The increase in luminosity, and consequent higher backgrounds, of the LHC upgrades require improved rejection of fake tracks in the forward region of the ATLAS Muon Spectrometer. The New Small Wheel upgrade of the Muon Spectrometer aims to reduce the large background of fake triggers from track segments that don't originate from the interaction point. The New Small Wheel employs two detector technologies, the resistive strip Micromegas detectors and the “small” Thin Gap Chambers, with a total of 2.45 million electrodes to be sensed. The two technologies require the design of a complex electronics system given that it consists of two different detector technologies and is required to provide both precision readout and a fast trigger. It will operate in a high background radiation region up to about 20 kHz/cm 2 at the expected HL-LHC luminosity of $\mathcal{L}$= 7.5 × 10 34 cm -2 s -1 . The architecture of the system is strongly defined by the GBTx data aggregation ASIC, the newly-introduced FELIX data router and the software based data handler of the ATLAS detector. The electronics complex of this new detector was designed and developed in the last ten years and consists of multiple radiation tolerant Application Specific Integrated Circuits, multiple front-end boards, dense boards with FPGA's and purpose-built Trigger Processor boards within the ATCA standard. The New Small Wheel has been installed in 2021 and is undergoing integration within ATLAS for LHC Run 3. It should operate through the end of Run 4 (December 2032). In this manuscript, the overall design of the New Small Wheel electronics is presented.

47 OTHER INSTRUMENTATION↗

Ex Situ Spark Plasma Sintering of Short Powder-in-Tube MgB{sub 2} Tapes with Open and Closed Ends

Short powder-in-tube tapes of MgB{sub 2} in the Fe sheath were fabricated by ex situ route from a commercial powder containing some free Mg and MgO impurity phases. The final heat treatment was performed by spark plasma sintering (SPS). Tapes were with open (OT) or closed (CT) endings. Closed endings were made by folding and pressing. The MgB{sub 2} core of the OT sample has shown a higher low-field critical current density, a higher maximum pinning force, a slightly higher disorder, smaller average MgB{sub 2} crystallite size, a weak contact between Fe and MgB{sub 2} core, and more macro-flux jumps. The upper and irreversibility fields were similar for OT and CT samples. In the center of the MgB{sub 2} cores, the detected impurity phase is MgO, while at the interface with Fe, MgB{sub 4} also occurs. Impurity phases found at interface, MgO and MgB{sub 4}, are present in the center of the bulk SPSed samples. Reactions and pinning-force-related parameters are discussed with respect to Mg behavior influenced by condition of endings. It is inferred that the presence of free Mg in the raw MgB{sub 2} powder has an important contribution to observed differences, and its removal or control is recommended.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Dwell Time Influence on Spark Plasma-Sintered MgB{sub 2}

Samples of MgB{sub 2} with relative density above 95% were obtained by spark plasma sintering (SPS) at 1150 °C for a heating time of 100 °C/min and a maximum pressure of 95 MPa. Dwell time was of 1, 4, 7, 10, and 20 min. Samples show that dwell time has a low influence on superconducting characteristics. However, small differences were observed and they are discussed from the viewpoint of density, structural, microstructural, critical current density, irreversibility field, and pinning type. The dominant contribution for all investigated samples is given by point and δT{sub c} pinning.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Graphene addition to MgB{sub 2} superconductor obtained by ex-situ spark plasma sintering technique

Highlights: • Graphene-added dense MgB{sub 2} was prepared by ex-situ spark plasma sintering. • There is a limited interaction between graphene and MgB{sub 2}. • Addition of graphene (G) shows a small enhancement of J{sub c} and μ{sub 0}H{sub irr}. • G is one of the least effective C-containing additions. - Abstract: Graphene nanopowder (G) with average thickness particle size of about 6–8 nm was added to MgB{sub 2} commercial powder. Starting composition was (MgB{sub 2}){sub (1−x)}(G){sub x}, x = 0.0125, 0.025, 0.05. Processing was performed by Spark Plasma Sintering (SPS) technique. All added samples have high density (above 95%). The critical temperature (T{sub c}) and the lattice parameter a (c-axis lattice parameter is constant) show a small variation suggesting that carbon substitution for boron is low. TEM observations show the presence of un-reacted graphene plates supporting the T{sub c} and structural results. It also indicates that G-addition does not modify the MgB{sub 2} microstructure. Despite this, there is an optimum doped sample (MgB{sub 2}){sub 0.9875}(G){sub 0.0125} for which the critical current density at temperatures below 25 K is slightly higher at high magnetic fields than for the pristine sample. The addition of G is found as one of the least effective C-source additions enhancing J{sub c}. We discuss results as being strongly related to variation of the residual stress.