Light Gas Separations and Storage with MOFs via DFT Modeling Synthesis and Pressurized Induced Structural Changes.
Abstract not provided.
Engineering topics
Publications and source records attributed to Nenoff, Tina Maria.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided.
Abstract not provided
Abstract not provided.
Abstract not provided.
Herein, we study the durability of the Sandia Bi-Si oxide Glass Composite Material (GCM) waste form when formulated with different weight percent levels of AgI-MOR. The post-iodine exposure AgI-MOR material was provided to SNL by ORNL. Durability results for the GCM fabricated with 22 and 25% AgI-MOR indicate releases of Ag and I at the same low rates as 15% AgI-MOR GCM, and by the same mechanism. Iodine and Ag release is controlled by the low solubility of an amorphous, hydrated silver iodide, not by the surface-controlled dissolution of I 2 - loaded Ag-Mordenite. Based on this data, we postulate that much higher loading levels of AgIMOR are probable in this GCM waste form, and limits will govern by retention of mechanical integrity of the GCM versus the solubility of silver iodide.
Silver-containing mordenite (MOR) is a longstanding benchmark for radioiodine capture, reacting with molecular iodine (I 2 ) to form AgI. However the mechanisms for organoiodine capture are not well understood. Here we investigate the capture of methyl iodide from complex mixed gas streams by combining chemical analysis of the effluent gas stream with in depth characterization of the recovered sorbent.
We are purusing an understand of the durability and materials processability of the low temperature sintering Bi-Si oxide Glass Composite Material (GCM)1 Waste Form for iodine capture materials. The chemical and physical controls over iodine release from candidate 129 I waste forms must be quantified to predict long-term waste form effectiveness.