IMPACT OF NUCLEAR MATERIAL DISSOLUTION ON VESSEL CORROSION

Different nuclear materials require different processing conditions. In order to maximize the dissolver vessel lifetime, corrosion testing was conducted for a range of chemistries and temperature used in fuel dissolution. Compositional ranges of elements regularly in the dissolver were evaluated for corrosion of 304L, the material of construction. Corrosion rates of AISI Type 304 stainless steel coupons, both welded and non-welded coupons, were calculated from measured weight losses and post-test concentrations of soluble Fe, Cr and Ni.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

CORROSION TESTING OF CARBON STEEL IN OXALIC ACID CHEMICAL CLEANING SOLUTIONS

Radioactive liquid waste has been stored in underground carbon steel tanks for nearly 60 years at the Savannah River Site. The site is currently in the process of removing the waste from these tanks in order to place it into vitrified, stable state for longer term storage. The last stage in the removal sequence is a chemical cleaning step that breaks up and dissolves metal oxide solids that cannot be easily pumped out of the tank. Oxalic acid has been selected for this purpose because it is an effective chelating agent for the solids and is not as corrosive as other acids. Electrochemical and immersion studies were conducted to investigate the corrosion behavior of carbon steel in simulated chemical cleaning environments. The effects of temperature, agitation, and the presence of sludge solids in the oxalic acid on the corrosion rate and the likelihood of hydrogen evolution were determined. The testing showed that the corrosion rates decreased significantly in the presence of the sludge solids. Corrosion rates increased with agitation, however, the changes were less noticeable.

08 HYDROGEN↗

PREDICTION OF DISSOLVER LIFETIMES THROUGH NON-DESTRUCTIVE EVALUATION AND LABORATORY TESTING

Non-destructive evaluation was used as the primary method of monitoring the corrosion degradation of nuclear material dissolvers and assessing the remaining lifetimes. Materials were typically processed in nitric acid based (4-14M) solutions containing fluoride concentrations less than 0.2 M. The primary corrosion issue for the stainless steel dissolvers is the occurrence of localized corrosion near the tank bottom and the heat affected zones of the welds. Laboratory data for a range of operational conditions, including solution chemistry and temperature, was used to assess the impact of processing changes on the dissolver corrosion rate. Experimental and NDE-based general corrosion rates were found to be in reasonable agreement for standard dissolution chemistries consisting of nitric acid with fluorides and at temperatures less than 95 C. Greater differences were observed when chloride was present as an impurity and temperatures exceeded 100 C.

36 MATERIALS SCIENCE↗

DEPOSITION TANK CORROSION TESTING FOR ENHANCED CHEMICAL CLEANING POST OXALIC ACID DESTRUCTION

An Enhanced Chemical Cleaning (ECC) process is being developed to aid in the high level waste tank closure at the Savannah River Site. The ECC process uses an advanced oxidation process (AOP) to destroy the oxalic acid that is used to remove residual sludge from a waste tank prior to closure. The AOP process treats the dissolved sludge with ozone to decompose the oxalic acid through reactions with hydroxyl radicals. The effluent from this oxalic acid decomposition is to be sent to a Type III waste tank and may be corrosive to these tanks. As part of the hazardous simulant testing that was conducted at the ECC vendor location, corrosion testing was conducted to determine the general corrosion rate for the deposition tank and to assess the susceptibility to localized corrosion, especially pitting. Both of these factors impact the calculation of hydrogen gas generation and the structural integrity of the tanks, which are considered safety class functions. The testing consisted of immersion and electrochemical testing of A537 carbon steel, the material of construction of Type III tanks, and 304L stainless steel, the material of construction for transfer piping. Tests were conducted in solutions removed from the destruction loop of the prototype ECC set up. Hazardous simulants, which were manufactured at SRNL, were used as representative sludges for F-area and H-area waste tanks. Oxalic acid concentrations of 1 and 2.5% were used to dissolve the sludge as a feed to the ECC process. Test solutions included the uninhibited effluent, as well as the effluent treated for corrosion control. The corrosion control options included mixing with an inhibited supernate and the addition of hydroxide. Evaporation of the uninhibited effluent was also tested since it may have a positive impact on reducing corrosion. All corrosion testing was conducted at 50 C. The uninhibited effluent was found to increase the corrosion rate by an order of magnitude from less than 1 mil per year (mpy) for an inhibited waste to a range of 5 to 23.4 mpy, depending on sludge chemistry. F-area-based effluents were, in general, more corrosive. Effective corrosion control measures included evaporation, hydroxide additions and mixing with supernates containing a representative supernate chemistry (5 M hydroxide and 1.5 M nitrite). Corrosion rates with these measures were generally 0.2 mpy. The A537 carbon steel was found to be susceptible to pitting when the corrosion control measure involved mixing the ECC effluent with a supernate chemistry having minimal inhibitor concentrations (0.5 M hydroxide and 0.3 M nitrite). Corrosion rates in this case were near 1 mpy.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

