Search NASA⌕ Search

Engineering topics

Owen-Bellini, Michael

Publications and source records attributed to Owen-Bellini, Michael.

At least 19 records

TTW (Transition to Wire Device) [SWR-25-02]

The Transition to Wire (TTW) hardware project is a method for connecting solar research samples with fragile interconnects to robust, weatherproof and consistent commercial connectors. The Transition to Wire device is a printed circuit board designed to facilitate the transition from tab ribbon or other unsecured electrical contacts on research samples to either wires or a connector. The four pin connector provides a kelvin (4 wire) connection at the solder pad where the sample connects.

McDanold, Byron↗

Recovery of Glass and Silicon Solar Cells from Si-Modules Through Laser Processing

This study demonstrates an innovative and environmentally friendly laser-based approach for the efficient recovery of glass and silicon solar cells, allowing the recycling of photovoltaic modules. The methodology involves the use of a high-power pulsed laser beam focusing at various interfaces within the modules. Specifically, the delivery of ultra-short pulse laser energy at the interfaces of glass and polymeric encapsulants, as well as at the encapsulants and silicon solar cells, facilitates the debonding of polymers from both glass and silicon cell surfaces. The debonding occurs through photothermal, ablation, chemical modification, and localized heat generation. The research successfully demonstrates the recovery of glass from commercial mini solar modules of size 11.5 x 6.8 cm 2 and a silicon wafer of size 3.0x1.6 cm 2 . Ongoing efforts aim to extend the effectiveness of this laser-based methodology to comprehensively recycle larger-size components. This innovative approach holds promise for addressing environmental concerns associated with the disposal of solar modules, contributing to sustainable practices in the renewable energy sector.

glass↗

Photovoltaic Reliability Workshop (PVRW) 2024 Proceedings: Posters

NREL hosts an annual Photovoltaic Reliability Workshop (PVRW) so that solar technology experts can discuss current and future issues in PV reliability. Longer-lasting PV systems make lower-cost solar electricity and have less impact on the environment, human health, and natural resources. PVRW offers a combination of oral presentations, panel discussions with vigorous audience participation, and poster presentations. This document collects posters that were presented at PVRW 2024.

degradation↗

Photovoltaic Reliability Workshop (PVRW) 2024 Proceedings: Presentations

NREL hosts an annual Photovoltaic Reliability Workshop (PVRW) so that solar technology experts can discuss current and future issues in PV reliability. Longer-lasting PV systems make lower-cost solar electricity and have less impact on the environment, human health, and natural resources. PVRW offers a combination of oral presentations, panel discussions with vigorous audience participation, and poster presentations. This document collects oral presentations that were presented at PVRW 2024.

degradation↗

DuraMAT: Building a Consortium to Accelerate the Photovoltaic Module Reliability Learning Cycle

Durable and reliable photovoltaic (PV) modules are critical to enabling an efficient transition to sustainable energy generation. The rate at which new module designs and materials are developed and deployed currently outpaces the rate at which we can identify failure mechanisms and understand degradation rates. Increasing the service life of PV modules, and our ability to predict performance over time, requires more durable materials and designs, better durability testing, more extensive material characterization, robust modeling, and methods to cross-examine historical performance data to extract meaningful results. This is a multidisciplinary challenge that requires expertise from a broad range of fields and, therefore, benefits significantly from a collaborative approach. In this Perspective, we outline the approach taken by the Durable Module Materials Consortium (DuraMAT), present a few case studies where our approach was successful, and provide an outlook on where this approach might be applied as the PV technology landscape continues to rapidly evolve. Published by the American Physical Society 2024

14 SOLAR ENERGY↗

Strong-Bonding Hole-Transport Layers Reduce Ultraviolet Degradation of Perovskite Solar Cells

The light-emitting diodes (LEDs) used in indoor testing of perovskite solar cells do not expose them to the levels of ultraviolet (UV) radiation that they would receive in actual outdoor use. We report degradation mechanisms of p-i-n-structured perovskite solar cells under unfiltered sunlight and with LEDs. Weak chemical bonding between perovskites and polymer hole-transporting materials (HTMs) and transparent conducting oxides (TCOs) dominate the accelerated A-site cation migration, rather than direct degradation of HTMs. An aromatic phosphonic acid, [2-(9-ethyl-9H-carbazol-3-yl)ethyl]phosphonic acid (EtCz3EPA), enhanced bonding at the perovskite/HTM/TCO region with a phosphonic acid group bonded to TCOs and a nitrogen group interacting with lead in perovskites. A hybrid HTM of EtCz3EPA with strong hole-extraction polymers retained high efficiency and improved the UV stability of perovskite devices, and a champion perovskite minimodule-independently measured by the Perovskite PV Accelerator for Commercializing Technologies (PACT) center-retained operational efficiency of >16% after 29 weeks of outdoor testing.

