Microwave Annealing for Fast and Effective Hydrogen Activation in Polycrystalline Silicon Passivating Contacts

Hydrogenation is a crucial step in the fabrication of high-efficiency silicon solar cells. In this study, the effectiveness of hydrogen activation is demonstrated via microwave annealing of hydrogen-rich dielectrics coated on poly-Si passivating contacts. This method is compared with conventional hydrogenation techniques, such as annealing in N2 in the presence of a hydrogen-rich source (such as hydrogenated aluminum oxide (AlOx:H), hydrogenated silicon nitride (SiNy:H), or a AlOx:H/SiNy:H stack). Key improvements observed include a reduction in J0 from 30 to <5 fA cm-2, an increase in iVoc from 690 to >730 mV, and an enhancement in effective lifetime (teff) from 0.6 to ~3.5 milliseconds on phosphorus-doped poly-Si/SiO2 passivating contact samples. With a very short annealing time of ~1-2 min, the samples passivated by AlOx:H, SiNy:H, or the stack show similar performance to samples subjected to 30 min of nitrogen annealing. Photoluminescence (PL) spectra corroborate the findings regarding the hydrogenation of the poly-Si layer and the c-Si substrate, with an increase in PL intensity after microwave annealing. Ultimately, this work suggests that microwave annealing could be a promising addition, offering flexibility to traditional firing hydrogenation processes.

hydrogenation↗

Effect of Iron Contamination and Polysilicon Gettering on the Performance of Polysilicon‐Based Passivating Contact Solar Cells

Over the past decade, silicon solar cells with carrier-selective passivating contacts based on polysilicon capping an ultra-thin silicon oxide (commonly known as TOPCon or POLO) have demonstrated promising efficiency potentials and are regarded as an evolutionary upgrade to the PERC (passivated emitter and rear contact) cells in manufacturing. The polysilicon-based passivating contacts also exhibit excellent gettering effects that relax the wafer and cleanroom requirements to some extent. Here, in this work, we experimentally explore the impact of bulk iron contamination and polysilicon gettering on the passivation quality of the polysilicon/oxide structure and the resulting solar cells performance. Results show that both n- and p-type polysilicon/oxide passivating contacts are not affected by iron gettering, demonstrating robust and stable passivation quality. However, for a very high bulk iron contamination (1 × 10 13 cm −3 ), the accumulated iron in the p-type lightly boron-doped emitter in crystalline silicon would degrade the emitter saturation current density. This can cause a reduction in both open-circuit voltage and short-circuit current. Meanwhile, this very high iron content (1 × 10 13 cm −3 ) can further degrade the fill factor and temperature coefficient of the cells. On the other hand, for an initial iron content of 2 × 10 12 cm −3 , which should be well above the iron level in the current industrial Czochralski silicon wafers, the resulting cells demonstrate similar performance as the control group with no intentional iron contamination. This work brings attention to both the benefits of polysilicon gettering effects as well as the potential degradation due to the accumulation of metal impurities in the p-type emitter region.

14 SOLAR ENERGY↗

Investigation of Gallium–Boron Spin-On Codoping for poly-Si/SiO x Passivating Contacts

A doping technique for p-type poly-Si/SiOx passivating contacts using a spin-on method for different mixtures of Ga and B glass solutions is presented. Effects of solution mixing ratios on the contact performance (implied open circuit voltage iV oc , contact resistivity ..rho..c) are investigated. For all as-annealed samples at different drive-in temperatures, increasing the percentage of Ga in the solution shows a decrement in iV oc (from ~680 to ~610 mV) and increment in ..rho..c (from ~3 to ~800 mO cm 2 ). After a hydrogenation treatment by depositing a SiN x /AlO x stack followed by forming gas annealing, all samples show improved iVoc (~700 mV with Ga-B co-doped, and ~720 mV with all Ga). Interestingly, when co-doping Ga with B, even a small amount of B in the mixing solution shows negative effects on the surface passivation. Active and total dopant profiles obtained by electrical capacitance voltage and secondary-ion mass spectrometry measurements, respectively, reveal a relatively low percentage of electrically-active Ga and B in the poly-Si and Si layers. Overall, these results help understand the different features of the two dopants: a low ρ c with B, a good passivation with Ga, their degree of activation inside the poly-Si and Si layers, and the annealing effects.

