24 records · Page 2

High Ductility Aluminum Alloy made from Powder by Friction Extrusion

Shear processing has been used to consolidate and extrude aluminum alloy Al-12.4TM powder into bulk nanostructured rods. Extrudates exhibited 450 MPa ultimate tensile strength, 380 MPa yield strength, and 15.7% elongation at ambient temperature. Twice the elongation was achieved compared to conventional extrusion, with similar ultimate and yield strengths, and is attributed to reduction of the Al grain size and refinement and redistribution of nanoscale second phases. Quasicrystalline approximants within the starting powder were not observed in the extrudate, indicating shear processing was effective in solutionizing some fraction of the alloying elements and re-precipitating them as second phase nanoscale intermetallics.

Extrusion, Friction, Nanostructured Materials, Alu↗

Self-learning kinetic Monte Carlo simulations of diffusion in ferromagnetic α -Fe–Si alloys

Diffusion in α-Fe-Si alloys is studied using AKSOME, an on-lattice self-learning KMC code, in the ferromagnetic state. Si diffusivity in the α-Fe matrix were obtained with and without the magnetic disorder in various temperature ranges. In addition we studied vacancy diffusivity in ferromagnetic α-Fe at various Si concentrations up to 12.5at.% in the temperature range of 350–550 K. The results were compared with available experimental and theoretical values in the literature. Local Si-atom dependent activation energies for vacancy hops were calculated using a broken-model and were stored in a database. The migration barrier and prefactors for Si-diffusivity were found to be in reasonable agreement with available modeling results in the literature. Magnetic disorder has a larger effect on the prefactor than on the migration barrier. Prefactor was approximately an order of magnitude and the migration barrier a tenth of an electron-volt higher with magnetic disorder when compared to a fully ferromagnetic ordered state. In addition, the correlation between various have a larger effect on the Si-diffusivity extracted in various temperature range than the magnetic disorder. In the case of vacancy diffusivity, the migration barrier more or less remained constant while the prefactor decreased with increasing Si concentration in the disordered or A2-phase of Fe-Si alloy. Important vacancy-Si/Fe atom exchange processes and their activation barriers were also identified and discuss the effect of energetics on the formation of ordered phases in Fe-Si alloys.

AKSOME↗

Friction consolidation of gas-atomized Fe−Si powders for soft magnetic applications

Soft magnetic materials are often limited in scalability due to conventional processes that do not retain beneficial microstructures, and their associated physical properties, during densification. In this work, friction consolidation (FC) has been studied to fabricate Fe−Si soft magnetic materials from gas-atomized powder precursors. Fe−Si powder is consolidated using variable pressure and tool rotation speed in an effort to evaluate this unique densification approach for potential improvements in magnetic properties. FC, due to the high shear deformation involved, is shown to result in uniform gradual grain structure refinement across the consolidated workpiece from the center nearest the tool to the edge. Magnetic properties along different orientations indicate little, if any, textural orientation in the refined grain structure. The effect of annealing on the magnetic properties is evaluated and shown to decrease coercivity. FC processing was able to retain the magnetization of the original gas-atomized powders but further process optimization is needed to reach the optimal coercivity for the soft magnetic materials applications. - Highlights: •Friction stir processing was utilized to consolidate Fe−Si soft magnetic powders. •The resultant microstructure and magnetic properties were correlated to the processing conditions. •Friction consolidation refined the grain size of the materials by ~ 40%. •Annealing successfully reduced the coercivity induced by the stress during processing. •The results shine light on the possible scaling up of nanostructured materials.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of a novel rapidly solidified, high-temperature Al-alloy

Rapid solidification (RS) processing, as a production method, offers a variety of unique properties based on far-from-equilibrium microstructures obtained through rapid cooling rates. In this study, we seek to investigate the microstructures and properties of a novel Al-alloy specifically designed for high temperature mechanical stability. Synthesis of, AlFe{sub 11.4}Si{sub 1.8}V{sub 1.6}Mn{sub 0.9} (wt.%), was performed by two approaches: rotating cup atomization (“shot”) and melt spinning (“flake”). These methods were chosen because of their ability to produce alloys with tailored microstructures due to their inherent differences in cooling rate. The as-solidified precursor materials were microstructurally characterized with electron microscopy. The results show that the higher cooling rate flake material exhibited the formation of nanocrystalline regions as well additional phase morphologies not seen in the shot material. Secondary dendritic branching in the flake material was on the order of 0.1–0.25 μm whereas branching in the shot material was 0.5–1.0 μm. Consolidated and extruded material from both precursor materials was mechanically evaluated at both ambient and high (300 °C) temperature. The consolidated RS flake material is shown to exhibit higher strengths than the shot material. The ultimate tensile strength of the melt spun flake was reported as 544.2 MPa at room temperature and 298.0 MPa at 300 °C. These results forecast the ability to design alloys and processing approaches with unique non-equilibrium microstructures with robust mechanical properties at elevated temperatures. - Highlights: • A novel alloy, AlFe{sub 11.4}Si{sub 1.8}V{sub 1.6}Mn{sub 0.9} was fabricated by rapid solidification. • Room temperature yield strength exceeded 500 MPa. • Elevated temperature (300 °C) yield strength exceeded 275 MPa. • Forging, after extrusion of the alloy resulted in microstructural coarsening. • Decreased strength and ductility was identified as a result of forging.

36 MATERIALS SCIENCE↗

Thermal Stability: The Next Frontier for Nanocrystalline Materials

For the past quarter decade, the science and technology of nanocrystalline materials (materials with grain sizes less than 100 nm) has been an extremely rich and diverse field of study.1,2 Generally, it has been observed that tremendous improvements in physical and mechanical properties, including order-of-magnitude increases in yield strength, are possible.2 As predicted by the Hall– Petch equation,3,4 a reduction in grain size should be accompanied by an increase in strength. But, despite the promise of nanocrystalline materials for a host of structural and functional applications, their use has been severely limited by their lack of microstructural stability at elevated temperatures5 or under mechanical loads.6,7 In the case of pure metals, this coarsening often occurs even at ambient temperatures.5 Ironically, the same features that often result in the enhancement of properties in nanocrystalline materials, namely the high volume fraction of high-energy grain boundaries, are responsible for the observed grain growth or phase transformation.8

Mathaudhu, Suveen↗