Continue Effort to Improve Alloy 800H Weldment

This memorandum formally documents the completion of the Level 3 milestone M3AT-22IN0604055 titled, “Continue effort to improve Alloy 800H weldment creep rupture performance,” by the transmittal of this deliverable document, entitled, “Issue memo ‘Preliminary assessment of UTP A 2133 Mn as a matching filler metal for Alloy 800H in Section III Division 5 applications.’” The deadline for this milestone is August 27, 2022. This milestone is part of the ART GCR work package AT-22IN060405, “Long-Term Very-High Temperature Reactor (VHTR) Material Qualification – INL.”

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

GCR: Development of Improved Alloy 800H Weldment

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1000°C (1292 to 1832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with an Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal, UTP A 2133 Mn.

36 MATERIALS SCIENCE↗

Multi-Pass Hybrid Laser Arc Welding of Alloy 740H

The presentation reviews the progress made toward reducing the joining time of an advanced nickel-based alloy, Alloy 740H by a factor of two using a novel two step fusion welding approach. In the first step, a high powered laser is used to rapidly join thick weld groove lands (~10-12 mm thick) during a single pass. Hybrid laser arc welding (HLAW) is then used to fill the remaining weld groove and complete the joint. This sequential process also utilizes laser wobble in both steps to reduce welding defects and refine the weld microstructure to obtain improved properties compared to conventional gas tungsten or gas metal arc welds, GTAW and GMAW, respectively. The creep behavior of laser-only thick weld groove land welds and HLAW welds were found to be the same or slightly improved compared to conventional GMAW or GTAW welds in this alloy. Creep tests have been started to verify the long-term creep behavior (~10,000 hrs) of these welds. Modeling results on deep penetration laser welding are presented and the initial simulations of laser welding with laser wobble are shown. The next phase of the project will combine the two processes to make complete welds - deep penetration laser welds of thick weld groove lands followed by rapid filling of the remaining weld groove by HLAW - in thick plates (32 mm thick) Alloy 740H plate and entails development of narrow weld groove welding to further decrease the joining time of this alloy.

36 MATERIALS SCIENCE↗

Understanding Weld Formation and Microstructure Evolution in Laser Welded Stainless Steels and Ti-6Al-4V

High energy density welding processes are used for many industrial applications, such as aerospace and defense, and certain joint configurations and welding situations render post-weld inspection techniques difficult. Due to the inability to confirm penetration, there is a continual industrial need to improve prediction capabilities to aid in parameter selection. It is also necessary to understand the microstructural evolution to modify phase fractions and mitigate weldability related concerns such as solidification cracking or reduced corrosion performance.

42 ENGINEERING↗