(De)lithiation of spinel ferrites Fe3O4, MgFe2O4, and ZnFe2O4: a combined spectroscopic, diffraction and theory study
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to McCarthy, Alison H..
Explore the source record for details and available documents.
Ni-rich NMC is an attractive Li-ion battery cathode due to its combination of energy density, thermal stability, and reversibility. While higher delivered energy density can be achieved with a more positive charge voltage limit, this approach compromises sustained reversibility. Improved understanding of the local and bulk structural transformations as a function of charge voltage, and their associated impacts on capacity fade are critically needed. Through simultaneous operando synchrotron X-ray diffraction (XRD) and X-ray absorption spectroscopy (XAS) of cells cycled at 3–4.3 or 3–4.7 V, this study presents an in-depth investigation into the effects of voltage window on local coordination, bulk structure, and oxidation state. These measurements are complemented by ex situ X-ray fluorescence (XRF) mapping and scanning electrochemical microscopy mapping (SECM) of the negative electrode, X-ray photoelectron spectroscopy (XPS) of the positive electrode, and cell level electrochemical impedance spectroscopy (EIS). Initially, cycling between 3 and 4.7 V leads to greater delivered capacity due to greater lithium extraction, accompanied by increased structural distortion, moderately higher Ni oxidation, and substantially higher Co oxidation. Continued cycling at this high voltage results in suppressed Ni and Co redox, greater structural distortion, increased levels of transition metal dissolution, higher cell impedance, and 3× greater capacity fade.
The phase distribution of lithiated LVO in thick (~500 μm) porous electrodes (TPEs) designed to facilitate both ion and electron transport was determined using synchrotron-based operando energy dispersive X-ray diffraction (EDXRD). Probing 3 positions in the TPE while cycling at a 1C rate revealed a homogeneous phase transition across the thickness of the electrode at the 1st and 95th cycles. Additionally, continuum modelling indicated uniform lithiation across the TPE in agreement with the EDXRD results and ascribed decreasing accessible active material to be the cause of loss in delivered capacity between the 1st and 95th cycles. The model was supported by the observation of significant particle fracture by SEM consistent with loss of electrical contact. Overall, the combination of operando EDXRD, continuum modeling, and ex situ measurements enabled a deeper understanding of lithium vanadium oxide transport properties under high rate extended cycling within a thick highly porous electrode architecture.
Not Available
A primary barrier preventing repetitive fast charging of Li-ion batteries is lithium metal plating at the graphite anode. One approach toward mitigating Li metal deposition is the deliberate modification of the graphite anode surface with materials demonstrating high overpotentials unfavorable for Li metal nucleation, such as Ni or Cu nanoscale films. This research explores Ni and Cu surface coatings at different areal loadings (3 or 11 μg cm -2 ) on the electrochemistry of graphite/LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) type Li-ion batteries. Extended galvanostatic cycling of control and metal-coated electrodes in graphite/NMC622 pouch cells are conducted under high rate conditions. Based on the overpotential of Li deposition on metal foil, both Ni and Cu treatments were anticipated to result in reduced lithium deposition. The higher metal film loadings of 11 μg cm -2 Ni- or Cu-coated electrodes exhibit the highest capacity retention after 500 cycles, with mean improvements of 8% and 9%, respectively, over uncoated graphite electrodes. Li plating quantified by X-ray diffraction indicates that the metal films effectively reduce the quantity of plated Li compared to untreated electrodes, with 11 μg cm -2 Cu providing the greatest benefit.
A full depth of discharge mathematical model for the lithium trivanadate cathode, considering lithiation of the layered α-phase, phase change, and lithiation of the rock-salt like β-phase at lower potentials, is developed. The coupled electrode-scale and crystal-scale model is fit to electrochemical data, and additionally validated with operando EDXRD. There is good agreement between the simulated and measured spatial variation of the volume fraction of the β-phase. This mathematical model is used to guide electrode fabrication, accounting for both ionic and electronic transport effects. Values of three design parameters—electrode thickness, porosity, and volume fraction of conductor—are identified, and the sensitivity of the energy density to these design parameters is quantified. The model is also used to investigate electrode design to create electrodes that deliver the maximum achievable energy density under the constraint that the α to β-phase transition is avoided, since phase change has been demonstrated to reduce cycle life. The energy density sacrificed to avoid phase change decreases at higher discharge rates, but the target values for electrode fabrication remain the same as those when optimizing the electrode for the full depth of discharge.
Water-in-salt (WIS) electrolytes provide a promising path toward aqueous battery systems with enlarged operating voltage windows for better safety and environmental sustainability. In this work, a new electrode couple, LiV 3 O 8 -LiMn 2 O 4 , for aqueous Li-ion batteries is investigated to understand the mechanism by which the WIS electrolyte improves the cycling stability at an extended voltage window. Operando synchrotron transmission x-ray microscopy on the LiMn 2 O 4 cathode reveals that the WIS electrolyte suppresses the mechanical damage to the electrode network and dissolution of the electrode particles, in addition to delaying the water decomposition process. Because the viscosity of WIS is notably higher, the reaction heterogeneity of the electrodes is quantified with x-ray absorption spectroscopic imaging, visualizing the kinetic limitations of the WIS electrolyte. This work furthers the mechanistic understanding of electrode–WIS electrolyte interactions and paves the way to explore the strategy to mitigate their possible kinetic limitations in three-dimensional architectures.