Electrolyte Design for Multivalent Metal Battery Interphases
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Nazar, Linda.
Explore the source record for details and available documents.
A deep understanding of the interaction of the surface of cathode materials with solid electrolytes is crucial to design advanced solid-state batteries (SSBs). This is especially true for the new class of lithium metal chloride (Li-M-Cl) solid electrolytes which are receiving rapidly growing attention due to their very high oxidative stability (>4 V) in combination with good ionic conductivity that can enable long cell cycle life. While Li-M-Cl electrolytes typically contain resource-limited metals (M) such as indium or rare earths, work has focused on substituting M with more abundant elements such as zirconium. Via operando resistance measurements using intermittent current interruption we explore the dynamic evolution of the interphase at the surface of Ni-rich NCM85 or NCM111 cathode particles inside a working SSB with three different Li-(M 1 ,M 2 )-Cl catholytes (Li 3 InCl 6 , Li 2 Sc 1/3 In 1/3 Cl 4 and Li 5/2 Y 1/2 Zr 1/2 Cl 6 ) to reveal the impact of the cationic metal substitution on the interfacial chemistry. We show that the metal plays a critical role in determining high voltage stability, contrary to prior assumptions. Using a combination of cyclic voltammetry and ultraviolet photoelectron spectroscopy measurements of the electronic band structure to assess oxidative stability; coupled with DFT calculations and ToF-SIMS to evaluate products formed at the interface at different upper cutoff potentials and degrees of delithiation, we are able to differentiate between electrochemical and chemical degradation. We find that Li 2 Sc 1/3 In 1/3 Cl 4 yields the highest (and Li 3 InCl 6 the lowest) stability against electrochemical oxidation, while Li 5/2 Y 1/2 Zr 1/2 Cl 6 undergoes a detrimental chemical reaction with oxygen released from Ni-rich NCM85 at high potentials, resulting in fast capacity fading. Altogether, our work establishes a platform for the metrics and an approach that can be utilized to efficiently evaluate the stability of new halide SEs in SSB cells.
Electrolytes used in rechargeable batteries must enable rapid translation of the working ion between macroscopically separated electrodes. These electrolytes are, however, usually designed and synthesized using atomic-level insights. Whether the ideal electrolyte for a particular battery is a solid or a liquid remains an important unresolved question, especially as solids with conductivities comparable with liquids are discovered. Here, to help resolve such questions, we present the first steps toward a unified framework for relating atomic and continuum scale phenomena. Solvation shells in liquids are entities that translate with the working ion for a short while before they break up due to Brownian motion. By contrast, solvation cages in classical solids and polymers cannot not translate with the working ion. Mobility of the entities that make up the cages and shells, which is quantified by an order parameter, is shown to influence translation of the working ion on continuum length scales.
Diffusion coefficients (D) for both Li+ and Mg2+ in Ti2S4 were measured using the galvanic intermittent titration technique (GITT) as a function of both ion concentration (x) and temperature. During discharge at 60 degrees C, D-Li descends gradually from 2 X 10(-8) cm(2)/s at x(Li) approximate to 0 to 2 X 10(-9) cm(2)/s at x(Li) approximate to 1.9. In contrast, D-Mg decreases sharply from 2 X 10(-8) to 1 x 10(-12) cm(2)/s by x(Mg) approximate to 0.8. This kinetic factor limits the maximum practical discharge capacity of MgxTi2S4. The difference in behavior vis a vis Li+ implies that either increasing Mg2+ occupation of the tetrahedral site at x(Mg) > 0.6 and/or interactions between diffusing cations play a larger role in mediating the diffusion of divalent compared to monovalent cations. Diffusion activation energies (E-a) extracted from the temperature-dependent data revealed that E-a,E-Mg (540 +/- 80 meV) is about twice that of E-a,E-Li (260 +/- 50 meV), explaining the poorer electrochemical performance of MgxTi2S4 at room temperature.
Abstract not provided.