Search NASA⌕ Search

Engineering topics

Misra, Amit

Publications and source records attributed to Misra, Amit.

At least 109 records · Page 6

W11-ExtremeMat (Report) [Slides]

These slides are part of the final report of the Project W11_ExtremeMat (PI: A. Caro), an Institutional Computing project giving us access to LANL’s computers for the CMIME EFRC computational work. They will be posted in the IC web page visible both internal and external to LANL.

36 MATERIALS SCIENCE↗

X-ray Diffraction Studies of Forward and Reverse Plastic Flow in Nanoscale Layers during Thermal Cycling

The biaxial stress-strain response of layers within Cu/Ni nanolaminates is determined from in-plane x-ray diffraction spectra during heating/cooling. Thinner (11 nm) Cu and Ni layers with coherent, cube-on-cube interfaces reach ~1.8 GPa (Cu) and ~2.9 GPa (Ni) without yielding. Thicker (21 nm) layers with semi-coherent interfaces exhibit unusual plastic phenomena, including extraordinary plastic work hardening rates, and forward vs. reverse plastic flow with small (~10%) changes in stress, and evidence that threshold plastic stress in Ni layers is altered by preceding plastic flow in Cu layers. Line energy, pinning strength, net interfacial dislocation density and hardness are provided.

Gram, Michael D↗

Study of MPLNET-Derived Aerosol Climatology over Kanpur, India, and Validation of CALIPSO Level 2 Version 3 Backscatter and Extinction Products

The level 2 aerosol backscatter and extinction profiles from the NASA Micropulse Lidar Network (MPLNET) at Kanpur, India, have been studied from May 2009 to September 2010. Monthly averaged extinction profiles from MPLNET shows high extinction values near the surface during October March. Higher extinction values at altitudes of 24 km are observed from April to June, a period marked by frequent dust episodes. Version 3 level 2 Cloud Aerosol Lidar with Orthogonal Polarization (CALIOP) aerosol profile products have been compared with corresponding data from MPLNET over Kanpur for the above-mentioned period. Out of the available backscatter profiles, the16 profiles used in this study have time differences less than 3 h and distances less than 130 km. Among these profiles, four cases show good comparison above 400 m with R2 greater than 0.7. Comparison with AERONET data shows that the aerosol type is properly identified by the CALIOP algorithm. Cloud contamination is a possible source of error in the remaining cases of poor comparison. Another source of error is the improper backscatter-to-extinction ratio, which further affects the accuracy of extinction coefficient retrieval.

extinction profiles↗

First Principles Modeling of Metal/Ceramic Multilayer Nano-heterostructures.

Nanoscaled multilayer films composed of metals and ceramics have been explored for their potential applications as ductile, yet strong, materials. It is believed that at the nanoscale, the interfaces between the two materials constituting the multilayer assume an increasingly important role in determining the properties, as they comprise a more significant volume fraction of the multilayer with decreasing layer thickness. In this ab initio work, density functional theory was used to calculate the ideal shear strengths of pure Al, pure TiN, the Al/TiN interfacial region, and Al/TiN multilayers. The ideal shear strength of the Al/TiN interface was found to vary from very low (on the order of the ideal shear strength of Al) to very high (on the order of the ideal shear strength of TiN), depending on whether the TiN at the interface was Ti- or N-terminated, respectively. The results suggest that the shear properties of Al/TiN depend strongly on the chemistry of the interface, Al:N versus Al:Ti terminations. Nevertheless, for the Al/TiN multilayers, the ideal shear strength was limited by shear in the Al layer away from the interface, even when the individual layer thickness is less than a nanometer. Further we found an unusual structural rotation of bulk single-crystal Al under uniaxial compressive strains. It was found that under strains either along the <11-2> or the <111> directions, beyond a critical stress of about 13 GPa, the Al crystal can rotate through shear in the Shockley partial direction (i.e.,<11-2>) on the {l_brace}111{r_brace} plane, in an attempt to relieve internal stresses. This phenomenon reveals a possible mechanism leading to the onset of homogeneous dislocation nucleation in Al under high uniaxial compressions.

36 MATERIALS SCIENCE↗

Mechanism for recombination of radiation-induced point defects at interphase boundaries

MD studies of collision cascades in KS-type Cu-Nb interfaces are performed, revealing that Cu interstitials are preferentially loaded into the interface while on the bcc Nb side there is very little absorption of interstitials. The interstitial loading effect at two types of heterogeneous Cu-Nb interfaces, both KS-type and SPD {l_brace}112{r_brace}-type interfaces is studied: (a) The Cu interstitials are observed to spontaneously emit from both types of interfaces to annihilate vacancies in the nearby bulk, (b) MD and NEB studies are used to characterize low barrier emission processes. Our study also indicates that interstitials do not lose their identity when absorbed even at interfaces where they become significantly delocalized.

36 MATERIALS SCIENCE↗

Defect Interactions at Metal/Ceramic Interfaces in Thin Film Multilayers

Summary of metal-ceramic multilayer deformation: (1) In nanolayered Al/TiN, Al layers grow in a twin orientation with the underlying TiN/Al layers favored by N-terminated TiN layers; (2) The shear strength of Al/TiN interface varies significantly depending on whether the interface is Ti or N terminated; (3) 2 nm Al - 2 TiN multilayers exhibit unusual mechanical properties as revealed by compression testing - (a) High maximum flow strength of 4.5 GPa, which is significantly higher than hardness (6 GPa) divided by a factor of 3, (b) Extraordinarily high strain hardening rates in Al nanolayers (16-35 GPa, {approx} E/2 to E/4), (c) Co-deformability of the TiN nanolayers with Al (confirmed by TEM on nanoindents) to plastic strains in excess of 5%.

COMPRESSION↗