Search NASA⌕ Search

Engineering topics

Ohriner, Evan Keith

Publications and source records attributed to Ohriner, Evan Keith.

Design and Demonstration of a Material-Plasma Exposure Target Station for Neutron Irradiated Samples

Fusion energy is the most promising energy source for the future, and one of the most important problems to be solved progressing to a commercial fusion reactor is the identification of plasma-facing materials compatible with the extreme conditions in the fusion reactor environment. The development of plasma–material interaction (PMI) science and the technology of plasma-facing components are key elements in the development of the next step fusion device in the United States, the so-called Fusion Nuclear Science Facility (FNSF). All of these PMI issues and the uncertain impact of the 14-MeV neutron irradiation have been identified in numerous expert panel reports to the fusion community. The 2007 Greenwald report classifies reactor plasma-facing materials (PFCs) and materials as the only Tier 1 issues, requiring a “. . . major extrapolation from the current state of knowledge, need for qualitative improvements and substantial development for both the short and long term.” The Greenwald report goes on to list 19 gaps in understanding and performance related to the plasma–material interface for the technology facilities needed for DEMO-oriented R&D and DEMO itself. Of the 15 major gaps, six (G7, G9, G10, G12, G13) can possibly be addressed with ORNL’s proposal of an advanced Material Plasma Exposure eXperiment. Establishing this mid-scale plasma materials test facility at ORNL is a key element in ORNL’s strategy to secure a leadership role for decades of fusion R&D. That is to say, our end goal is to bring the “signature facility” FNSF home to ORNL. This project is related to the pre-conceptual design of an innovative target station for a future Material–Plasma Exposure eXperiment (MPEX). The target station will be designed to expose candidate fusion reactor plasma-facing materials and components (PFMs and PFCs) to conditions anticipated in fusion reactors, where PFCs will be exposed to dense high-temperature hydrogen plasmas providing steady-state heat fluxes of 5–20 MW/m 2 and ion fluxes up to 10 24 m -2 s -1 . Since PFCs will have to withstand neutron irradiation displacement damage up to 50 dpa, the target station design must accommodate radioactive specimens (materials to be irradiated in HFIR or at SNS) to enable investigations of the impact of neutron damage on materials. Therefore, the system will have to be able to install and extract irradiated specimens using equipment and methods to avoid sample modification, control contamination, and minimize worker dose. Included in the design considerations will be an assessment of all the steps between neutron irradiation and post-exposure materials examination/characterization, as well as an evaluation of the facility hazard categorization. In particular, the factors associated with the acquisition of radioactive specimens and their preparation, transportation, experimental configuration at the plasma-specimen interface, post-plasma-exposure sample handling, and specimen preparation will be evaluated. Neutronics calculations to determine the dose rates of the samples were carried out for a large number of potential plasma-facing materials.

42 ENGINEERING↗

Facility for high heat flux testing of irradiated fusion materials and components using infrared plasma arc lamps

A new high-heat flux testing facility using water-wall stabilized high-power high-pressure argon Plasma Arc Lamps (PALs) has been developed for fusion applications. It can handle irradiated plasma facing component materials and mock-up divertor components. Two PALs currently available at ORNL can provide maximum incident heat fluxes of 4.2 and 27 MW/m2 over a heated area of 9x12 and 1x10 cm2, respectively, which are fusion-prototypical steady state heat flux conditions. The facility will be described and the main differences between the photon-based high-heat flux testing facilities, such as PALs, and the e-beam and particle beam facilities more commonly used for fusion HHF testing are discussed. The components of the test chamber were designed to accommodate radiation safety and materials compatibility requirements posed by high-temperature exposure of low levels irradiated tungsten articles. Issues related to the operation and temperature measurements during testing are presented and discussed.

Sabau, Adrian S↗

Analysis of Abrasive Blasting of DOP-26 Iridium Alloy

The effects of abrasive blasting on the surface geometry and microstructure of DOP-26 iridium alloy (Ir-0.3% W-0.006% Th 0.005% Al) have been investigated. Abrasive blasting has been used to control emissivity of components operating at elevated temperature. The effects of abrasive blasting conditions on surface morphology were investigated both experimentally and by numerical modeling. The simplified model, based on finite element analysis of a single angular particle impacting on Ir alloy disk, calculates the surface deformation and residual strain distribution. The experimental results and modeling results both indicate that the surface geometry is not sensitive to the abrasive blast process conditions of nozzle pressure and standoff distance considered in this study. On the other hand, the modeling results suggest that the angularity of the abrasive particle has an important role in determining surface geometry, which in turn, affects the emissivity. Abrasive blasting causes localized surface strains and localized recrystallization, but it does not affect grain size following extended exposure at elevated temperature. The dependence of emissivity of the DOP-26 alloy on mean surface slope follows a similar trend to that reported for pure iridium.

36 MATERIALS SCIENCE↗

High-Temperature Galling Characteristics of Ti-6Al-4V with and without Surface Treatments

Galling is a severe form of surface damage in metals and alloys that typically arises under relatively high normal force, low-sliding speed, and in the absence of effective lubrication. It can lead to macroscopic surface roughening and seizure. The occurrence of galling can be especially problematic in high-temperature applications like diesel engine exhaust gas recirculation system components and adjustable turbocharger vanes, because suitable lubricants may not be available, moisture desorption promotes increased adhesion, and the yield strength of metals decreases with temperature. Oxidation can counteract these effects to some extent by forming lubricative oxide films. Two methods to improve the galling resistance of titanium alloy Ti-6Al-4V were investigated: (a) applying an oxygen diffusion treatment, and (b) creating a metal-matrix composite with TiB2 using a high-intensity infrared heating source. A new, oscillating three-pin-on-flat, high-temperature test method was developed and used to characterize galling behavior relative to a cobalt-based alloy (Stellite 6B ). The magnitude of the oscillating torque, the surface roughness, and observations of surface damage were used as measures of galling resistance. Owing to the formation of lubricative oxide films, the galling resistance of the Ti-alloy at 485o C, even non-treated, was considerably better than it was at room temperature. The IR-formed composite displayed reduced surface damage and lower torque than the substrate titanium alloy.

