Thermal annealing of laser damage precursors on fused silica surfaces

Previous studies have identified two significant precursors of laser damage on fused silica surfaces at fluences <35 J/cm2: photoactive impurities from polishing and surface fractures. We evaluate isothermal heating as a means of remediating the defect structure associated with surface fractures. Vickers indentations are applied to silica surfaces at loads between 0.5 and 10 N, creating fracture networks. The indentations are characterized before and following thermal annealing under various time and temperature conditions using confocal time-resolved photo-luminescence (CTP) imaging, and R/1 damage testing with 3-ns, 355-nm laser pulses. Improvements in the damage thresholds with reductions in CTP intensity are observed at temperatures well below the glass transition temperature (Tg). The damage threshold on 0.5-N indentations improves from <8 to >35 J/cm2 after annealing at approximately 750°C. Larger fracture networks require longer or higher temperature treatment to achieve similar results. At an annealing temperature >1100°C, optical microscopy indicates morphological changes in some of the fractures surrounding the indentations, although remnants of the original fractures are still observed. In conclusion, we demonstrate the potential of using isothermal annealing to improve the laser damage resistance of silica optics, and provide a means of further understanding the physics of optical damage and mitigation.

36 MATERIALS SCIENCE↗

Fracture Induced Sub-Band Absorption as a Precursor to Optical Damage on Fused Silica Surfaces

The optical damage threshold of indentation induced flaws on fused silica surfaces was explored. Mechanical flaws were characterized by laser damaged testing, SEM, optical, and photoluminescence microscopy. Localized polishing, chemical etching, and the control of indentation morphology were used to isolate the structural features which limit optical damage. A thin defect layer on fracture surfaces, including those smaller than the wavelength of visible light, was found to be the dominant source of laser damage initiation during illumination with 355nm, 3ns laser pulses. Little evidence was found that either displaced or densified material or fluence intensification plays a significant role in optical damage at fluences >35J/cm{sup 2}. Elimination of the defect layer was shown to increase the overall damage performance of fused silica optics.

36 MATERIALS SCIENCE↗

HF-based etching processes for improving laser damage resistance of fused silica optical surfaces

The effect of various HF-based etching processes on the laser damage resistance of scratched fused silica surfaces has been investigated. Conventionally polished and subsequently scratched fused silica plates were treated by submerging in various HF-based etchants (HF or NH{sub 4}F:HF at various ratios and concentrations) under different process conditions (e.g., agitation frequencies, etch times, rinse conditions, and environmental cleanliness). Subsequently, the laser damage resistance (at 351 or 355 nm) of the treated surface was measured. The laser damage resistance was found to be strongly process dependent and scaled inversely with scratch width. The etching process was optimized to remove or prevent the presence of identified precursors (chemical impurities, fracture surfaces, and silica-based redeposit) known to lead to laser damage initiation. The redeposit precursor was reduced (and hence the damage threshold was increased) by: (1) increasing the SiF{sub 6}{sup 2-} solubility through reduction in the NH4F concentration and impurity cation impurities, and (2) improving the mass transport of reaction product (SiF{sub 6}{sup 2-}) (using high frequency ultrasonic agitation and excessive spray rinsing) away from the etched surface. A 2D finite element crack-etching and rinsing mass transport model (incorporating diffusion and advection) was used to predict reaction product concentration. The predictions are consistent with the experimentally observed process trends. The laser damage thresholds also increased with etched amount (up to {approx}30 {micro}m), which has been attributed to: (1) etching through lateral cracks where there is poor acid penetration, and (2) increasing the crack opening resulting in increased mass transport rates. With the optimized etch process, laser damage resistance increased dramatically; the average threshold fluence for damage initiation for 30 {micro}m wide scratches increased from 7 to 41 J/cm{sup 2}, and the statistical probability of damage initiation at 12 J/cm{sup 2} of an ensemble of scratches decreased from {approx}100 mm{sup -1} of scratch length to {approx}0.001 mm{sup -1}.

42 ENGINEERING↗

Ultra-fast photoluminescence as a diagnostic for laser damage initiation

Using high-sensitivity confocal time-resolved photoluminescence (CTP) techniques, we report an ultra-fast photoluminescence (40ps-5ns) from impurity-free surface flaws on fused silica, including polished, indented or fractured surfaces of fused silica, and from laser-heated evaporation pits. This fast photoluminescence (PL) is not associated with slower point defect PL in silica which has characteristic decay times longer than 5ns. Fast PL is excited by the single photon absorption of sub-band gap light, and is especially bright in fractures. Regions which exhibit fast PL are strongly absorptive well below the band gap, as evidenced by a propensity to damage with 3.5eV ns-scale laser pulses, making CTP a powerful non-destructive diagnostic for laser damage in silica. The use of CTP to provide insights into the nature of damage precursors and to help develop and evaluate new damage mitigation strategies will be presented.

