Quantifying optical loss of high-voltage degradation modes in photovoltaic modules using spectral analysis

The direct current bias for photovoltaic (PV) modules interconnected in series-strings may include both high voltage negative (“HV-”) and positive (“HV+”) polarity with respect to the electrical ground. Multiple degradation modes, resulting in quantifiable optical loss, were found to occur during HV-/HV+ sequential stress, including corrosion of the external glass surface, encapsulant delamination (at its interfaces with the glass and the PV cell), internal haze formation (resulting from a chemical interaction between the glass and the encapsulant), corrosion and migration of the gridlines, and corrosion of the silicon nitride (Si x N y ) antireflective coating on the cell. The effects of these separate modes were examined using monolithic (e.g., glass or PV cell) and laminated-coupon (glass/encapsulant/glass or glass/encapsulant/cell/encapsulant/backsheet) specimens. Characterizations during and after unbiased accelerated testing at 85°C/85% relative humidity included spectrophotometry, optical microscopy, electron microscopy, and ellipsometry. For some module components (i.e., the glass and the Si x N y coating), the optical performance was determined through iterative analysis of empirical measurements. Concentrating on just their spectral effect, a novel model was then developed to estimate the transfer of light to the PV cell and the return of light from the PV module with simultaneous degradation mechanisms, which was compared with a mini-module previously subjected to HV-/HV+ stress. Here the model suggests that one third of the current loss observed for the mini-module can be attributed to the optical degradation of the packaging materials. The dominant degradation modes include encapsulant delamination and corrosion of the Si x N y coating. Recommendations are given so that the optical model may be improved relative to accelerated testing and validated relative to field aging.

14 SOLAR ENERGY↗

Quantifying Optical Loss of High-Voltage Degradation Modes in PV Modules Using Spectral Analysis [Slides]

The direct current bias for photovoltaic (PV) modules interconnected in series-strings may include both high voltage negative ("HV-") and positive ("HV+") polarity with respect to the electrical ground. Multiple degradation modes, resulting in quantifiable optical loss, were found to occur during HV-/HV+ sequential stress, including: corrosion of the external glass surface, encapsulant delamination (at its interfaces with the glass and the PV cell), internal haze formation (resulting from a chemical interaction between the glass and the encapsulant), corrosion and migration of the gridlines, and corrosion of the silicon nitride (SixNy) antireflective coating on the cell. The effects of these separate modes were examined using monolithic (e.g., glass or PV cell) and laminated-coupon (glass/encapsulant/glass or glass/encapsulant/cell/encapsulant/backsheet) specimens. Characterizations during and after unbiased accelerated testing at 85 degrees C/85% relative humidity included: spectrophotometry, optical microscopy, electron microscopy, and ellipsometry. For some module components (i.e., the glass and the SixNy coating), the optical performance was determined through iterative analysis of empirical measurements. Concentrating on just their spectral effect, a novel model was then developed to estimate the transfer of light to the PV cell and the return of light from the PV module with simultaneous degradation mechanisms, which was compared to a mini-module previously subjected to HV-/HV+ stress. The model suggests one-third of the current loss observed for the mini-module can be attributed to the optical degradation of the packaging materials. The dominant degradation modes include encapsulant delamination and corrosion of the SixNy coating. Recommendations are given so that the optical model may be improved relative to accelerated testing and validated relative to field aging.

14 SOLAR ENERGY↗

Value Proposition of UV-Absorbers in PV Module Encapsulation

Various common crystalline silicon cell technologies were exposed to UVA radiation (1.24 Wm-2 nm-1 at 340 nm peak) on the front and back faces at 45 degrees Celsius for periods up to 3000 h, representing about 3 y of solar exposure in Phoenix, Arizona, USA. The resulting degradation of the open-circuit voltage and short-circuit current is presented. Of the various cell types examined, significant levels of degradation were seen in all cases. Less degradation was generally found after UV irradiation of cell fronts and older cell types, whereas a bifacial PERC type exposed on the rear showed about 25% degradation in short circuit current, attributable to lack of a diffused surface field. Selected cells were exposed to UV irradiation with the addition of long pass UV filters to replicate UV-absorbers in encapsulants. Modern cell designs are sensitive to UV-ID because of reduced or eliminated front and back surface field and increased dependence on high quality surface passivation. Single transformation of the independent variable (t, kW h/m^2) could be used to achieve a linear model of the data to extrapolate to 50 y. Solar Advisor Model (SAM) shows appropriate filtering of UV-irradiation can improve LCOE and net present value of plant. Some advanced cell types are seen to be UV-resistant (cell level solutions also exist). Solutions therefore exist on the cell, glass, and encapsulant level. Changes over time in each of these would also need to be considered (solarization, encapsulant browning...).

ENGINEERING,SOLAR ENERGY↗

Module-Level Solutions For Degradation by Ionization Damage

After years of improving module efficiency while targeting mean degradation rates of 0.5 to 0.6 %/y for crystalline silicon technology, there is much evidence that the degradation rates are now increasing significantly. Contributing factors include:Radiation damage (UV-Light Induced Degradation): Trina solar: -4.5%/y degradation rate in Singapore, DOE National Laboratory Regional Test Centers showed degradation of -1% < r < -2%/y in crystalline silicon modules, Jinko Solar: -4% < r < -7% efficiency loss from 540 MJ/m-2 of UV-A light, ISFH: 15% relative power loss during of 1.8 GJ/m-2 UV exposure, attributed to H+. Electrical bias from positive system voltage (e.g., +1000 V, +1500 V) can drive ions and metallization through the encapsulation, NREL: Ion transport can affect the cell passivation, resulting in power loss of 5% to 40% in p-PERC+ (bifacial), NREL: Damage at cell rear with up to 17% power at cell fronts in n-PERT modules. Delamination can also occur due to cell surface reactions driven by light and bias.