TESTING OF 304L STAINLESS STEEL IN NITRIC ACID ENVIRONMENTS WITH FLUORIDES AND CHLORIDES

Impure radioactive material processed in nitric acid solutions resulted in the presence of chlorides in a dissolver fabricated from 304L stainless steel. An experimental program was conducted to study the effects of chloride in nitric acid/fluoride solutions on the corrosion of 304L stainless steel. The test variables included temperature (80, 95, and 110 C) and the concentrations of nitric acid (6, 12, and 14 M), fluoride (0.01, 0.1, and 0.2 M) and chloride (100, 350, 1000, and 2000 ppm). The impact of welding was also investigated. Results showed that the chloride concentration alone was not a dominant variable affecting the corrosion, but rather the interaction of chloride with fluoride significantly affected corrosion.

36 MATERIALS SCIENCE↗

PASSIVATION LAYER STABILITY OF A METALLIC ALLOY WASTE FORM

Alloy waste form development under the Waste Forms Campaign of the DOE-NE Fuel Cycle Research & Development program includes the process development and characterization of an alloy system to incorporate metal species from the waste streams generated during nuclear fuel recycling. This report describes the tests and results from the FY10 activities to further investigate an Fe-based waste form that uses 300-series stainless steel as the base alloy in an induction furnace melt process to incorporate the waste species from a closed nuclear fuel recycle separations scheme. This report is focused on the initial activities to investigate the formation of oxyhydroxide layer(s) that would be expected to develop on the Fe-based waste form as it corrodes under aqueous repository conditions. Corrosion tests were used to evaluate the stability of the layer(s) that can act as a passivation layer against further corrosion and would affect waste form durability in a disposal environment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

RESIDUAL STRESSES IN 3013 CONTAINERS

The DOE Complex is packaging plutonium-bearing materials for storage and eventual disposition or disposal. The materials are handled according to the DOE-STD-3013 which outlines general requirements for stabilization, packaging and long-term storage. The storage vessels for the plutonium-bearing materials are termed 3013 containers. Stress corrosion cracking has been identified as a potential container degradation mode and this work determined that the residual stresses in the containers are sufficient to support such cracking. Sections of the 3013 outer, inner, and convenience containers, in both the as-fabricated condition and the closure welded condition, were evaluated per ASTM standard G-36. The standard requires exposure to a boiling magnesium chloride solution, which is an aggressive testing solution. Tests in a less aggressive 40% calcium chloride solution were also conducted. These tests were used to reveal the relative stress corrosion cracking susceptibility of the as fabricated 3013 containers. Significant cracking was observed in all containers in areas near welds and transitions in the container diameter. Stress corrosion cracks developed in both the lid and the body of gas tungsten arc welded and laser closure welded containers. The development of stress corrosion cracks in the as-fabricated and in the closure welded container samples demonstrates that the residual stresses in the 3013 containers are sufficient to support stress corrosion cracking if the environmental conditions inside the containers do not preclude the cracking process.

42 ENGINEERING↗

DETERMINATION OF CORROSION INHIBITOR CRITERIA FOR TYPE III/IIIA TANKS DURING SALT DISSOLUTION OPERATIONS SUMMARY DOCUMENT

