Search NASA⌕ Search

Engineering topics

Prithivirajan, Veerappan

Publications and source records attributed to Prithivirajan, Veerappan.

Examining Graphite Degradation in Molten Salt Environments: A Chemical, Physical, and Material Analysis

Molten-salt reactors (MSRs) are Generation IV nuclear reactors that use liquid salt as a coolant and/or fuel. In several MSR designs, graphite serves as a moderator and/or reflector. However, due to limited experimental data and operational experience, our understanding of graphite behavior in molten salt environments remains incomplete. This report aims to identify the degradation mechanisms of nuclear graphite in MSRs, detail the mechanisms of each factor, and provide an initial assessment of their impact on the structural integrity of graphite components. This assessment is based on an extensive literature review and insights from subject matter experts. Furthermore, given the limited data, a modeling strategy using existing Grizzly software is proposed for a more thorough analysis where appropriate. Additionally, it presents mitigation strategies where applicable. The report covers physical degradation mechanisms such as infiltration, erosion, and abrasion, as well as chemical degradation mechanisms including fluorination, intercalation, corrosion, and oxidation. Molten salt can infiltrate the porous structure of graphite, leading to several detrimental effects. Entrapment of fissile products within the graphite pores can cause radiation damage and could pose challenges in the handling and disposal of contaminated components. The differential thermal expansion between the infiltrated salt and graphite, along with internal stress from pressurized molten salt and volumetric heating, can compromise the structural integrity of graphite. To mitigate these effects, employing ultra-fine graphite grades and applying sealants and coatings are effective strategies. A computational model based on coupled solid mechanics and heat transfer phenomena could be used to predict the internal stresses using Grizzly software. In pebble-bed MSRs, graphite fuel pebbles can cause abrasion against reactor components due to friction and wear. The severity of wear is influenced by various factors such as temperature, environment, and the presence of lubricants. Tribological studies reveal that higher temperatures and molten salt environments, such as FLiBe, significantly reduce wear rates compared to dry conditions. Additionally, the chemical composition of the salt can further optimize graphite's tribological performance. Long-term wear effects can be modeled by incorporating surface defects into the geometry and predict stresses under thermal and radiation effects using Grizzly software. Chemical degradation of graphite in a molten salt environment can occur through fluorination and intercalation. Fluorination can occur via replacement of hydrogen or oxygen atoms, or at the active sites, but does not cause structural degradation. Intercalation, on the other hand, can lead to exfoliation, where layers of graphite separate and peel away, damaging the graphite. Protective coatings can enhance graphite's resistance to intercalation. Graphite generally exhibits good chemical stability in molten salt environments, though it can corrode under specific conditions, particularly in the presence of impurities or oxidants. Studies have shown that protective coatings, such as plasma-sprayed partially stabilized zirconia (PSZ), can effectively prevent such degradation. Corrosion behavior varies significantly with different graphite grades and coating applications, underscoring the need for detailed studies on uncoated and coated graphite to understand and mitigate corrosion mechanisms in MSRs. Research indicates that the presence of oxidants and impurities can accelerate graphite degradation in molten salts, making it essential to explore acceptable impurity limits. Oxidation is another critical degradation mechanism, leading to weight loss and structural damage due to the formation of CO and CO 2 from the reaction of carbon atoms with oxygen. This process creates new porosity and compromises graphite's integrity. While extensive research on graphite oxidation has been conducted for gas-cooled reactors, studies specific to MSRs are limited. Findings from the coal industry suggest that molten alkali metal salts can significantly accelerate graphite oxidation, a hypothesis worth exploring for fluoride salts in MSRs. Understanding oxidation behavior in MSRs is vital for developing protective measures. The analysis of post-irradiated graphite from the MSRE experiment demonstrated exceptional chemical compatibility with molten fluoride salt, suggesting that the extent of chemical attack on graphite largely depends on the salt's infiltration capability. Therefore, the use of ultra-fine grade graphite could help mitigate chemical degradation effects. Existing oxidation modeling capabilities in Grizzly, which use reaction-diffusion equations to model graphite-air interactions, could be adapted to simulate the chemical degradation effects of graphite in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Overview of Graphite Model Development

