Search NASA⌕ Search

Engineering topics

McShane, Eric J.

Publications and source records attributed to McShane, Eric J..

Steam‐Assisted Selective CO 2 Hydrogenation to Ethanol over Ru−In Catalysts

Abstract Multicomponent catalysts can be designed to synergistically combine reaction intermediates at interfacial active sites, but restructuring makes systematic control and understanding of such dynamics challenging. We here unveil how reducibility and mobility of indium oxide species in Ru‐based catalysts crucially control the direct, selective conversion of CO 2 to ethanol. When uncontrolled, reduced indium oxide species occupy the Ru surface, leading to deactivation. With the addition of steam as a mild oxidant and using porous polymer layers to control In mobility, Ru−In 2 O 3 interface sites are stabilized, and ethanol can be produced with superior overall selectivity (70 %, rest CO). Our work highlights how engineering of bifunctional active ensembles enables cooperativity and synergy at tailored interfaces, which unlocks unprecedented performance in heterogeneous catalysts.

Zhou, Chengshuang↗

Steam-Assisted Selective CO 2 Hydrogenation to Ethanol over Ru–In Catalysts

Multicomponent catalysts can be designed to synergistically combine reaction intermediates at interfacial active sites, but restructuring makes systematic control and understanding of such dynamics challenging. In this work, we unveil how reducibility and mobility of indium oxide species in Ru-based catalysts crucially control the direct, selective conversion of CO 2 to ethanol. When uncontrolled, reduced indium oxide species occupy the Ru surface, leading to deactivation. With the addition of steam as a mild oxidant and using porous polymer layers to control In mobility, Ru–In 2 O 3 interface sites are stabilized, and ethanol can be produced with superior overall selectivity (70 %, rest CO). Our work highlights how engineering of bifunctional active ensembles enables cooperativity and synergy at tailored interfaces, which unlocks unprecedented performance in heterogeneous catalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Combined, time-resolved, in situ neutron reflectometry and X-ray diffraction analysis of dynamic SEI formation during electrochemical N 2 reduction

One means of improving performance for electrochemical ammonia production through the Li-mediated N 2 reduction reaction (Li-NRR) is by cycling the current driving the reaction between open-circuit conditions and periods of applied current density. Herein, we have investigated the dynamics of the electrode–electrolyte interface under Li-NRR conditions during current cycling using in situ time-resolved neutron reflectometry and grazing-incidence synchrotron X-ray diffraction. During cycling, measured neutron reflectivity curves indicated bilayer formation in which Li-containing species such as LiOH, Li 2 O, and small quantities of Li 3 N and metallic Li primarily appeared in a thin layer at the cathode surface, above which formed a much larger, porous, ‘solid–electrolyte interface’ (SEI) layer. Upon return to open-circuit conditions, Li-containing species quickly moved out of the thin layer, leaving a compact, stable layer of decomposition products underneath the SEI layer. This SEI layer concomitantly filled with electrolyte or dissolved, becoming indistinguishable from the electrolyte via contrast in scattering-length density (SLD). During the second current cycle, Li-containing species again preferentially deposited directly atop the cathode, with the thick SEI-like layer again appearing within a minute. This SEI layer exhibited a lower SLD more quickly than in the first cycle, which might suggest that Li-containing species become distributed within the porous SEI layer. Furthermore, these time-resolved observations of SEI and plated layers during current cycling suggest that benefits associated with return to open-circuit conditions between periods of applied current density may be related to the concomitant loss of Li-containing species from a thin layer at the cathode surface into a porous SEI layer that becomes filled with electrolyte or dissolves.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-throughput Li plating quantification for fast-charging battery design

Fast charging of most commercial lithium-ion batteries is limited due to fear of lithium plating on the graphite anode, which is difficult to detect and poses considerable safety risk. In this report we demonstrate the power of simple, accessible and high-throughput cycling techniques to quantify irreversible Li plating spanning data from over 200 cells. We first observe the effects of energy density, charge rate, temperature and state of charge on lithium plating, use the results to refine a mature physics-based electrochemical model and provide an interpretable empirical equation for predicting the plating onset state of charge. We then explore the reversibility of lithium plating and its connection to electrolyte design for preventing irreversible Li accumulation. Finally, we design a method to quantify in situ Li plating for commercially relevant graphite|LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC) cells and compare with results from the experimentally convenient Li|graphite configuration. The hypotheses and abundant data herein were generated primarily with equipment universal to the battery researcher, encouraging further development of innovative testing methods and data processing that enable rapid battery engineering.

25 ENERGY STORAGE↗

Multimodal quantification of degradation pathways during extreme fast charging of lithium-ion batteries

