Modeling the non-Schmid crystallographic slip in MAX phases

We present a crystal plasticity constitutive relation for the description of experimentally observed non-Schmid crystallographic slip in a class of ternary carbides and nitrides commonly referred to as MAX phases. In the constitutive relation, we assume that the evolution of the slip system strength in MAX phases has two components – a classical component that depends on the Taylor cumulative shear strain and a non-Schmid component that depends on the stress normal to the slip plane. The non-Schmid crystal plasticity constitutive relation is then used to carry out finite element simulations of micropillar compression of single crystals of two MAX phases, Ti 2 AlC and Ti 3 AlC 2 . The finite element simulations not only quantitatively predict the stress – strain response of a wide range of crystallographic orientations of the micropillars but also rationalize the non-uniform deformation and the deformed shape of the micropillars observed in the experiments for the two materials. As a result, parametric studies are also carried out to quantify the role of the non-Schmid effect and understand the effects of key experimental parameters on the stress – strain response of the micropillars of the two MAX phases.

36 MATERIALS SCIENCE↗

Fracture Toughness of Thin Plates by the Double-Torsion Test Method

Double torsion testing can produce fracture toughness values without crack length measurement that are comparable to those measured via standardized techniques such as the chevron-notch, surface-crack-in-flexure and precracked beam if the appropriate geometry is employed, and the material does not exhibit increasing crack growth resistance. Results to date indicate that 8 < W/d < 80 and L/W > 2 are required if crack length is not considered in stress intensity calculations. At L/W = 2, the normalized crack length should be 0.35 < a/L < 0.65; whereas for L/W = 3, 0.2 < a/L < 0.75 is acceptable. In addition, the load-points need to roll to reduce friction. For an alumina exhibiting increasing crack growth resistance, values corresponding to the plateau of the R-curve were measured. For very thin plates (W/d > 80) nonlinear effects were encountered.

Salem, Jonathan A.↗