Search NASA⌕ Search

Engineering topics

Rebak, Raul

Publications and source records attributed to Rebak, Raul.

Effect of nickel on the oxidation behavior of FeCrAl alloy in simulated PWR and BWR conditions

FeCrAl alloys are being investigated as candidate materials for light water reactor fuel claddings. The chemical composition of FeCrAl determines its resistance to corrosion under normal operating conditions. The purpose of this paper is to investigate the effect of 0, 1, 3 wt% Ni addition on the passivation characteristics of Fe17Cr5.5Al in oxygenated and hydrogenated simulated reactor waters for 3-month immersion. Current results show that Ni addition improves the passivation of FeCrAl under oxygenated condition and decreases the mass loss under hydrogenated conditions.

36 MATERIALS SCIENCE↗

Oxidation Resistance in 1200°C Steam of a FeCrAl Alloy Fabricated by Three Metallurgical Processes

Abstract FeCrAl alloys are a leading candidate material for accident tolerant fuel cladding due to their good performance in both normal light-water reactor operating conditions as well as their resilience to high-temperature accident scenarios. For commercial-scale production, new fabrication techniques need to be investigated. In this study, the effects of fabrication methods on the high-temperature steam oxidation performance of C26M (Fe12Cr6Al2Mo in wt.%) were investigated. Three variants of C26M were manufactured: wrought (cast and forged) (WC26M), powder metallurgy hot isostatic pressing (PMC26M), and laser powder bed fusion additive manufacturing (AMC26M). All three variants were exposed to steam at 1200°C for 2 h. Results showed no significant variation in mass change between the variants after steam exposure. All three variants effectively formed stable protective alumina films with ~0.6–1.3 µ m thickness. This study suggests FeCrAl alloys have excellent resilience to high-temperature steam in nuclear reactor accident scenarios regardless of the fabrication method.

Materials Science↗

Hydrothermal corrosion of 2nd generation FeCrAl alloys for accident tolerant fuel cladding

As part of an effort to develop advanced fuel cladding for use in light water reactors, several FeCrAl alloys have been developed at Oak Ridge National Laboratory. A second generation of these alloys bearing additional alloying elements over the previously tested model alloys were tested in boiling water reactor (BWR) conditions to determine their resistance to hydrothermal corrosion. Coupons with alloy compositions Fe–10Cr–6Al–2Mo, Fe–13Cr–5Al–2Mo, Fe–13Cr–6Al–2Mo, Fe–13Cr–7Al–2Mo, and Fe–13Cr–5Al–2Mo–1Nb were tested in normal water chemistry (NWC) and hydrogen water chemistry (HWC) for 9 months in continuously refreshing autoclaves. Commercial FeCrAl alloy APMT and Zircaloy-2 were also tested for comparison. Among samples exposed to HWC, Fe–13Cr–7Al–2Mo performed worst with an average mass loss of 1.3 mg/cm2 over 9 months. This mass loss represents an estimated thickness loss of approximately 60 μm over 6 years. Samples exposed to NWC had very small mass losses of less than 0.15 mg/cm2 or mass gains up to 0.05 mg/cm2. Based on the results of this testing, the 2nd generation FeCrAl alloys tested exhibit low wall thickness loss and are suitable in terms of corrosion resistance for use as LWR cladding in BWR-HWC and BWR-NWC under normal operating conditions.

Raiman, Stephen↗

Hydrothermal Corrosion of Second Generation FeCrAl Alloys in Boiling Water Reactor Conditions

As part of an effort to develop advanced fuel cladding for use in light water reactors, several ORNL-developed FeCrAl alloys were tested in BWR conditions to determine their resistance to hydrothermal corrosion. Coupons with alloy compositions Fe-10Cr-6Al-2Mo, Fe-13Cr-5Al-2Mo, Fe-13Cr-6Al-2Mo, Fe-13Cr-7Al-2Mo, and Fe-13Cr-5Al-2Mo-1Nb were tested in BWR-NWC and BWR-HWC for 9 months in continuously refreshing autoclaves. Commercial APMT and Zircaloy-2 were also tested for comparison. Among samples exposed to HWC, Alloy C06M (10Cr-6Al) performed best, with a mass loss of 0.34 mg/cm 2 over 9 months, and C037M performed worst with a mass loss of 1.2 mg/cm 2 over 9 months. This mass loss was similar to Gen-1 FeCrAl alloys, and represents an estimated annual thickness loss of approximately a few µm per year. Samples exposed to NWC had very small mass losses of less than 0.15 mg/cm 2 or mass gains up to 0.05 mg/cm 2 . These represent very small annual losses in thickness. Based on the results of this testing, the Gen-2 FeCrAl alloys tested have suitable resistance to hydrothermal corrosion for use as fuel cladding in BWR-NWC and BWR-HWC conditions.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Oxidation of Advanced Steel Cladding Alloys in Extreme Environments

Accident tolerant claddings must withstand the loss of coolant for longer times than conventional zirconium-based reactor claddings. Advanced steel alloys (such as Alloy 33, APMT) offer enhanced resistance to high-temperature oxidation in steam environments due to the formation of protective oxide layers of chromia and/or alumina oxides on the surface of the alloy, which enhance their stability at high temperatures by acting as an effective diffusion barrier, so resulting in low rate of oxidation. These passivating oxide layers, resistant to accelerated oxidation, offer an improvement over the current designs by reducing the production of hydrogen gas, and by delaying the release of fission products into the environment. Hence, these alloys present a great opportunity to explore alternative cladding materials with better accident tolerance for commercial light water reactors. Alloy 33 and APMT showed enhanced resistance to corrosion under the normal operation and off-nominal conditions of light water reactors.