Enabling fast charging of Li-ion batteries will be a key step towards realizing the technology's full potential in electric vehicles. Currently, fast charging is limited by a variety of processes that reduce cell capacity upon extended cycling. Using a multimodal approach combining incremental capacity analysis (dQ/dV), high energy X-ray diffraction (HEXRD), and mass spectrometry titration (MST), we identify specific degradation mechanisms—including Li plating, dead Li x C 6 formation, Li 2 C 2 formation, solid carbonate solid-electrolyte interphase (SEI) deposition, and loss of positive electrode active material (LAM PE )—that occur during extended fast charge cycling. We find that Li plating is the major source of capacity loss in cells cycled at 6C, while non-carbonate SEI species deposition on the graphite anode is the main source of capacity loss when cycled at 4C. We also study local degradative phenomena by examining specific ~1–5 cm 2 regions of the cells using HEXRD and MST. Here, we find that plated Li is often collocated with dead Li x C 6 , Li 2 C 2 , and solid carbonate SEI species, and these additional species cumulatively account for ~20% of the capacity lost during 6C cycling. Finally, in a cell with an anomalously high amount of LAM PE (quantified via dQ/dV), we find that regions of cathode degradation were accompanied by non-carbonate SEI products on the adjacent region of the anode. We postulate that this phenomenon arises due to crosstalk between the electrodes, wherein soluble electrolyte oxidation products formed at the delithiated cathode migrate to the graphite anode and are ultimately deposited on the graphite surface. This work demonstrates the utility of combining multiple characterization techniques to reveal a more holistic understanding of degradative phenomena that occur across multiple length scales during fast charge.

25 ENERGY STORAGE↗

Quantifying Graphite Solid-Electrolyte Interphase Chemistry and its Impact on Fast Charging

The solid-electrolyte interphase (SEI) enables the remarkable capacity retention of lithium-ion batteries, yet a comprehensive quantitative description of the SEI composition remains elusive. Using a combination of differential electrochemical mass spectrometry and mass spectrometry titration, we quantify graphite SEI components formed under electrolytes of varying salt concentrations. We find that, regardless of salt concentration, a conversion of initially deposited lithium ethylene dicarbonate to monocarbonates (likely lithium ethylene monocarbonate) and noncarbonate species occurs, and the extent of this conversion increases with electrolyte aging. Here, we additionally demonstrate that as the concentration increases (up to 2.0 M LiPF6), the SEI becomes progressively thinner with more LiF and less solid carbonates deposited. Finally, we reveal that less dead lithium formation and less solid carbonate deposition occur during prolonged fast charging for higher-concentration electrolytes. Because of the advantages imparted by a thinner SEI, the onset state of charge for lithium plating for the 2.0 M electrolyte is later than that predicted by a standard electrochemical model, underscoring the importance of explicit SEI effects in future electrochemical models.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Detecting onset of lithium plating during fast charging of Li-ion batteries using operando electrochemical impedance spectroscopy

Electrochemical plating of Li metal on the graphite electrode is the key limitation behind slow charging times of Li-ion batteries (LIBs) in electric vehicles (EVs). Currently, electrochemical methods to detect the onset of Li plating while a battery is fast charging are sparse. In this study, we use operando electrochemical impedance spectroscopy to reliably detect the onset of Li plating on graphite electrodes in three-electrode LIBs. An increase in the graphite solid-electrolyte interface (SEI) resistance indicates that Li plating has occurred. By cross-validating with a highly sensitive ex situ chemical titration, we determine that this technique can detect very small amounts of plated Li (<0.6% of the graphite electrode's capacity). We also offer physical explanations for the observed impedance behavior. Finally, we show that this technique can be applied to standard two-electrode LIB systems, making the method an important step toward safely implementing fast charging protocols for LIBs in EVs.

25 ENERGY STORAGE↗

A Review of Existing and Emerging Methods for Lithium Detection and Characterization in Li-Ion and Li-Metal Batteries

Whether attempting to eliminate parasitic Li metal plating on graphite (and other Li-ion anodes) or enabling stable, uniform Li metal formation in ‘anode-free’ Li battery configurations, the detection and characterization (morphology, microstructure, chemistry) of Li that cannot be reversibly cycled is essential to understand the behavior and degradation of rechargeable batteries. In this review, various approaches used to detect and characterize the formation of Li in batteries are discussed. Each technique has its unique set of advantages and limitations, and works towards solving only part of the full puzzle of battery degradation. Going forward, multimodal characterization holds the most promise towards addressing two pressing concerns in the implementation of the next generation of batteries in the transportation sector (viz. reducing recharging times and increasing the available capacity per recharge without sacrificing cycle life). Such characterizations involve combining several techniques (experimental- and/or modeling-based) in order to exploit their respective advantages and allow a more comprehensive view of cell degradation and the role of Li metal formation in it. Additionally, it is also discussed which individual techniques, or combinations thereof, can be implemented in real-world battery management systems on-board electric vehicles for early detection of potential battery degradation that would lead to failure.

25 ENERGY STORAGE↗

Quantification of Inactive Lithium and Solid–Electrolyte Interphase Species on Graphite Electrodes after Fast Charging

Rapid charging of Li-ion batteries is limited by lithium plating on graphite anodes, whereby Li+ ions are reduced to Li metal on the graphite particle surface instead of inserting between graphitic layers, which directly contributes to cell capacity loss because of the low reversibility of the Li plating/stripping process. Furthermore, precisely identifying the onset and amount of Li plating is therefore vital in order to remedy these issues. We demonstrate a titration technique with a detection limit of 20 nmol (5 × 10 –4 mAh) of Li that can be used to quantify inactive Li that remains on the graphite electrode after fast charging. The titration is extended to quantify the total amount of solid carbonate species and lithium acetylide (Li 2 C 2 ) within the solid–electrolyte interphase (SEI), and electrochemical modeling is used to determine the Li plating exchange current density (10 A/m 2 ) and stripping efficiency (65%) of plated Li metal on graphite. These techniques provide a highly accurate measure of the onset of Li plating and quantitative insight into graphite SEI evolution during fast charging.

25 ENERGY STORAGE↗