Dissolution of salt from Type III/IIIA waste tanks at the Savannah River Site may create solutions with inhibitor concentrations below those currently required (0.6M OH{sup -} and 1.1M OH{sup -} + NO{sub 2}{sup -}) per the Corrosion Control Program for high nitrate salt solutions (5.5 to 8.5M NO{sub 3}{sup -}). An experimental program was conducted to evaluate the corrosion susceptibility of grade A537 carbon steel for waste simulants containing 4.5-8.5M NaNO{sub 3} with maximum inhibitor concentrations of 0.6M NaOH and 0.2M NaNO{sub 2}. These maximum inhibitor concentrations used in this program are at a reduced level from those currently required. Current requirements were initially established for the Types I, II and IV tanks made of A285 carbon steel. The experimental program involved corrosion testing to evaluate the pitting and stress corrosion stress corrosion cracking (SCC) susceptibility of the Type III/IIIA waste tank materials. The program was conducted in two phases; the results of the first phase were reported previously (WSRC-STI-2006-00029). In this second phase, the corrosion specimens were modified to represent the 'as-fabricated' condition of the tank wall, and included specimens with mill scale, ground welds and stress-relief heat treatments. The complete description of the corrosion testing and the results are reported herein. The collective corrosion test results for A537 carbon steel in high nitrate waste simulants (4.5 - 8.5M) with the maximum inhibitor concentrations of 0.6M NaOH and 0.2M NaNO{sub 2} were as follows: (1) In long-term non-polarized U-bend testing, heat treatment, similar to the waste tank stress relief regime, reduced the incidence of cracking over the 18-month test period. Vapor space SCC was found to initiate on non-heat treated U-bend coupons. (2) In polarized U-bend testing, cracking occurred on U-bend coupons that had welds prepared similar to those in the waste tanks, i.e. ground and heat treated. (3) In electrochemical testing, pitting occurred on all coupons independent of heat treatment, inhibitor concentration, temperature, surface preparation, or welding. (4) In slow strain rate testing, cracking occurred on samples tested in solutions containing up to the maximum inhibitor concentration. The primary conclusion derived from this experimental program is that A537 carbon steel exposed to high nitrate (> 5.5M) solutions at inhibitor levels below the current specifications (0.6M OH{sup -} and 1.1M OH{sup -} + NO{sub 2}{sup -}) are susceptible to localized corrosion in the form of pitting and stress corrosion cracking. Long-term storage (e.g., greater than 100 days) of dissolved salt solutions not meeting the current inhibitor specifications for high nitrate salt chemistries in Type III waste tanks shall be avoided. Short term storage (e.g., less than 100 days) at low temperatures (e.g., less than 50 C) in these tanks is permissible for waste removal purposes. The stress relief process reduces the risk of SCC in the Type III waste tanks. On the other hand, the current inhibitor specifications should be strictly followed for the Type I, II and IV waste chemistry to prevent initiation of localized corrosion mechanisms. These tanks were not stress relieved and are more susceptible to SCC.

36 MATERIALS SCIENCE↗

DEGRADATION EVALUATION OF HEAVY WATER DRUMS AND TANKS

Heavy water with varying chemistries is currently being stored in over 6700 drums in L- and K-areas and in seven tanks in L-, K-, and C-areas. A detailed evaluation of the potential degradation of the drums and tanks, specific to their design and service conditions, has been performed to support the demonstration of their integrity throughout the desired storage period. The 55-gallon drums are of several designs with Type 304 stainless steel as the material of construction. The tanks have capacities ranging from 8000 to 45600 gallons and are made of Type 304 stainless steel. The drums and tanks were designed and fabricated to national regulations, codes and standards per procurement specifications for the Savannah River Site. The drums have had approximately 25 leakage failures over their 50+ years of use with the last drum failure occurring in 2003. The tanks have experienced no leaks to date. The failures in the drums have occurred principally near the bottom weld, which attaches the bottom to the drum sidewall. Failures have occurred by pitting, crevice and stress corrosion cracking and are attributable, in part, to the presence of chloride ions in the heavy water. Probable degradation mechanisms for the continued storage of heavy water were evaluated that could lead to future failures in the drum or tanks. This evaluation will be used to support establishment of an inspection plan which will include susceptible locations, methods, and frequencies for the drums and tanks to avoid future leakage failures.

36 MATERIALS SCIENCE↗

ASSESSMENT OF RESIDUAL STRESSES IN SRS AND HANFORD 3013 INNER AND CONVENIENCE CANS

Chloride stress corrosion cracking (SCC) is a plausible corrosion mechanism for the stainless steel 3013 containers during their lifetime for plutonium material storage if sufficient electrolyte is present within the container. Contributing factors for SCC, such as fabrication and welding residual stresses, are present in the 3013 cans. Convenience and inner cans from both Hanford and SRS are made by a flow form process, which cold works the stainless steel during fabrication. Additionally, the inner cans also are sealed at the can top with a closure weld to the sealing plug. Only SRS and Hanford were tested since moisture levels were significant for SCC. As part of the 3013 corrosion plan for FY09, testing in a boiling magnesium chloride solution was performed on actual 3013 convenience and inner cans to determine if the residual stresses were sufficient for the initiation and propagation of SCC. Additional testing in a 40% calcium chloride solution was also performed on 304L stainless steel SCC coupons, i.e. stressed teardrop-shaped samples (teardrops), and an inner can welded top to provide comparative results and to assess the effect of residual stresses in a less aggressive environment. The testing performed under this task consisted of 3013 inner and convenience cans and 304L teardrops exposed to a boiling magnesium chloride solutions per ASTM G36 and a 40% calcium chloride solution at 100 C following the guidance of ASTM G123. Cracking occurred in all can types including the inner can bottom and welded top and the bottoms of the SRS and Hanford convenience cans when exposed to the boiling magnesium chloride solution at 155 C. Cracking occurred at different times indicative of the residual stress levels in the cans. 304L teardrops cracked in the shortest time interval and therefore provide a conservative estimate for can performance. Testing in a 40% calcium chloride solution at 100 C demonstrated that cracking occurs in a less aggressive environment but at significantly longer times than in the boiling magnesium chloride. Vapor space cracking was also found to occur in the inner can welded top exposed over the boiling magnesium chloride solution and on 304L teardrops exposed over a hot calcium chloride solution.