14 SOLAR ENERGY↗

Interpreting accelerated tests on perovskite modules using photooxidation of MAPbI 3 as an example

Solar panels (modules) based on metal halide perovskites are following a fast track to commercialization. Unlike more established solar cell materials, there are not yet decades-long field observations to increase consumer confidence. The "physics and chemistry of failure" approach is used in other industries and estimates product degradation based on laboratory accelerated tests integrated with an understanding of degradation mechanisms. This work uses that approach to quantify the relationship between accelerated tests and projected product behavior for metal halide perovskite modules. Degradation involving photooxidation of methylammonium lead iodide is used to illustrate the method. Acceleration factors in common accelerated tests are found to be low. Conclusions emphasize that the accelerated tests on photovoltaics should not be interpreted as equivalent across module types or as a green light for commercialization unless supported by the appropriate field data or physics and chemistry of failure analysis.

14 SOLAR ENERGY↗

Residual Stress Limits Gridline Bridging in Cracked Solar Cells

Cracks in solar cells can be generated in various ways, but this does not mean immediate power loss. Previous studies showed that gridlines bridge cracked silicon cells, and the bridging behavior decreases during the contact and separation of gridlines within bare cells. In this study, we investigate bridging behavior in laminated monocrystalline cells. We characterize the behavior with Weibull analysis of critical crack opening distance (COD), at which the gridline is completely separated. The Weibull analysis of the laminated cell shows a good agreement with bare cells at the first cycle. However, we observe different behavior during cyclic bending. Bare cells show gradual decay of critical COD, while laminated cells show instant decay and plateau. We hypothesize that the difference is due to residual stress, squeezing gridlines, and causing plastic deformation. This is justified by the correlation between critical COD and gridline morphology. In the presentation, we shall present a Weibull analysis of the cyclic bending of a laminated cell with a reduced residual stress effect.

bending↗

Reliability of tandem solar cells and modules: what's next?

Hybrid tandem photovoltaic (PV) technology development has gained momentum in the last few years. This has been motivated by a need to push module efficiencies beyond what is theoretically capable with single-junction technologies to further accelerate total global PV deployment. Significant advances have been made with multiple material systems achieving tandem efficiencies over 30% in the last decade. All of the highest record efficiencies have been from laboratory-scale devices, with areas of 1 cm2 or less. Interestingly, there are multiple material combinations and terminal configurations that have demonstrated promising results. Despite these high laboratory efficiencies, reasonable service lifetimes (a useful operating lifetime of at least 25 years) are needed for tandems to compete with the levelized cost of energy (LCOE) of traditional single junction PV technologies. Existing commercial Si PV products have demonstrated performance in the field with an average of less than 1% relative annual degradation in module and system performance, and many manufacturers now provide 30 year warranties on their products.

14 SOLAR ENERGY↗

Accelerated Stress Testing of Perovskite Photovoltaic Modules: Differentiating Degradation Modes with Electroluminescence Imaging

Herein, electroluminescence (EL) and thermal imaging are used to examine p–i–n metal halide perovskite (MHP) photovoltaic (PV) mini-modules (MA0.6FA0.4PbI3, 20 cells, 78 cm2) before and after indoor-accelerated stress testing or outdoor deployment. Distinct spatial patterns in the EL images emerge, which depend on the external stress conditions experienced by the mini-module. Imaging results highlight a distribution of dark speckle features that dominate after UV stress, attributed to widespread interfacial contact degradation. Lateral intensity gradients across cells dominate after thermal cycling (TC) stress, attributed to current crowding near scribe defects. While current–voltage analysis alone does not give full insight on the degradation process, this study shows that distinct degradation modes can be further defined by multimodal electro-optical imaging (i.e., EL combined with photoluminescence and dark lock-in thermography). Neither UV exposure nor TC-accelerated stress testing alone replicates the same degradation signatures observed after outdoor deployment, suggesting that multiple degradation modes occur under concurrent stressors outdoors. Finally, spatial characterization of degradation modes in MHP PV mini-modules before and after accelerated stress testing lays the groundwork for developing targeted accelerated stress testing procedures through comparison with outdoor aging.

