Search NASA⌕ Search

Engineering topics

Moffitt, Stephanie

Publications and source records attributed to Moffitt, Stephanie.

Module-Level Solutions For Degradation by Ionization Damage

After years of improving module efficiency while targeting mean degradation rates of 0.5 to 0.6 %/y for crystalline silicon technology, there is much evidence that the degradation rates are now increasing significantly. Contributing factors include:Radiation damage (UV-Light Induced Degradation): Trina solar: -4.5%/y degradation rate in Singapore, DOE National Laboratory Regional Test Centers showed degradation of -1% < r < -2%/y in crystalline silicon modules, Jinko Solar: -4% < r < -7% efficiency loss from 540 MJ/m-2 of UV-A light, ISFH: 15% relative power loss during of 1.8 GJ/m-2 UV exposure, attributed to H+. Electrical bias from positive system voltage (e.g., +1000 V, +1500 V) can drive ions and metallization through the encapsulation, NREL: Ion transport can affect the cell passivation, resulting in power loss of 5% to 40% in p-PERC+ (bifacial), NREL: Damage at cell rear with up to 17% power at cell fronts in n-PERT modules. Delamination can also occur due to cell surface reactions driven by light and bias.

module efficiency↗

Mechanisms of adhesion degradation at the photovoltiac module's cell metallization-encapsulant interface

Adhesion measurements and chemical characterization of the encapsulant/silver metallization interface of a photovoltaic (PV) module through temperature, humidity, and voltage bias exposures were conducted. Results demonstrate two independent degradation mechanisms: (a) with voltage bias, the ionic conduction of Na + ions through the encapsulant results in the formation of sodium silicate at the silver metallization surface, thereby weakening that interface and (b) with moisture ingress, dissociation of the silane bonding to silver in the silver oxide similarly weakens this interface resulting in significantly lower debond energies.

14 SOLAR ENERGY↗