Search NASA⌕ Search

Engineering topics

Myers, Deborah J. (ORCID:0000000192993916)

Publications and source records attributed to Myers, Deborah J. (ORCID:0000000192993916).

A scalable membrane electrode assembly architecture for efficient electrochemical conversion of CO2 to formic acid

Abstract The electrochemical reduction of carbon dioxide to formic acid is a promising pathway to improve CO 2 utilization and has potential applications as a hydrogen storage medium. In this work, a zero-gap membrane electrode assembly architecture is developed for the direct electrochemical synthesis of formic acid from carbon dioxide. The key technological advancement is a perforated cation exchange membrane, which, when utilized in a forward bias bipolar membrane configuration, allows formic acid generated at the membrane interface to exit through the anode flow field at concentrations up to 0.25 M. Having no additional interlayer components between the anode and cathode this concept is positioned to leverage currently available materials and stack designs ubiquitous in fuel cell and H 2 electrolysis, enabling a more rapid transition to scale and commercialization. The perforated cation exchange membrane configuration can achieve >75% Faradaic efficiency to formic acid at <2 V and 300 mA/cm 2 in a 25 cm 2 cell. More critically, a 55-hour stability test at 200 mA/cm 2 shows stable Faradaic efficiency and cell voltage. Technoeconomic analysis is utilized to illustrate a path towards achieving cost parity with current formic acid production methods.

08 HYDROGEN↗

Effect of Particle Size on the Dissolution of Pt 3 Co/C and Pt/C PEMFC Electrocatalysts

Potentiostatic and potentiodynamic Pt and Co dissolution were investigated for three Pt 3 Co/C catalysts with particle sizes of 4.9, 8.1, and 14.8 nm in aqueous electrolyte at potentials encountered by the PEMFC cathode. For all three Pt 3 Co/C catalysts under prolonged potentiostatic dissolution, the dissolved Pt steady state concentration increases from 0.85 V to reach a maximum at 1.1−1.15 V and decreases at higher potentials. The dependence of the dissolved Pt steady state concentration on particle size reveals that catalyst stability decreases with decreasing mean particle size, whereas the stability under potential cycling conditions is non-monotonic with particle size. Preferential dissolution of Co from all three Pt 3 Co catalysts was observed at all potentials, which increases at >1.1 V, the region over which Pt dissolution decreases, reflecting the opposing effects of Pt oxide formation on Pt and Co dissolution. Comparison of Pt 3 Co/C and Pt/C with similar mean particle sizes (4.9 vs 5.0 nm) and particle size distributions reveals that the Pt 3 Co/C has a higher potentiostatic dissolution rate (4–5 times), a higher steady state concentration of dissolved Pt (∼2 times), and a larger change in electrochemically-active surface area (ECA) (18 times) after prolonged cycling, indicating that Pt 3 Co has inferior stability. The higher rates of Pt dissolution for Pt 3 Co vs Pt have been attributed to higher extents of surface Pt oxidation, as determined using voltammetric oxide reduction charges and the white line intensities in Pt L 3 X-ray absorption spectra.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