Electrochemical Evolution of Fuel Cell Platinum Nanocatalysts on Carbon Nanotubes at the Atomic Scale

The evolution of Pt nanoparticles supported on carbon nanotubes is analyzed before and after electrochemical potential cycling, using identical location aberration-corrected transmission electron microscopy, for applications in proton exchange membrane fuel cells. The work is focused on the half-cell accelerated stress test protocol of potential cycles ranging between 1.0 and 1.5 V RHE to represent the start-up/shutdown settings of a fuel cell vehicle. The research work reveals that particle migration and coalescence are key mechanisms for a reduction in the Pt nanoparticle surface area at the early stages of potential cycling. Further, the mechanism for particle movement and coalescence is attributed to carbon corrosion, catalyzed either by Pt or by bulk corrosion of the carbon nanotubes. Carbon corrosion results in the appearance of carbon vacancies at the carbon nanotube/Pt nanoparticle interface during cycling, as well as the formation of edge and surface defects. During cycling, the concentration of the dissoluble Pt increases. As soon as a significant amount is reached, subnanometer/atomic clusters emerge on the carbon nanotube support, which can move and coalesce, or redeposit on the surface of larger particles through Ostwald ripening.

25 ENERGY STORAGE↗

Electrochemical Degradation of Pt–Ni Nanocatalysts: An Identical Location Aberration-Corrected Scanning Transmission Electron Microscopy Study

The evolution of Pt–Ni nanoparticles supported on amorphous carbon is investigated before and after electrochemical potential cycling (0.6-1.1 V), using aberration-corrected scanning transmission electron microscopy (STEM) and energy dispersive X-ray spectroscopy (EDS). During voltage cycling and due to the dissolution of nanoparticles, single ions/atoms and ionic/atomic clusters emerge and diffuse across the carbon support toward larger nanoparticles, where they redeposit. We observe that the preferred locations for the dissolution are the steps and corners of the nanoparticles. On the other hand, the redeposition process happens often on {111} type planes. In addition, contrary to the conventional view, where larger particles grow isotropically from smaller ones, this research work shows that anisotropic growth of smaller particles occurs during potential cycling. The reason for this behavior seems to be related to the fact that smaller particles with thicker Pt-rich shells trigger the nucleation and deposition of Pt.

catalysts↗

Effect of Particle Size and Operating Conditions on Pt 3 Co PEMFC Cathode Catalyst Durability

The initial performance and decay trends of polymer electrolyte membrane fuel cells (PEMFC) cathodes with Pt 3 Co catalysts of three mean particle sizes (4.9 nm, 8.1 nm, and 14.8 nm) with identical Pt loadings are compared. Even though the cathode based on 4.9 nm catalyst exhibited the highest initial electrochemical surface area (ECA) and mass activity, the cathode based on 8.1 nm catalyst showed better initial performance at high currents. Owing to the low mass activity of the large particles, the initial performance of the 14.8 nm Pt3Co-based electrode was the lowest. The performance decay rate of the electrodes with the smallest Pt 3 Co particle size was the highest and that of the largest Pt 3 Co particle size was lowest. Interestingly, with increasing number of decay cycles (0.6 to 1.0 V, 50 mV/s), the relative improvement in performance of the cathode based on 8.1 nm Pt 3 Co over the 4.9 nm Pt 3 Co increased, owing to better stability of the 8.1 nm catalyst. The electron microprobe analysis (EMPA) of the decayed membrane-electrode assembly (MEA) showed that the amount of Co in the membrane was lower for the larger particles, and the platinum loss into the membrane also decreased with increasing particle size. This suggests that the higher initial performance at high currents with 8.1 nm Pt 3 Co could be due to lower contamination of the ionomer in the electrode. Furthermore, lower loss of Co from the catalyst with increased particle size could be one of the factors contributing to the stability of ECA and mass activity of electrodes with larger cathode catalyst particles. To delineate the impact of particle size and alloy effects, these results are compared with prior work from our research group on size effects of pure platinum catalysts. The impact of PEMFC operating conditions, including upper potential, relative humidity, and temperature on the alloy catalyst decay trends, along with the EMPA analysis of the decayed MEAs, are reported.

30 DIRECT ENERGY CONVERSION↗