14 SOLAR ENERGY↗

Morphology, microstructure, and doping behaviour: A comparison between different deposition methods for poly-Si/SiO x passivating contacts

In this work, we study how crystallographic structures, optoelectronic properties, and nanoscale surface morphologies of ex situ phosphorus-doped polycrystalline silicon (poly-Si)/SiO x passivating contacts, formed by different deposition methods (sputtering, plasma-enhanced chemical vapour deposition [PECVD], and low-pressure chemical vapour deposition [LPCVD]), are investigated and compared. Across all these deposition technologies, we noted the same trend: higher diffusion temperatures yield films that are more crystalline but that have rougher surface morphologies due to bigger surface crystal grains. Also, the recrystallization process of the as-deposited Si films starts from the SiO x interface, rather than from the film surface and bulk. However, there are some distinct differences among these technologies. First, the LPCVD method yields the lowest deposition rate, roughest surfaces, and smallest degree of crystallinity on finished poly-Si films. In contrast, the PECVD method has the highest deposition rate and smoothest surfaces for both as-deposited Si and annealed poly-Si films. Second, as-deposited sputtered and PECVD Si films contain only an amorphous phase, whereas as-deposited LPCVD films already has some crystalline phase. Third, the LPCVD phosphorus in-diffusion into the substrate depends strongly on the initial film thickness, whereas for the other two methods, it is weakly dependent on thickness. Finally, the passivation quality of every poly-Si film type has different responses to the film thickness and diffusion temperature, suggesting that the ex situ doping optimization should be performed independently.

14 SOLAR ENERGY↗

Deposition pressure dependent structural and optoelectronic properties of ex-situ boron-doped poly-Si/SiO x passivating contacts based on sputtered silicon

Among common methods to form polycrystalline silicon (poly-Si) films for passivating-contact solar cells, physical vapor deposition, in particular sputtering, is the safest one as it does not require any toxic gaseous precursors. One of the critical parameters to control the properties of sputtered silicon films is their deposition pressure. In this work, structural and optoelectronic characteristics of ex-situ boron-doped poly-Si/SiO x passivating contacts, formed from sputtered intrinsic amorphous silicon (a-Si) deposited at different pressures on top of SiO x /c-Si substrates and subjected to a high-temperature boron diffusion step, are investigated. The deposition rate and density of the as-deposited a-Si films increase with reducing pressure. Low-temperature photoluminescence spectra captured from the as-deposited samples at different pressures do not show typical emissions from hydrogenated a-Si. Meanwhile, their Fourier-transform infrared absorption spectra all show Si–H stretching modes, indicating that hydrogen had been initially incorporated into the chemical SiO x layers and eventually hydrogenated the a-Si/SiO x interfaces during the sputtering process. After the high-temperature boron-diffusion step, all hydrogen-related peaks disappear. Lower pressure films (1.5 and 2.5 mTorr) show more consistent improved performance after hydrogen treatments, compared to higher pressure films (4 and 5 mTorr). Overall, the resultant passivating contacts at 2.5 mTorr achieve a low single-side recombination current density Jo of ~9 fA/cm 2 , whereas their contact resistivity is still low at 15 mO cm 2 .

14 SOLAR ENERGY↗

Emission Control from Transition Metal Dichalcogenide Monolayers by Aggregation-Induced Molecular Rotors

Organic–inorganic (O–I) heterostructures, consisting of atomically thin inorganic semiconductors and organic molecules, present synergistic and enhanced optoelectronic properties with a high tunability. Here, we develop a class of air-stable vertical O–I heterostructures comprising a monolayer of transition-metal dichalcogenides (TMDs), including WS 2 , WSe 2 , and MoSe 2 , on top of tetraphenylethylene (TPE) core-based aggregation-induced emission (AIE) molecular rotors. The created O–I heterostructures yields a photoluminescence (PL) enhancement of up to ~950%, ~500%, and ~330% in the top monolayer WS 2 , MoSe 2 , and WSe 2 as compared to PL in their pristine monolayers, respectively. The strong PL enhancement is mainly attributed to the efficient photogenerated carrier process in the AIE luminogens (courtesy of their restricted intermolecular motions in the solid state) and the charge-transfer process in the created type I O–I heterostructures. Moreover, we observe an improvement in photovoltaic properties of the TMDs in the heterostructures including the quasi-Fermi level splitting, minority carrier lifetime, and light absorption. Overall, this work presents an inspiring example of combining stable, highly luminescent AIE-based molecules, with rich photochemistry and versatile applications, with atomically thin inorganic semiconductors for multifunctional and efficient optoelectronic devices.