33 ADVANCED PROPULSION SYSTEMS↗

PURIFICATION OF IRIDIUM BY ELECTRON BEAM MELTING

The purification of iridium metal by electron beam melting has been characterized for 48 impurity elements. Chemical analysis was performed by glow discharge mass spectrographic (GDMS) analysis for all elements except carbon, which was analyzed by combustion. The average levels of individual elemental impurities in the starting powder varied from 37 g/g to 0.02 g/g. The impurity elements Li, Na, Mg, P, S, Cl, K, Ca, Mn, Co, Ni, Cu, Zn, As, Pd, Ag, Cd, Sn, Sb, Te, Ba, Ce, Tl, Pb, and Bi were not detectable following the purification. No significant change in concentration of the elements Ti, V, Zr, Nb, Mo, and Re was found. The elements B, C, Al, Si, Cr, Fe, Ru, Rh, and Pt were partially removed by vaporization during electron beam melting. Langmuir's equation for ideal vaporization into a vacuum was used to calculate for each impurity element the expected ratio of impurity content after melting to that before melting. Equilibrium vapor pressures were calculated using Henry's law, with activity coefficients obtained from published data for the elements Fe, Ti, and Pt. Activity coefficients were estimated from enthalpy data for Al, Si, V, Cr, Mn, Co, Ni, Zr, Nb, Mo, and Hf and an ideal solution model was used for the remaining elements. The melt temperature was determined from measured iridium weight loss. Excellent agreement was found between measured and calculated impurity ratios for all impurity elements. The results are consistent with some localized heating of the melt pool due to rastering of the electron beam, with an average vaporization temperature of 3100 K as compared to a temperature of 2965 K calculated for uniform heating of the melt pool. The results are also consistent with ideal mixing in the melt pool.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comments on Americium Volatilization during Fuel Fabrication for Fast Reactors

The physical processes relevant to the fabrication of metallic and ceramic nuclear fuels are analyzed, with attention to recycling of fuels containing U, Pu, and minor volatile actinides for the use in fast reactors. This analysis is relevant to the development of a process model that can be used for the numerical simulation and prediction of the spatial distribution of composition in the fuel, an important factor in fuel performance.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Weldable ductile molybdenum alloy development

Molybdenum and its alloys are attractive structural materials for high-temperature applications. However, various practical issues have limited its use. One concern relates to the loss of ductility occurring in the heat-affected weld zone caused by segregation of oxygen to grain boundaries. In this study, a series of arc melted molybdenum alloys have been produced containing controlled additions of B, C, Zr, and Al. These alloys were characterized with respect to their tensile properties, smooth bend properties, and impact energy for both the base metal and welds. These alloys were compared with a very high purity low carbon arc cast molybdenum reference. For discussion purposes the alloys produced are separated into two categories: Mo Al B alloys, and Mo Zr B alloys. The properties of Mo Zr B alloy welds containing higher carbon levels exhibited slight improvement over unalloyed molybdenum, though the base-metal properties for all Mo Zr B alloys were somewhat inconsistent with properties better, or worse, than unalloyed molybdenum. A Mo Al B alloy exhibited the best DBTT values for welds, and the base metal properties were comparable to or slightly better than unalloyed molybdenum. The Mo Al B alloy contained a low volume fraction of second-phase particles, with segregation of boron and carbon to grain boundaries believed to displace oxygen resulting in improved weld properties. The volume fractions of second-phase particles are higher for the Mo Zr B alloys, and these alloys were prone to brittle fracture. It is also noted that these Mo Zr B alloys exhibited segregation of zirconium, boron and carbon to the grain boundaries.

Cockeram, B. V.↗

Processing of Iridium and Iridium Alloys

Iridium and its alloys have been considered to be difficult to fabricate due to their high melting temperatures, limited ductility, sensitivity to impurity content, and chemical properties. The variety of processing methods used for iridium and its alloys are reviewed, including purification, melting, forming, joining, and powder metallurgy techniques. Also included are coating and forming by the methods of electroplating, chemical and physical vapor deposition, and melt particle deposition.

36 MATERIALS SCIENCE↗

DEFORMATION MODELING OF IRIDIUM DOP-26 ALLOY TO DETERMINE POTENTIAL FOR SECONDARY RECRYSTALLIZATION

The DOP-26 iridium alloy (Ir-0.3%W-0.006%Th-0.005% Al) contains a distribution of thorium-containing intermetallic particles, typically less than 1 micrometer in size, which serve to pin grain boundaries. The alloy is thus subject to secondary recrystallization during long-term exposure at elevated temperature if prior plastic strains are within a critical range. A finite element method was used to model the deformation and resulting local plastic strains introduced by sizing operations on recrystallized iridium alloy cups. The results of the analysis show that local strains introduced by the deformation of cups are in all cases maintained below 0.025, the lower critical level for secondary recrystallization at 1600 K. The effects of die clearance and applied load on local plastic strain values were also treated.

36 MATERIALS SCIENCE↗