Surface damage on diamond membranes fabricated by ion implantation and lift-off

Thin membranes with excellent optical properties are essential elements in diamond based photonic systems. Due to the chemical inertness of diamond, ion beam processing must be employed to carve photonic structures. One method to realize such membranes is ion-implantation graphitization followed by chemical removal of the sacrificial graphite. The interface revealed when the sacrificial layer is removed has interesting properties. To investigate this interface, we employed the surface sensitive technique of grazing angle channeled Rutherford backscattering spectroscopy. Even after high temperature annealing and chemical etching a thin layer of damaged diamond remains, however, it is removed by hydrogen plasma exposure.

36 MATERIALS SCIENCE↗

Photophysics of chromium-related diamond single-photon emitters

A detailed study of the photophysical properties of several chromium-related color centers produced within chemical vapor deposition diamond is presented. These emitters show narrow luminescence lines in the range of 740-770 nm. Single-photon emission was verified with continuous and pulsed excitation with detected emission rates at saturation in the range of (2-3) x 10{sup 6} counts/s, while direct lifetime measurements reveal excited state lifetimes for the distinct centers ranging 1-14 ns. In addition, a number of quantum emitters demonstrate two-level behavior with no bunching present in the second-order correlation function. The three-level systems revealed typically photoluminescence lines with width half-maximum of {approx}4 nm while the two-level emitters have full width half-maximum of {approx}10 nm at room temperature. In addition, the quantum efficiency of the two-level system was measured to be four times higher than that of the three-level system.

36 MATERIALS SCIENCE↗

Microstructure evolution in carbon-ion implanted sapphire

Carbon ions of MeV energy were implanted into sapphire to fluences of 1x10{sup 17} or 2x10{sup 17} cm{sup -2} and thermally annealed in forming gas (4% H in Ar) for 1 h. Secondary ion mass spectroscopy results obtained from the lower dose implant showed retention of implanted carbon and accumulation of H near the end of range in the C implanted and annealed sample. Three distinct regions were identified by transmission electron microscopy of the implanted region in the higher dose implant. First, in the near surface region, was a low damage region (L{sub 1}) composed of crystalline sapphire and a high density of plateletlike defects. Underneath this was a thin, highly damaged and amorphized region (L{sub 2}) near the end of range in which a mixture of i-carbon and nanodiamond phases are present. Finally, there was a pristine, undamaged sapphire region (L{sub 3}) beyond the end of range. In the annealed sample some evidence of the presence of diamond nanoclusters was found deep within the implanted layer near the projected range of the C ions. These results are compared with our previous work on carbon implanted quartz in which nanodiamond phases were formed only a few tens of nanometers from the surface, a considerable distance from the projected range of the ions, suggesting that significant out diffusion of the implanted carbon had occurred.

36 MATERIALS SCIENCE↗

Bulk and surface thermal stability of ultra nanocrystalline diamond films with 10-30 nm grain size prepared by chemical vapor deposition.

The thermal stability of nanocrystalline diamond films with 10-30 nm grain size deposited by microwave enhanced chemical vapor deposition on silicon substrate was investigated as a function of annealing temperature up to 1200 C. The thermal stability of the surface-upper atomic layers was studied with near edge x-ray absorption fine structure (NEXAFS) spectroscopy recorded in the partial electron yield mode. This technique indicated substantial thermally induced graphitization of the film within a close proximity to the surface. While in the bulk region of the film no graphitization was observed with either Raman spectroscopy or NEXAFS spectroscopy recorded in total electron yield mode, even after annealing to 1200 C. Raman spectroscopy did detect the complete disappearance of transpolyacetylene (t-PA)-like v{sub 1} and v{sub 3} modes following annealing at 1000 C. Secondary ion mass spectroscopy, applied to investigate this relative decrease in hydrogen atom concentration detected only a {approx}30% decrease in the bulk content of hydrogen atoms. This enhanced stability of sp{sup 3} hybridized atoms within the bulk region with respect to graphitization is discussed in terms of carbon bond rearrangement due to the thermal decomposition of t-PA-like fragments.