14 SOLAR ENERGY↗

Extracting Optical Bandgaps from Luminescence Images of Perovskite Solar Cells

We report a camera-based method to capture optical bandgap images of perovskite solar cells (PSCs). It is fast and non-destructive. It can also provide micron-scale spatial resolution. This imaging technique utilizes well-defined and relatively symmetrical band-to-band luminescence spectra emitted from perovskite materials. Their spectra can be fitted with Gaussian functions whose peak locations are similar to absorption thresholds and thus represent the material optical bandgaps. We apply the technique to resolve relative variations in optical bandgaps across various PSCs, and to show optical bandgap inhomogeneity within the same device due to material degradation and impurities. Degradation and impurities were found to both cause optical bandgap shifts inside the materials. Our results are independently confirmed with photoluminescence and absorption spectroscopy.

14 SOLAR ENERGY↗

Origins of hydrogen that passivates bulk defects in silicon heterojunction solar cells

Silicon heterojunction solar cell fabrication incorporates a significant amount of hydrogen into the silicon wafer bulk, and the amount of injected hydrogen is comparable to that introduced by silicon nitride films during a high-temperature firing step. In this work, the origins of the hydrogen injected during heterojunction cell processing have been identified. We demonstrate that the hydrogen plasma treatment that is routinely included to improve surface passivation considerably increases the hydrogen concentration in the wafers. We also show that the hydrogenated amorphous silicon i/p+ stack is more effective than the i/n+ stack for bulk hydrogen incorporation, and both are more effective than intrinsic films alone.

Sun, Chang (ORCID:0000000282140458)↗

Hydrogen-Assisted Defect Engineering of Doped Poly-Si Films for Passivating Contact Solar Cells

Hydrogen-assisted defect engineering, via a hydrogenated silicon nitride (SiN x :H) capping layer, on doped polycrystalline silicon (poly-Si) passivating-contact structures, is explored using complementary techniques. The hydrogen treatment universally improves the passivation quality of poly-Si/SiO x stacks on all samples investigated. Meanwhile, their contact resistivity remains very low at ~6 m$\Omega$cm 2 . Moreover, the nature of charge carrier recombination within the poly-Si films is also investigated by means of photoluminescence. On planar c-Si substrates, the poly-Si films emit two broad photoluminescence peaks ~850-1050 nm and ~1300-1500 nm. The former is the characteristic peak of the hydrogenated amorphous Si (a-Si:H) phase and only appears after the treatment, demonstrating that i) a significant amount of hydrogen has been driven into the poly-Si film and ii) an amorphous phase is present within it. The second peak originates from sub-bandgap radiative defects inside the poly-Si films and increases after the treatment, suggesting a suppression of their non-radiative recombination channels. For films deposited on textured c-Si substrates, there is a disrupted oxide boundary, preventing a build-up of excess carriers inside the films and leading to quenching of the film luminescence.

36 MATERIALS SCIENCE↗

Hydrogenation Mechanisms of Poly-Si/SiO x Passivating Contacts by Different Capping Layers

Herein, posttreatment techniques of phosphorus-doped poly-Si/SiO x passivating contacts, including forming gas annealing (FGA), atomic layer deposition (ALD) of hydrogenated aluminum oxide (AlO x :H), and plasma-enhanced chemical vapor deposition (PECVD) of hydrogenated silicon nitride (SiN x :H), are investigated and compared in terms of their application to silicon solar cells. A simple FGA posttreatment produces a significant increase in the implied open circuit voltage (iV oc ) and the effective minority-carrier lifetime (teff) of high-resistivity crystalline Si (c-Si) samples, whereas low-resistivity samples show a minimal change. Treatment by means of AlO x :H and/or SiN x :H followed by postdeposition FGA results in a universal increase in t eff and iV oc for all substrate resistivities (as high as 12.5 ms and 728 mV for 100 Ω cm and 5.4 ms and 727 mV for 2 Ω cm n-type c-Si substrates). In addition, both the FGA and AlO x :H + FGA techniques can inject sufficient hydrogen into the samples to passivate defects at the SiO x /c-Si and poly-Si/SiO x interfaces. However, this hydrogen concentration is insufficient to neutralize both the nonradiative defects inside the poly-Si films and dangling bonds associated with the amorphous Si phase present in them. The hydrogen injected by the SiN x :H + FGA technique can passivate both the interfaces and the defects and dangling bonds within the poly-Si film. These results are confirmed by low-temperature photoluminescence spectroscopy, Fourier transform infrared spectroscopy, and dynamic secondary-ion mass spectrometry measurements.