module efficiency↗

UV‐induced degradation of high‐efficiency silicon PV modules with different cell architectures

Abstract Degradation from ultraviolet (UV) radiation has become prevalent in the front of solar cells due to the introduction of UV‐transmitting encapsulants in photovoltaic (PV) module construction. Here, we examine UV‐induced degradation (UVID) in various commercial, unencapsulated crystalline silicon cell technologies, including bifacial silicon heterojunction (HJ), interdigitated back contact (IBC), passivated emitter and rear contact (PERC), and passivated emitter rear totally diffused (PERT) solar cells. We performed UV exposure tests using UVA‐340 fluorescent lamps at 1.24 W·m −2 (at 340 nm) and 45°C through 4.02 MJ·m −2 (2000 h). Our results showed that modern cell architectures are more vulnerable to UVID, leading to a significant power decrease (−3.6% on average; −11.8% maximum) compared with the conventional aluminum back surface field (Al‐BSF) cells (<−1% on average). The power degradation is largely caused by the decrease in short‐circuit current and open‐circuit voltage. A greater power decrease is observed in bifacial cells with rear‐side exposure compared with those with front‐side exposure, indicating that the rear side is more susceptible to UV damage. Secondary ion mass spectroscopy (SIMS) confirmed an increase in hydrogen concentration near the Si/passivation interface in HJ and IBC cells after UV exposure; the excess of hydrogen could result in hydrogen‐induced degradation and subsequently cause higher recombination losses. Additionally, surface oxidation and hot‐carrier damage were identified in PERT cells. Using a spectral‐based analysis, we obtained an acceleration factor of 5× between unpackaged cells (containing a silicon nitride antireflective coating on the front) in the UV test and an encapsulated module (with the front glass and encapsulant blocking 90% of the UV at 294 nm and 353 nm, respectively) in outdoor conditions. From the analytical calculations, we show that a UV‐blocking encapsulant can reduce UV transmission in the module by an additional factor of ~50.

14 SOLAR ENERGY↗

Interfacial Characterization of Positive Bias Voltage Degradation in PV Modules

Degradation from high system voltage is a prevailing failure mode in fielded photovoltaic modules, and the degradation mechanism is inherently dependent on the bias polarity. Here we report the effects of positive bias. Modules under positive bias demonstrated a significant photocurrent loss caused by two routes. First, delamination and discoloration of the silicon nitride layer, leading to optical loss determined by reflectance measurements. Second, chemical discoloration of the cell gridlines and encapsulant (EVA), which is linked to an electrochemical reaction at the silver electrodes. Chemical compositional analysis using X-ray photoemission spectroscopy demonstrated that the discoloration is attributed to Ag 2 S and/or Ag 2 O. Evidence of Ag ion migration from the cell grid into the encapsulant is observed after shallow depth profiling on the EVA surface. However, Ag was not detected at the EVA/glass interface, inferring limited Ag ion transport through the EVA. The source of sulfur is believed to be ambient air, which diffused into the module through the breathable backsheet.

characterization↗

UV-Induced Degradation of High-Efficiency Solar Cells with Different Architectures

The ultraviolet-induced degradation (UVID) of solar panels is associated with the deterioration of cell performance and reduced reliability of packaging materials. Here we examine the UV stability of different architectures of high-efficiency solar cells without any encapsulation. Identical UV exposure tests were performed at two different labs using UVA-340 fluorescent lamps under different electrical bias configurations (open- or short-circuit) and irradiated cell surfaces (for bifacial technologies). Cell technologies, including heterojunction (HJ), interdigitated back-contact cells (IBC), passivated emitter rear contact (PERC), passivated emitter rear totally-diffused (PERT), are found to be more susceptible to UVID, leading to significant Isc loss (up to 4%) and P max loss (up to 15%) as compared to the conventional back surface field (Al-BSF) cells after exposure to UV irradiation of 8.92 MJ-m -2 -nm -1 at 340 nm. Additionally, the bifacial cells when irradiated from the backside exhibited greater photocurrent loss compared to the front side exposure, indicating potential sensitivity of rear surface passivation to UV radiation.

crystalline silicon↗

Destructive reverse bias pinning in perovskite/silicon tandem solar modules caused by perovskite hysteresis under dynamic shading

In this work, we demonstrate how perovskite hysteresis can result in permanent reductions in power output in perovskite/silicon tandem modules—including irreversible hotspot-induced damage—from only brief periods of shading. We show that reverse bias events in which a perovskite cell is biased above a threshold voltage—which in this work we find to be as low as –1.1 V—produces a temporary reduction in power output that is of sufficient magnitude to keep the cell pinned in reverse bias after the shading event ends. As a hysteretic phenomena, this crucial failure mode may be overlooked by static models of perovskite-based solar cells. Higher reverse bias voltages exacerbate the temporary reduction in short-circuit photocurrent, which is also sensitive to the level of illumination under reverse bias. Numerical device modelling demonstrates that this effect is consistent with our understanding of perovskite hysteresis as a consequence of mobile ion-electron coupling controlling rates of non-radiative recombination over time. Measurements of the dynamic response of single-junction perovskite cells are extrapolated to two-terminal and four-terminal perovskite/silicon tandem module modelling. We validate these models with measurements from an equivalent electronic circuit that represents a two-terminal perovskite–silicon tandem mini module. Two module-level solutions are discussed that address this issue, which includes increasing the number of bypass diodes and choosing better suited silicon bottom cells with higher shunter resistance in two-terminal tandem modules.