Search NASA⌕ Search

Engineering topics

Qiao, Junwei

Publications and source records attributed to Qiao, Junwei.

Shear band velocity and activation volume during shear deformation by acoustic emission in a Zr-based bulk metallic glass

Here, an analysis is presented for the shear band velocity of plastic deformation and activation volume of the shear transformation zone (STZ) in a Zr 60 Cu 30 Al 10 bulk metallic glass (BMG). Compared to the values calculated by the stick-slip model, the values of shear band velocity calculated after optimization by the acoustic emission technique are much larger than those reported previously. Plastic flow in BMGs is found to be described by a power-law correlation between the maximum velocity of the shear band and the strain rates. Combining the free volume theory and the STZ theory, the relationship between the volume change in the STZ and the shear band velocity is derived as $Ω=A$(27–ln$v/l$). The value of A, which is a material dependent constant, is 5.43 × 10 –3 for the current BMG at room temperature.

36 MATERIALS SCIENCE↗

Relation Between the Defect Interactions and the Serration Dynamics in a Zr-Based Bulk Metallic Glass

For this study, the effects of thermal annealing and compressive strain rate on the complexity of the serration behavior in a Zr-based bulk metallic glass (BMG) was investigated. Here, as-cast and thermally-annealed (300 °C, 1 week) Zr 52.5 Cu 17.9 Ni 14.6 Al 10 Ti 5 BMG underwent room-temperature compression tests in the unconstrained condition at strain rates of 2 × 10 -5 s -1 and 2 × 10 -4 s -1 . The complexity of the serrated flow was determined, using the refined composite multiscale entropy technique. Nanoindentation testing and X-ray diffraction characterization were performed to assess the changes in the microstructure and mechanical properties of the BMG that occurred during annealing. The results indicated that the BMG did not crystallize during annealing in the prescribed heating condition. Nanoindentation tests revealed that annealing led to a significant increase in the depth-dependent nanoindentation hardness and Young’s modulus, which were attributed to the structural relaxation in the glass. Furthermore, both annealing and an increased strain rate resulted in a marked enhancement in the complexity of the serrated flow during compression. It was concluded that the increase in the sample entropy with increasing strain rate is related to an increase in the number of defect interactions during the serrated flow.

36 MATERIALS SCIENCE↗