14 SOLAR ENERGY↗

Dopant-Free Partial Rear Contacts Enabling 23% Silicon Solar Cells

Over the past five years, there has been a significant increase in both the intensity of research and the performance of crystalline silicon devices which utilize metal compounds to form carrier-selective heterocontacts. Such heterocontacts are less fundamentally limited and have the potential for lower costs compared to the current industry dominating heavily doped, directly metalized contacts. A low temperature (≤230 °C), TiO x /LiF x /Al electron heterocontact is presented here, which achieves mΩcm 2 scale contact resistivities ρ c on lowly doped n-type substrates. Here, as an extreme demonstration of the potential of this heterocontact, it is trialed in a newly developed, high efficiency n-type solar cell architecture as a partial rear contact (PRC). Despite only contacting ≈1% of the rear surface area, an efficiency of greater than 23% is achieved, setting a new benchmark for n-type solar cells featuring undoped PRCs and confirming the unusually low ρ c of the TiO x /LiF x /Al contact. Finally, in contrast to previous versions of the n-type undoped PRC cell, the performance of this cell is maintained after annealing at 350–400 °C, suggesting its compatibility with conventional surface passivation activation and sintering steps.

14 SOLAR ENERGY↗

Imaging Spatial Variations of Optical Bandgaps in Perovskite Solar Cells

A fast, nondestructive, camera-based method to capture optical bandgap images of perovskite solar cells (PSCs) with micrometer-scale spatial resolution is developed. This imaging technique utilizes well-defined and relatively symmetrical band-to-band luminescence spectra emitted from perovskite materials, whose spectral peak locations coincide with absorption thresholds and thus represent their optical bandgaps. The technique is employed to capture relative variations in optical bandgaps across various PSCs, and to resolve optical bandgap inhomogeneity within the same device due to material degradation and impurities. Degradation and impurities are found to both cause optical bandgap shifts inside the materials. The results are confirmed with micro-photoluminescence spectroscopy scans. The excellent agreement between the two techniques opens opportunities for this imaging concept to become a quantified, high spatial resolution, large-area characterization tool of PSCs. This development continues to strengthen the high value of luminescence imaging for the research and development of this photovoltaic technology.

14 SOLAR ENERGY↗

Sub-Bandgap Luminescence from Doped Polycrystalline and Amorphous Silicon Films and Its Application to Understanding Passivating-Contact Solar Cells

We report luminescence phenomena from doped polycrystalline silicon (poly-Si) films and their applications to study carrier transport properties in passivating-contact solar cells. Low-temperature luminescence spectra emitted from doped poly-Si layers are found to be very broad and stretched from the crystalline silicon (c-Si) luminescence peak to significantly lower energies. This suggests that these layers contain radiative defect levels whose energies are continuously distributed from the band edges to deep levels in the poly-Si bandgap. Moreover, photoinduced carriers inside poly-Si layers are found to be completely blocked by an ultrathin SiOx interlayer (~1.3 nm). This demonstrates that there is no free-carrier coupling from poly-Si layers in practical passivating-contact solar cells. Finally, we demonstrate that the same principle can be applied to study carrier transport properties in hydrogenated amorphous silicon films.

14 SOLAR ENERGY↗

Imaging the Thickness of Passivation Layers for Crystalline Silicon with Micron‐Scale Spatial Resolution Using Spectral Photoluminescence

Thin films deposited on crystalline silicon surfaces are critical components of many silicon‐based devices, including high‐efficiency photovoltaic cells. Knowledge of their optical and electronic properties is important in designing and fabricating efficient solar cells, especially as the device complexity increases and includes micron‐scale features. Here, a camera‐based photoluminescence (PL) technique is developed to image the thickness of specific passivating films on silicon wafers. The technique is entirely contactless and nondestructive, requires minimal sample preparation, and provides a large dynamic range in terms of field of view, with micron‐scale spatial resolution possible. It retains the advantages of PL imaging, a mainstream technique for photovoltaic material and device characterization, and it has some extra capabilities similar to those of ellipsometry. This newly developed technique is demonstrated on hydrogenated amorphous silicon and silicon nitride films, two important passivation technologies for high‐efficiency silicon solar cells.