Overview of graphite model development. Discuss graphite in motel salt, potential degradation mechanisms, stress due to volumetric heating, and the role of different parameters. Also wear modeling, modeling salt infiltration into graphite, oxidation modeling, and the existing graphite models.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Development of Graphite Thermal and Mechanical Modeling Capabilities in Grizzly

Nuclear-grade graphites are used extensively in the core designs of multiple types of advanced nuclear reactors. In the reactor environment, graphite is exposed over long durations to extreme conditions, including high temperatures, radiation and potentially molten salt and oxygen. Exposure to these conditions can cause several degradation mechanisms in graphite, including nonuniform volumetric strains induced by irradiation and thermal expansion, which lead to stresses that can compromise the performance of graphite components. Evaluating component integrity, predicting component performance over the reactor lifetime, and developing design standards all require robust tools for predicting fracture initiation and propagation in graphite structural components in nuclear reactors. This report documents progress in an ongoing effort to develop modeling and simulation tools in the Grizzly code for predicting the performance of graphite exposed to reactor conditions. Recent developments include a set of thermal and mechanical models that now include the IG-110, NBG-18, and H-451 graphite grades. Improvements have also been made to a nonlinear damaged plasticity model applicable to predicting damage under tension and compression to quasibrittle materials, including graphite. In addition, enhancements have been made to the extended finite element method implementation targeted at simulating graphite fracture. These include new capabilities for crack nucleation in the interior of a solid body, improved treatment of crack nucleation on free surfaces, and more robust modeling approaches for crack growth approaching free surfaces or other cracks.

36 MATERIALS SCIENCE↗

Initial Fracture Propagation Modeling of Graphite Components with Grizzly

Graphite has historically been extensively used in power reactor cores and will be used in multiple types of advanced reactors currently under development. These graphite structural components can experience significant stresses due to nonuniform volumetric strains induced by irradiation and thermal expansion, which can lead to fracture. Robust tools for predicting fracture initiation and propagation in graphite structural components in nuclear reactors are important for evaluating component integrity, developing design standards, and interpreting experimental results to characterize graphite performance. The U.S. Department of Energy’s Nuclear Energy Advanced Modeling and Simulation program has been developing degradation models for other structural components in nuclear reactors within the Grizzly and BlackBear codes. This report documents an effort to develop initial capabilities for modeling graphite fracture within these codes, building on prior efforts to model fracture in other materials. Major elements of this effort include developing a new system for modeling fracture nucleation and growth in two dimensions using the extended finite element method and incorporating a damage and plasticity model. These capabilities are applied here to model a representative graphite component and a splitting disc experiment used to obtain tensile strength.

36 MATERIALS SCIENCE↗

ICME Approach to Determining Critical Pore Size of IN718 Produced by Selective Laser Melting

A degree of porosity is expected in additively manufactured (AM) materials. To aid in the qualification of AM materials, the smallest pore size that results in a debit in the fatigue performance is quantified. In the work presented herein, crystal plasticity simulations are used to identify the stress concentration around pores of various sizes, revealing that a single 20-mu m pore or two 10-mu m pores (with centers spaced 15 mu m apart) localize stress at the pore, as opposed to elsewhere in the microstructure. In situ microtomography and far-field high-energy x-ray diffraction microscopy were used to identify crack formation and the evolution of the grain-level micromechanical fields during cyclic loading. Eighteen cracks were observed (15 at pores, 3 at the surface) at highly stressed grains in a sample, although most did not propagate. The dominant crack was seen to originate from the free surface, which is rationalized by fracture mechanics.

36 MATERIALS SCIENCE↗