36 MATERIALS SCIENCE↗

RESULTS OF EXPERIMENT TO DETERMINE CORROSION RATES FOR 304L IN HB-LINE DISSOLVER VESSEL VENTILATION SYSTEM

Radioactive material being processed as part of the DE3013 program for HB-Line will result in the presence of chlorides, and in some cases fluorides, in the dissolver. Material Science and Technology developed an experimental plan to evaluate the impact of chloride on corrosion of the dissolver vessel ventilation system. The plan set test variables from the proposed operating parameters, previous test results, and a desired maximum chloride concentration for processing. The test variables included concentrations of nitric acid, fluorides and chlorides, and the presence of a welded and stressed metal coupon. Table 1 contains expected general corrosion rates in the HB-Line vessel vent system from dissolution of 3013 contents of varying nitric acid and chloride content. These general corrosion rates were measured upstream of the condenser in the experiment's offgas system near the entrance to the dissolver. However, they could apply elsewhere in the offgas system, depending on factors not simulated in the testing, including offgas system temperatures and airflow. Localized corrosion was significant in Tests One, Two, and Three. This corrosion is significant because it will probably be the first mode of penetration of the 304L steel in several places in the system. See Table 2. For Tests One and Three, the penetration rate of localized corrosion was much higher than that for general corrosion. It was approximately four times higher in Test One and at least 45 times higher in Test Three, penetrating an entire coupon thickness of 54 mils in 186 hours or less. There was no significant difference in corrosion between welded areas and un-welded areas on coupons. There was also no significant attack on stressed portions of coupons. It is probable that the lack of corrosion was because the stressed areas were facing downwards and offered no place for condensation or deposits to form. Had deposits formed, pitting may have occurred and led to stress corrosion cracking. The significant localized corrosion observed was usually associated with deposits. General corrosion on the offgas coupons was extremely high for the test containing 10,000 ppm chloride in the dissolver solution. Localized corrosion caused deep penetration of coupon surfaces with a solution of 2000 ppm chloride, both at 12 M and 8 M nitric acid. We recommend that when processing chloride-containing solutions, the pre-condenser side of the vessel vent system be inspected at a frequency calculated from acceptable material losses and expected general corrosion rate. The presence of deposits and heavy condensation during inspection should be taken as indicators of possibly severe localized corrosion.

36 MATERIALS SCIENCE↗

EVALUATION OF FLOWSHEET CHANGES FOR THE HIGHLY ENRICHED URANIUM BLENDDOWN PROGRAM

H Canyon is considering a flowsheet change for Plutonium (Pu) Contaminated Scrap (PuCS) material. The proposed change is to route dissolved PuCS material directly to a uranium (U) storage tank. As a result, the PuCS solution will bypass Head End and First U Cycle, and will be purified by solvent extraction in Second U Cycle. The PuCS solution contains appreciable amounts of boron (B) and fluoride (F{sup -}), which are currently at trace levels in the U storage tank. Though unlikely, if the B concentration in the U storage tank were to reach 1.8 g B/g U, the entire contents of the U storage tank would likely require a second pass through Second U Cycle to provide sufficient decontamination to meet the Tennessee Valley Authority (TVA) Blend Grade Highly Enriched Uranium (HEU) specification for B, which is 30 {micro}g/g U. In addition, Second U Cycle is expected to provide sufficient decontamination of F{sup -} and Pu regardless of the amount of PuCS solution sent to the storage tank. Though aluminum (Al) is not present in the PuCS solution, B can be credited as a complexant of F{sup -}. Both stability constants from the literature and Savannah River National Laboratory (SRNL) corrosion studies were documented to demonstrate that B complexation of F{sup -} in nitric acid solutions is sufficient to prevent excessive corrosion. Though B and Al complex F{sup -} to a similar degree, neither completely eliminates the presence of free F{sup -} in solution. Therefore, a limited amount of corrosion is expected even with complexed F{sup -} solutions. Tanks maintained at ambient temperature are not expected to experience significant corrosion. However, the Low Activity Waste (LAW) evaporators may be subjected to a corrosion rate of about 25 mils per year (mpy) as they reach their highest F{sup -} concentrations. The feed adjustment evaporator would only be subjected to the corrosion rate of about 25 mpy in the latter stages of the PuCS campaign. An issue that must be addressed as part of the proposed PuCS flowsheet change is that B has limited solubility in concentrated nitric acid solutions. As the proposed PuCS campaign progresses, the B concentration will increase in the U storage tank, in Second U Cycle feed, and in the 1DW stream sent to the LAW evaporators. Limitations on the B concentration in the LAW evaporators will be needed to prevent formation of boron-containing solids.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