Nguyen, Hieu T.↗

Quantification of Sheet Resistance in Boron-Diffused Silicon Using Micro-Photoluminescence Spectroscopy at Room Temperature

A micro-photoluminescence-based technique is presented, to quantify and map sheet resistances of boron-diffused layers in silicon solar cell precursors with micron-scale spatial resolution at room temperature. The technique utilizes bandgap narrowing effects in the heavily-doped layers, yielding a broader photoluminescence spectrum at the long-wavelength side compared to the spectrum emitted from lightly doped silicon. By choosing an appropriate spectral range as a metric to assess the doping density, the impacts of photon reabsorption on the analysis can be avoided; thus, an accurate characterization of the sheet resistance can be made. This metric is demonstrated to be better representative of the sheet resistance than the surface doping density or the total dopant concentration of the diffused layer. The technique is applied to quantify sheet resistances of 12-um-wide diffused fingers in interdigitated back-contact solar cell precursors and large diffused areas. The results are confirmed by both 4-point probe and time-of-flight secondary-ion mass spectrometry measurements. Lastly, the practical limitations associated with extending the proposed technique into an imaging mode are presented and explained.

14 SOLAR ENERGY↗

Microscopic Distributions of Defect Luminescence From Subgrain Boundaries in Multicrystalline Silicon Wafers

We investigate the microscopic distributions of sub-band-gap luminescence emission (the so-called D-lines D1/D2/D3/D4) and the band-to-band luminescence intensity, near recombination-active sub-grain boundaries in multicrystalline silicon wafers for solar cells. We find that the sub-band-gap luminescence from decorating defects/impurities (D1/D2) and from intrinsic dislocations (D3/D4) have distinctly different spatial distributions, and are asymmetric across the sub-grain boundaries. The presence of D1/D2 is correlated with a strong reduction in the band-to-band luminescence, indicating a higher recombination activity. In contrast, D3/D4 emissions are not strongly correlated with the band-to-band intensity. Based on spatially-resolved, synchrotron-based micro-X-ray fluorescence measurements of metal impurities, we confirm that high densities of metal impurities are present at locations with strong D1/D2 emission but low D3/D4 emission. Finally, we show that the observed asymmetry of the sub-band-gap luminescence across the sub-grain boundaries is due to their inclination below the wafer surface. Based on the luminescence asymmetries, the sub-grain boundaries are shown to share a common inclination locally, rather than be orientated randomly.

14 SOLAR ENERGY↗

A unified approach to modelling the charge state of monatomic hydrogen and other defects in crystalline silicon

There are a number of existing models for estimating the charge states of defects in silicon. In order of increasing complexity, these are (a) the Fermi-Dirac distribution, (b) the Shockley-Last model, (c) the Shockley-Read-Hall model, and (d) the Sah-Shockley model. In this work, we demonstrate their consistency with the general occupancy ratio α, and show that this parameter can be universally applied to predict the charge states of both monovalent and multivalent deep levels, under either thermal equilibrium or steady-state conditions with carrier injection. The capture cross section ratio is shown to play an important role in determining the charge state under non-equilibrium conditions. The application of the general occupancy ratio is compared with the quasi-Fermi levels, which are sometimes used to predict the charge states in the literature, and the conditions where the latter can be a good approximation are identified. The general approach is then applied to the prediction of the temperature- and injection level-dependent charge states for the technologically important case of multivalent monatomic hydrogen, and several other key monovalent deep levels including Fe, Cr, and the boron-oxygen complex in silicon solar cells. For the case of hydrogen, we adapt the model of Herring et al., which describes the charge states of hydrogen in thermal equilibrium, and generalize it for non-equilibrium conditions via the inclusion of the general occupancy ratio, while retaining the pre-factors which make the model more complete. Based on these results, the impact of temperature and injection on the hydrogenation of the key monovalent defects, and other pairing reactions, are discussed, demonstrating that the presented model provides a rigorous methodology for understanding the impact of charge states.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Hydrogen passivation of interstitial iron in boron-doped multicrystalline silicon during annealing

Effective hydrogenation of interstitial iron in boron-doped multicrystalline silicon wafers is reported. The multicrystalline silicon wafers were annealed with plasma-enhanced chemical vapour deposited silicon nitride films, at temperatures of 400 °C – 900 °C and for times from minutes to hours. At low temperatures where a combined effect of hydrogenation and precipitation of dissolved Fe is expected, results show that the hydrogenation process dominates the effect of precipitation. The concentrations of dissolved interstitial iron reduce by more than 90% after a 30-min anneal at temperatures between 600 and 900 °C. The most effective reduction occurs at 700 °C, where 99% of the initial dissolved iron is hydrogenated after 30 min. The results show that the observed reductions in interstitial Fe concentrations are not caused by the internal gettering of Fe at structural defects or by an enhanced diffusivity of Fe due to the presence of hydrogen. The hydrogenation process is conjectured to be the pairing of positively charged iron with negatively charged hydrogen, forming less recombination active Fe-H complexes in silicon.

36 MATERIALS SCIENCE↗