36 MATERIALS SCIENCE↗

Synchrotron Characterization of the Oxidation of Advanced Steel Cladding Alloys

Advanced steel alloys are proposed as nuclear fuel claddings due to their high corrosion resistance under extreme conditions of pressure and temperature. APMT is an iron based alloy (Fe-22wt.%Cr-5.8wt.%Al) and Alloy 33 is a mixture of iron, chromium, and nickel (32wt.%Fe-33wt.%Cr-31wt.%Ni). This paper focuses on studying the corrosion mechanisms for these alloys under exposure to superheated steam at 800 deg. C and 1000 deg. C using the synchrotron based X-ray diffraction (XRD) and Hard X-ray photoelectron spectroscopy (HAXPES) techniques. HAXPES data was collected using 4 keV X-rays with a 1x1 mm spot size at X24A beamline. Specimens were mounted on the sample holder. The specimens were tilted 5 degrees relative to the beam and the estimated probe depth (for this fixed energy) is 63 A. The X-ray wavelength for XRD studies at X14A beamline is 0.7792 A with a beam size of of 2 x 0.2 mm{sup 2}. Specimens were exposed to steam environment at 800 and 1000 deg. C for 8, 24, and 48 hours. For Alloy 33; a layer of mixed Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} oxides is formed after exposure to steam. Specimen tilting indicated that Cr{sub 2}O{sub 3} is formed near the metal/oxide interface and FeCr{sub 2}O{sub 4} was formed on the oxide surface. The oxide peak intensities increased with an increase in steam temperature. The specimen oxidized at 1000 deg. C had well-developed oxide peaks compared to the specimen oxidized at 800 deg. C. For APMT; a layer of mixed α-Al{sub 2}O{sub 3} and monoclinic θ-Al{sub 2}O{sub 3} oxides is formed on the outer surface. The peak intensities of the monoclinic θ-Al{sub 2}O{sub 3} phase, decreases relative to the peaks from the Al{sub 2}O{sub 3} phase with increasing tilt angle. This indicates that the surface is dominated by the θ-Al{sub 2}O{sub 3}. After exposure to steam at 800 deg. C, oxidation of Alloy 33 results in the formation of Cr{sub 2}O{sub 3} oxide with time and absence of both metallic and substoichiometric phases is observed. No nickel peaks are seen on the surface after oxidation at 800 deg. C, however Fe(II) peak is noticed after 8 and 24 hours of steam exposure, which then disappears after 48 hours. This presence of FeCr{sub 2}O{sub 4} oxide phase is observed after 8 and 24 hours. After exposure to steam at 1000 deg. C, the Cr{sub 2}p{sub 3/2} doublet persists at all exposure times, indicating the presence of the FeCr{sub 2}O{sub 4} oxide. Nickel peak is found on the surface at all exposure times and is attributed to the presence of Ni(OH){sub 2} phase. This may be due to increased diffusion of Ni through chromic oxide scale at higher temperature as compared to 800 deg. C. This nickel reacts with steam at 1000 deg. C to form Ni hydroxide at the surface. For APMT, after exposure to steam at 800 and 1000 deg. C, no Al and Cr metal peaks are seen. Growth of oxide layer is seen with increase in exposure time. The oxide structure contains mainly Al{sub 2}O{sub 3} oxide with the addition of mixed oxide (Al{sub x}Cr{sub 1-x}){sub 2}O{sub 3}. These results demonstrate that Cr diffuses into the alumina layer. (authors)

36 MATERIALS SCIENCE↗

Iron-Based Amorphous Metals: High-Performance Corrosion-Resistant Material Development

In this study, an overview of the High-Performance Corrosion-Resistant Materials (HPCRM) Program, which was cosponsored by the Defense Advanced Research Projects Agency (DARPA) Defense Sciences Office (DSO) and the U.S. Department of Energy (DOE) Office of Civilian and Radioactive Waste Management (OCRWM), is discussed. Programmatic investigations have included a broad range of topics: alloy design and composition, materials synthesis, thermal stability, corrosion resistance, environmental cracking, mechanical properties, damage tolerance, radiation effects, and important potential applications. Amorphous alloys identified as SAM2X5 (Fe 49.7 Cr 17.7 Mn 1.9 Mo 7.4 W 1.6 B 15.2 C 3.8 Si 2.4 ) and SAM1651 (Fe 48 Mo 14 Cr 15 Y 2 C 15 B 6 ) have been produced as meltspun ribbons (MSRs), dropcast ingots, and thermal-spray coatings. Chromium (Cr), molybdenum (Mo), and tungsten (W) additions provided corrosion resistance, while boron (B) enabled glass formation. Earlier electrochemical studies of MSRs and ingots of these amorphous alloys demonstrated outstanding passive film stability. More recently, thermal-spray coatings of these amorphous alloys have been made and subjected to long-term salt-fog and immersion tests; good corrosion resistance has been observed during salt-fog testing. Corrosion rates were measured in situ with linear polarization, while the open-circuit corrosion potentials (OCPs) were simultaneously monitored; reasonably good performance was observed. The sensitivity of these measurements to electrolyte composition and temperature was determined. The high boron content of this particular amorphous metal makes this amorphous alloy an effective neutron absorber and suitable for criticality-control applications. In general, the corrosion resistance of such iron-based amorphous metals is maintained at operating temperatures up to the glass transition temperature. These materials are much harder than conventional stainless steel and Ni-based materials, and are proving to have excellent wear properties, sufficient to warrant their use in earth excavation, drilling, and tunnel-boring applications. Large areas have been successfully coated with these materials, with thicknesses of approximately 1 cm. The observed corrosion resistance may enable applications of importance in industries such as oil and gas production, refining, nuclear power generation, shipping, etc.

36 MATERIALS SCIENCE↗