42 ENGINEERING↗

Modeling Wet Chemical Etching of Surface Flaws on Fused Silica

Fluoride-based wet chemical etching of fused silica optical components is useful to open up surface fractures for diagnostic purposes, to create surface topology, and as a possible mitigation technique to remove damaged material. To optimize the usefulness of etching , it is important to understand how the morphology of etched features changes as a function of the amount of material removed. In this study, we present two geometric etch models that describe the surface topology evolution as a function of the amount etched. The first model, referred to as the finite-difference etch model, represents the surface as an array of points in space where at each time-step the points move normal to the local surface. The second model, referred to as the surface area-volume model, more globally describes the surface evolution relating the volume of material removed to the exposed surface area. These etch models predict growth and coalescence of surface fractures such as those observed on scratches and ground surfaces. For typical surface fractures, simulations show that the transverse growth of the cracks at long etch times scales with the square root of etch time or the net material removed in agreement with experiment. The finite-difference etch model has also been applied to more complex structures such as the etching of a CO{sub 2} laser-mitigated laser damage site. The results indicate that etching has little effect on the initial morphology of this site implying little change in downstream scatter and modulation characteristics upon exposure to subsequent high fluence laser light. In the second part of the study, the geometric etch model is expanded to include fluid dynamics and mass transport. This later model serves as a foundation for understanding related processes such as the possibility of redeposition of etch reaction products during the etching, rinsing or drying processes.

42 ENGINEERING↗

Scratch Forensics

Scratches on optical components which are formed during fabrication, cleaning, handling and end-use, are widespread and almost always detrimental. The impact of scratches on the end-use of the optic includes increased optical scatter, reduced system performance, and reduced strength. In the case of optics used in high intensity laser applications, prevention of scratches is paramount because they are closely associated with laser damage. Evaluation of the characteristics (dimensions, location on optic, shape, and orientation) of a scratch can serve a powerful tool to identify the cause of the scratch and lead to mitigations to prevent their reoccurrence. It is likely that opticians have used such techniques for hundreds of years. In recent years, by applying techniques of fracture mechanics and tribology, several new semi-quantitative rules-of-thumb have been developed allowing one to estimate the size and shape of the scratch inducing asperity or rogue particle, the load on the particle, the depth of the fractures in the scratch, and properties of material housing the rogue particle. The following discussion reviews some these techniques, which as a whole, we refer to as 'Scratch Forsenics'.

42 ENGINEERING↗

The Effect of HF/NH4F Etching on the Morphology of Surface Fractures on Fused Silica

The effects of HF/NH{sub 4}F, wet chemical etching on the morphology of individual surface fractures (indentations, scratches) and of an ensemble of surface fractures (ground surfaces) on fused silica glass has been characterized. For the individual surface fractures, a series of static or dynamic (sliding) Vickers and Brinnell indenters were used to create radial, lateral, Hertzian cone and trailing indentation fractures on a set of polished fused silica substrates which were subsequently etched. After short etch times, the visibility of both surface and subsurface cracks is significantly enhanced when observed by optical microscopy. This is attributed to the removal of the polishing-induced Bielby layer and the increased width of the cracks following etching allowing for greater optical scatter at the fracture interface. The removal of material during etching was found to be isotropic except in areas where the etchant has difficulty penetrating or in areas that exhibit significant plastic deformation/densification. Isolated fractures continue to etch, but will never be completely removed since the bottom and top of the crack both etch at the same rate. The etching behavior of ensembles of closely spaced cracks, such as those produced during grinding, has also been characterized. This was done using a second set of fused silica samples that were ground using either fixed or loose abrasives. The resulting samples were etched and both the etch rate and the morphology of the surfaces were monitored as a function of time. Etching results in the formation of a series of open cracks or cusps, each corresponding to the individual fractures originally on the surface of the substrate. During extended etching, the individual cusps coalesce with one another, providing a means of reducing the depth of subsurface damage and the peak-to-valley roughness. In addition, the material removal rate of the ground surfaces was found to scale with the surface area of the cracks as a function of etch time. The initial removal rate for the ground surface was typically 3.5 x the bulk etch rate. The evolving morphology of ground surfaces during etching was simulated using an isotropic finite difference model. This model illustrates the importance that the initial distributions of fracture sizes and spatial locations have on the evolution of roughness and the rate at which material is removed during the etching process. The etching of ground surfaces can be used during optical fabrication to convert subsurface damage into surface roughness thereby reducing the time required to produce polished surfaces that are free of subsurface damage.

42 ENGINEERING↗