al-Si alloy during surface severe deformation is studied in this report. The intermediate temperature (473 K) produces the steepest gradient structure by an anomalous hardening on the top layer compared to lower (300 K) and higher temperature (673 K) counterparts. Our analysis shows profuse aluminum oxide particles in the top layer of the gradient structure under 473 K and thus lead to anomalous hardening by oxide-dispersion strengthening. Here, the counterintuitive enhancement of strengthening at the intermediate temperature is explained by the dynamic interplay between thermal-driven, mechanical-aided oxidation and the wear-induced loss of surface materials as a function of temperature, which yields a critical processing temperature to achieve the steepest gradient structure.
Rivet materials used in the aerospace and automotive industries are typically alloys of aluminum (Al) or steel. Magnesium (Mg) is an attractive alternative because it is 33% and 75% lighter than Al and steel, respectively. However, a primary barrier for using Mg as rivet material is its poor formability at room temperature, resulting in brittle fracture of the rivet head during cold riveting. Hot riveting is possible but suffers from high cycle time due to the need for pre-heating. A new friction-based riveting technique, Rotating Hammer Riveting (RHR), is reported to fully form AZ31 Mg rivet heads in a mere 0.23 seconds cycle time. Heat and pressure generated through severe plastic deformation during the process was sufficient to form the Mg rivet head without the need for a separate pre-heating operation. Due to dynamic recrystallization, AZ31 Mg grains in the rivet head were significantly refined from about 15 to 2.6 µm during RHR, which favors the formability of Mg rivet by triggering grain boundary sliding and reducing plastic anisotropy of Mg. In addition, RHR joints showed a metallurgical bond between the rivet head and top sheet, which eliminates a significant pathway for corrosion.
Forced mixing to a single phase or supersaturated solid solution (SSS) and its prerequisite microstructure evolution in immiscible systems has been a focus of research for both fundamental science and a variety of applications. Controlling the formation of SSS by shear deformation assisted processing could enable a material design beyond conventional equilibrium microstructure in immiscible systems. Here, a highly immiscible (mixing enthalpy of ~ 20 kJ·mol -1 ) Cu-50 at. % Cr binary alloy was employed to investigate the microstructure evolution and localized tendencies of SSS during severe shear deformation. The present results demonstrate distinctive microstructure refinement process in each phase and how they lead to localized SSS as a function of shear strain. Preferential dynamic recrystallization occurs in the softer Cu phase due to strain localization, leading to substantial grain refinement. The refinement of Cr phase in the top-most layer, however, is enabled by the progressive evolution of grain lamination, splitting, and fragmentation as a function of shear strain. The eventual SSS is found to be strongly dependent on the local environments that affect the dislocation activity, including the level of microstructure refinement, the interfacial orientation relationship, hardness difference, and supposed stability of oxidation. Ab initio simulations comfirm that it is more favorable to oxidize Cr than Cu at incoherent Cu/Cr interfaces which then limits the mass transport on an incoherent boundary. Our results shed light on the underpinning mechanism for non-equilibrium mass transport in immiscible systems upon severe deformation that can be applicable to a variety of processing techniques aimed at producing immiscible alloys with superior mechanical properties.
Mechanical performance of aluminum in terms of strength, wear and corrosion resistance, especially high-temperature strength has been shown to improve with the addition of transition metal (TM) elements of Fe, Cr, and Ti. However, these feedstock materials occur as powders. As such, the traditional fabrication process is complex and expensive because it requires multiple procedures and consumes considerable energy. This study developed Shear Assisted Processing and Extrusion (ShAPE) as a single-step process that manufactures tubes directly from Al-TM powders obtained via gas atomization. Meter-long Al-TM alloy tubes are extruded from powders with different processing conditions. The ShAPE tubes have very low porosity and the average density is 2.94 kg/cm 3 , which is equal to or higher than parts fabricated by hot extrusion and sintering. The powder-to-tube fabrication process was revealed and discussed by examining the microstructural evolution. The Vickers hardness of ShAPE tubes ranges from 110 to 140 HV through wall thickness and at different extrusion speeds. The variation in hardness was correlated with the extent of refinement of intermetallics and attributed to the shear deformation per unit extrusion length. Energy cost analysis shows that ShAPE save ~60% energy compared to the conventional sintering and extrusion processes. Results indicate ShAPE is a low-cost, high-efficiency manufacturing process for producing tubes from metallic powders.
Disentangling the intragranular and interfacial plasticity contribution to the overall strain accommodation is crucial to understanding the microstructural evolution and mass transport upon deformation in materials with the nanoscale feature size. In this study, we devise a new approach to tackle the issue by introducing shear strain gradients into Cu/Nb nanolaminates of different layer thicknesses with the shear perpendicular to the laminate interfaces. The measurement of the strain gradient and the resultant lattice disorientation enables a quantitative understanding of the intragranular and interfacial plasticity contribution. We found that intragranular slip entirely governs the deformation in the 300 nm-layer laminate and, unexpectedly, contributes ~80% of the total plasticity in the 30 nm-layer laminate. The high intragranular plasticity in the thin laminate is attributed to the large width of confined slip planes and their remnant potential for storing dislocations. In addition, substantial forced chemical mixing is observed in the top region of the 30 nm-layer laminate where the effective layer thickness is reduced below 8 nm. The transition of deformation mechanism from confined layer slip to dislocation transmission is largely responsible for the initiation of substantial mixing. Our method and findings shed light on the deformation mechanism and deformation-induced mass transport behavior in nanostructured materials.
Understanding the metallurgical joinability of pure Mg and pure Fe and their interfacial microstructure lays the foundation for deciphering the complicated mechanism of joining various magnesium alloys and steels in applications. We first produced a successful metallurgical joint between pure Mg and pure Fe using the friction stir assisted scribe technique. Through detailed characterization, we found that the two immiscible metals are bonded by a critical interfacial oxide layer that spans only ~40 ± 10 nm. We present the first direct experimental evidence of the presence of a Mg/Fe oxide rich interfacial layer using high-resolution electron microscopy and discuss the contribution of oxide formation toward a successful joining mechanism.