Using in-situ strain measurements to evaluate the accuracy of stress estimation procedures from fracture injection/shut-in tests

Fracture injection/shut-in tests are commonly used to measure the state of stress. Injection creates a hydraulic fracture (or in some cases, opens a preexisting fracture), and then the pressure after shut-in is monitored to identify fracture closure. Different interpretation procedures have been proposed for estimating closure, and the procedures sometimes yield significantly different results. In this study, direct, in-situ strain measurements are used to observe fracture reopening and closure. The tests were performed as part of the EGS Collab project, a mesoscale project performed at 1.25 and 1.5 km depth at the Sanford Underground Research Facility. The tests were instrumented with the SIMFIP tool, a double-packer probe with a high-resolution three-dimensional borehole displacement sensor. The measurements provide a direct observation of the fracture closure signature, enabling a high-fidelity estimate of the fracture closure stress (ie, the normal stress on the fracture). In two of the four tests, injection created an opening mode fracture, and so the closure stress can be interpreted as the minimum principal stress. In the other two tests, injection probably opened preexisting natural fractures, and so the closure stress can be interpreted as the normal stress on the fractures. The strain measurements are compared against different proposed methods for estimating closure stress from pressure transients. The shut-in transients are analyzed with two techniques that are widely used in the field of petroleum engineering – the ‘tangent’ method and the ‘compliance’ method. In three of the four tests, the tangent method significantly underestimates the closure stress. The compliance method is reasonably accurate in all four tests. Closure stress is also interpreted using two other commonly-used methods – ‘first deviation from linearity’ and the method of Hayashi and Haimson. In comparison with the SIMFIP data, these methods tend to overestimate the closure stress, evidently because they identify closure from early-time transient effects, such as near-wellbore tortuosity. In two of the tests, microseismic imaging provides an independent estimate of the size of the fracture created by injection. When combined with a simple mass balance calculation, the SIMFIP stress measurements yield predictions of fracture size that are reasonably consistent with the estimates from microseismic. In conclusion, the calculations imply an apparent fracture toughness 2-3x higher than typical laboratory-derived values.

58 GEOSCIENCES↗

The EGS Collab Project – Stimulations at Two Depths

The EGS Collab project, supported by the US Department of Energy, is performing intensively monitored rock stimulation and flow tests at the 10-m scale in an underground research laboratory to address challenges in implementing enhanced geothermal systems (EGS). Data and observations from the field tests are compared to simulations to understand processes and build confidence in numerical modeling of the processes. We have completed Experiment 1 (of 3), which examined hydraulic fracturing in a well-characterized underground fractured phyllite test bed at a depth of approximately 1.5 km at the Sanford Underground Research Facility (SURF) in Lead, South Dakota. Testbed characterization included fracture mapping, borehole acoustic and optical televiewers, full waveform sonic, conductivity, resistivity, temperature, campaign p- and s-wave investigations and electrical resistance tomography. Borehole geophysical techniques including passive seismic, continuous active source seismic monitoring, electrical resistance tomography, fiber-based distributed strain, distributed temperature, and distributed acoustic monitoring, were used to carefully monitor stimulation events and flow tests. More than a dozen stimulations and nearly one year of flow tests were performed. Quality data and detailed observations were collected and analyzed during stimulation and water flow tests using ambient temperature and chilled water. We achieved adaptive control of the tests using real-time monitoring and rapid dissemination of data and near-real-time simulation. More detailed numerical simulation was performed to answer key experimental design questions, forecast fracture propagation trajectories and extents, and analyze and evaluate results. Data are freely available from the Geothermal Data Repository. Experiment 2 examines the potential for hydraulic shearing in amphibolite at a depth of about 1.25 km at SURF. This site has a different set of stress and fracture conditions than Experiment 1. The Experiment 2 testbed consists of nine subhorizontal boreholes configured in two fans of two boreholes which surround the testbed and contain grouted-in electrical resistance tomography, seismic sensors, active seismic sources and distributed fiber sensors. A “five-spot” set of test wells that extends from a custom mined alcove includes an injection well and four production/monitoring wells. The testbed was characterized geophysically and hydrologically, and three stimulations have been performed using the Step-Rate Injection Method for Fracture In-Situ Properties (SIMFIP) tool to measure strains, and a new strain quantifying tool (downhole robotic strain analysis tool -DORSA) was deployed in a monitoring hole during stimulation. Real-time data were broadcast during stimulations to allow real-time response to arising issues.

EGS Collab, Enhanced Geothermal Systems, EGS, fiel↗

Inorganic Corrosion-Inhibitive Pigments for High-Temperature Alkali-activated Well Casing Foam Cement

This study evaluates inorganic pigments for improving carbon steel (CS) brine-corrosion protection by the sodium metasilicate-activated calcium aluminate cement/Fly Ash blend at 300°C. Calcium borosilicate (CBS) and zinc phosphate, significantly improved CS corrosion-protection by decreasing cement’s permeability for corrosive ions and inhibiting anodic corrosion. An amorphous Na 2 O-Al 2 O 3 -SiO 2 -H 2 O phase tightly attached to CS surface formed at 300oC in CBS-modified cement pore solution. The corrosion rate of the CS covered with this phase was nearly 4-fold lower than in the case of nonmodified cement pore solution where the major phase formed on the surface of CS was crystalline analcime.