14 SOLAR ENERGY↗

Acceleration Factors for Combined‐Accelerated Stress Testing of Photovoltaic Modules

Combined‐accelerated stress testing (C‐AST) is developed to establish the durability of photovoltaic (PV) products, including for degradation modes that are not a priori known or examined in standardized tests. C‐AST aims to comprehensively represent the sample, stress factors, and their combinations using levels at the statistical tails of the natural environment. Acceleration factors for relevant climate sequences within the C‐AST cycle with respect to the Florida USA climate are estimated for selected degradation mechanisms. It is found that for degradation of the outer backsheet polymer layer, the acceleration factor of the tropical climate sequence (the longest of the climate sequences) is f ( T , G ) = 17.3 with ultraviolet photodegradation; for polyethylene terephthalate hydrolysis (backsheets), f ( T , RH ) = 426; for electrochemical corrosion (PV cell), f ( I ) = 14.1; and for PbSn solder fatigue f (Δ T , r ( T )) = 17.3. Here, T is the module temperature, G is the broadband spectrum irradiance on the plane of array of the module, RH is the relative humidity on the module surface, I is the leakage current through the module packaging, and r ( T ), the number of temperature reversals. The methods discussed herein are generally applicable for evaluating acceleration factors in other accelerated test methods.

14 SOLAR ENERGY↗

PV encapsulant formulations and stress test conditions influence dominant degradation mechanisms

Polyethylene-based poly(ethylene-co-vinyl acetate) (EVA), polyolefin elastomer (POE), and thermoplastic polyolefin (TPO) are common polymer candidates for photovoltaic (PV) module encapsulants. The choice of encapsulant must be carefully considered in novel module designs, such as bifacial glass/glass laminates, to limit performance degradation through loss of optical transmittance, mechanical integrity, and corrosion - as well as potential-induced degradation. Encapsulant quality and resilience against environmental stressors are readily influenced by the additives in the encapsulant formulation. Here, we show that, the changes in optical transmittance after UV aging result from the discoloration caused by interactions between additives, and optical scattering from changes in the polymer crystal structure. We observed competing cross-linking and chain scission mechanisms, with their kinetics influenced by the presence of oxygen and elevated temperatures. Increasing chamber temperatures from 55 °C to 85 °C during the UV stress test amplified encapsulant discoloration and promoted polymer cross-linking, causing severe, irreversible damage that remains to be proven field relevant. Damp heat aging was found to be insufficient to produce significant encapsulant degradation; however, combining stress tests sequentially allowed detection of further degradation beyond the limitations of the damp heat test alone. Appropriate degradation screening methods are necessary to uncover potential encapsulant weaknesses.

14 SOLAR ENERGY↗

A study of degradation mechanisms in PVDF-based photovoltaic backsheets

Abstract Commercial backsheets based on polyvinylidene fluoride (PVDF) can experience premature field failures in the form of outer layer cracking. This work seeks to provide a better understanding of the changes in material properties that lead to crack formation and find appropriate accelerated tests to replicate them. The PVDF-based backsheet outer layer can have a different structure and composition, and is often blended with a poly(methyl methacrylate) (PMMA) polymer. We observed depletion of PMMA upon aging with sequential (MAST) and combined (C-AST) accelerated stress testing. In field-aged samples from Arizona and India, where PVDF crystallizes in its predominant α-phase, the degree of crystallinity greatly increased. MAST and C-AST protocols were, to some extent, able to replicate the increase in crystallinity seen in PVDF after ~ 7 years in the field, but no single-stress test condition (UV, damp heat, thermal cycling) resulted in significant changes in the material properties. The MAST regimen used here was too extreme to produce realistic degradation, but the test was useful in discovering weaknesses of the particular PVDF-based outer layer structure studied. No excessive β-phase formation was observed after aging with any test condition; however, the presence of β-phase was identified locally by Fourier transform infrared spectroscopy (FTIR). We conclude that both MAST and C-AST are relevant tests for screening outdoor failure mechanisms in PVDF backsheets, as they were successful in producing material degradation that led to cracking.

14 SOLAR ENERGY↗

Millions of Small Pressure Cycles Drive Damage in Cracked Solar Cells

Here, we applied time-varying air pressure to a PV module containing newly cracked cells. The test used a new dynamic mechanical acceleration (DMX) apparatus. We applied pressure cycles similar to natural, wind-driven cycles. Compared to standard dynamic mechanical load (DML) tests, we applied much lower pressure (10 Pa to 300 Pa RMS) and many more cycles (one million at each of four pressure levels). We present a case study on a single cell in a commercial module. We monitored electrical continuity loss across cracks using electroluminescence (EL) imaging. 10 Pa pressure cycles caused negligible change. 30 Pa pressure cycles caused permanent damage that continued worsening even after tens of thousands of cycles. After one million 30 Pa cycles, a series of 100 Pa cycles still caused new, permanent damage to existing cracks. 300 Pa cycles caused further worsening and introduced new cracks.

14 SOLAR ENERGY↗