15 GEOTHERMAL ENERGY↗

Corrosion-resistant Foamed Cements for Carbon Steels

The cementitious material consisting of Secar #80, Class F fly ash, and sodium silicate designed as an alternative thermal-shock resistant cement for the Enhanced Geothermal System (EGS) wells was treated with cocamidopropyl dimethylamine oxide-based compound as foaming agent (FA) to prepare numerous air bubble-dispersed low density cement slurries of and ≤1.3 g/cm 3 . Then, the foamed slurry was modified with acrylic emulsion (AE) as corrosion inhibitor.

15 GEOTHERMAL ENERGY↗

Self-decomposable Fibrous Bridging Additives for Temporary Cementitious Fracture Sealers in EGS Wells

This study evaluates compatibility of a self-degradable temporary fracture sealer with the drilling mud and plugging and self-degrading performance of different fibers to be used in combination with the sealer. The sodium silicate-activated slag/Class C fly ash (SSASC) cementitious sealer must plug fractures at 85oC to allow continuous well drilling and it must degrade and leave the fractures open for water at later times when exposed to temperatures above 200oC. The sealer showed good compatibility with the mud. Even the blend of 80/20 vol.% of sealer/mud reached a compressive strength of more than 2000 psi set as one of the material criteria, mostly due to the additional activation of the slag and Class C fly ash by the alkaline ingredient present in the drilling fluid. In contrast, the drilling fluid was detrimental to the compressive strength development in conventional Class G well cement, so that it failed to meet this criterion. Among several organic fibers tested both polyvinyl alcohol (PVA)-and nylon-based fibers showed adequate plugging of the sealer in slot nozzles of 1-in. wide x 6-in. long x 0.08 in. and 0.24 in. high under pressures up to 700 psi. PVA fibers displayed better compressive toughness and self-degrading properties than nylon. The compressive toughness of sealers made by adding 1.0 wt% 6 mm-length PVA and 0.5 wt% 19 mm-length PVA was 9.5-fold higher than that of a non-bridged sealer. One factor governing the development of such high toughness was an excellent adherence of PVA to the SSASC cement. The alkali-catalyzed self-decomposition of PVA at 200°C led to the morphological transformation of the material from a fibrous structure to a microscale flake-like structure that helped the desirable conversion of the sealer into small fragments. In contrast, nylon’s decomposition provided a reticular network structure in the self-degraded sealer resulting in bigger fragments compared against the sealer with PVA. The PVA fiber has a high potential as a self-decomposable bridging additive in the SSASC cement sealer.

15 GEOTHERMAL ENERGY↗

Effect of Sodium Carboxymethyl Celluloses on Water-catalyzed Self-degradation of 200°C-heated Alkali-Activated Cement

We investigated the usefulness of sodium carboxymethyl celluloses (CMC) in promoting self-degradation of 200°C-heated sodium silicate-activated slag/Class C fly ash cementitious material after contact with water. CMC emitted two major volatile compounds, CO 2 and acetic acid, creating a porous structure in cement. CMC also reacted with NaOH from sodium silicate to form three water-insensitive solid reaction products, disodium glycolate salt, sodium glucosidic salt, and sodium bicarbonate. Other water-sensitive solid reaction products, such as sodium polysilicate and sodium carbonate, were derived from hydrolysates of sodium silicate. Dissolution of these products upon contact with water generated heat that promoted cement’s self-degradation. Thus, CMC of high molecular weight rendered two important features to the water-catalyzed self-degradation of heated cement: One was the high heat energy generated in exothermic reactions in cement; the other was the introduction of extensive porosity into cement.

15 GEOTHERMAL ENERGY↗

Thermal Shock-resistant Cement

We studied the effectiveness of sodium silicate-activated Class F fly ash in improving the thermal shock resistance and in extending the onset of hydration of Secar #80 refractory cement. When the dry mix cement, consisting of Secar #80, Class F fly ash, and sodium silicate, came in contact with water, NaOH derived from the dissolution of sodium silicate preferentially reacted with Class F fly ash, rather than the #80, to dissociate silicate anions from Class F fly ash. Then, these dissociated silicate ions delayed significantly the hydration of #80 possessing a rapid setting behavior. We undertook a multiple heating -water cooling quenching-cycle test to evaluate the cement’s resistance to thermal shock. In one cycle, we heated the 200°C-autoclaved cement at 500°C for 24 hours, and then the heated cement was rapidly immersed in water at 25°C. This cycle was repeated five times. The phase composition of the autoclaved #80/Class F fly ash blend cements comprised four crystalline hydration products, boehmite, katoite, hydrogrossular, and hydroxysodalite, responsible for strengthening cement. After a test of 5- cycle heat-water quenching, we observed three crystalline phase-transformations in this autoclaved cement: boehmite → γ-Al 2 O 3 , katoite → calcite, and hydroxysodalite → carbonated sodalite. Among those, the hydroxysodalite → carbonated sodalite transformation not only played a pivotal role in densifying the cementitious structure and in sustaining the original compressive strength developed after autoclaving, but also offered an improved resistance of the #80 cement to thermal shock. In contrast, autoclaved Class G well cement with and without Class F fly ash and quartz flour failed this cycle test, generating multiple cracks in the cement. The major reason for such impairment was the hydration of lime derived from the dehydroxylation of portlandite formed in the autoclaved cement, causing its volume to expand.

15 GEOTHERMAL ENERGY↗